Indentation techniques for assessing fracture toughness are attractive due to the simplicity and expediency of experiments, and because they potentially allow the characterization of both local and bulk fracture properties. Unfortunately, rarely have such techniques been proven to give accurate fracture toughness values. This is a concern, as such techniques are seeing increasing usage in the study of biomaterials and biological hard tissues. Four available indentation techniques are considered in the present article: the Vickers indentation fracture (VIF) test, the cube corner indentation fracture (CCIF) test, the Vickers crack opening displacement (VCOD) test and the interface indentation fracture (IIF) test. Each technique is discussed in terms of its suitability for assessing the absolute and relative toughness of materials or material interfaces based on the published literature on the topic. In general, the VIF and CCIF techniques are found to be poor for quantitatively evaluating toughness of any brittle material, and the large errors involved (approximately +/-50%) make their applicability as comparative techniques limited. Indeed, indentation toughness values must differ by at least by a factor of three to conclude a significant difference in actual toughness. Additionally, new experimental results are presented on using the CCIF test to evaluate the fracture resistance of human cortical bone. Those new results indicate that inducing cracking is difficult, and that the cracks that do form are embedded in the plastic zone of the indent, invalidating the use of linear elastic fracture mechanics based techniques for evaluating the toughness associated with those cracks. The VCOD test appears to be a good quantitative method for some glasses, but initial results suggest there may be problems associated with applying this technique to other brittle materials. Finally, the IIF technique should only be considered a comparative or semi-quantitative technique for comparing material interfaces and/or the neighboring materials.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Orthopaedic implants and arthroplasty · Metal and Thin Film Mechanics · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. A critical evaluation of indentation techniques for measuring fracture toughness. I. Direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
2. Debonding of interfaces between beta-silicon nitride whiskers and Si–Al–Y oxynitride glasses10.1016/S1359-6454(96)00069-9 ↗
3. Crack opening profiles of indentation cracks in normal and anomalous glasses10.1016/j.actamat.2003.09.014 ↗
4. Composition of the cement line and its possible mechanical role as a local interface in human compact bone10.1016/0021-9290(88)90132-7 ↗
5. Validity of the bulk-staining technique to separate artifactual from in vivo bone damage10.1097/00003086-199011000-00047 ↗
6. Direct observation and analysis of indentation cracking in glasses and ceramics10.1111/j.1151-2916.1990.tb05119.x ↗
7. Elastic constants, Vickers hardness, and fracture toughness of fluorrichterite-based glass-ceramics10.1016/S0109-5641(03)00094-0 ↗
8. Fett, T., 2002. Computation of the crack opening displacements for Vickers indentation cracks. Karlsruhe, Germany, Forschungszentrum Karlsruhe, Report FZKA 6757
9. Stresses and stress intensity factor from COD of Vickers indentation cracks10.1023/B:JMSC.0000017792.25386.1d ↗
10. Influence of narrow starter notches on the initial crack growth resistance curve of ceramics10.1007/s00419-006-0055-3 ↗
11. Crack opening displacements of Vickers indentation cracks10.1016/j.engfracmech.2004.07.003 ↗
12. Vickers microtoughness of SiC in the median-crack regime
13. Crack deflection at an interface between dissimilar elastic materials10.1016/0020-7683(89)90021-8 ↗
14. The dentin-enamel junction and the fracture of human teeth10.1038/nmat1323 ↗
15. Johnson · 1985
16. Processing-microstructure-property relations in HVOF sprayed calcium phosphate based bioceramic coatings10.1016/S0142-9612(03)00027-9 ↗
17. Mechanical properties, phase stability, and biocompatibility of (Y,Nb)−TZP/Al2O3 composite abutments for dental implant10.1002/1097-4636(2000)53:4<438::AID-JBM19>3.0.CO;2-3 ↗
18. The true toughness of human cortical bone measured with realistically short cracks10.1038/nmat2221 ↗
19. Yield strength predictions from the plastic zone around nanocontacts10.1016/S1359-6454(98)00301-2 ↗
20. Crack blunting, crack bridging and resistance-curve fracture mechanics in dentin: Effect of hydration10.1016/S0142-9612(03)00458-7 ↗
21. Determining the toughness of ceramics from Vickers indentations using the crack-opening displacements: An experimental study10.1111/j.1151-2916.2003.tb03490.x ↗
22. Comments on Measurement of the microstructural fracture toughness of cortical bone using indentation fracture10.1016/j.jbiomech.2008.01.022 ↗
23. The elastic plastic indentation of ceramics10.1007/BF00721390 ↗
24. New formula for indentation toughness in ceramics10.1007/BF01729352 ↗
25. Elastic/plastic indentation damage in ceramics: The median/radial crack system10.1111/j.1151-2916.1980.tb10768.x ↗
26. Indentation fracture toughness of sintered silicon carbide in the Palmqvist crack regime10.1111/j.1151-2916.1989.tb06242.x ↗
27. Glass-reinforced hydroxyapatite composites: Fracture toughness and hardness dependence on microstructural characteristics10.1016/S0142-9612(99)00112-X ↗
28. Mechanical properties of the dentinoenamel junction: AFM studies of nanohardness, elastic modulus, and fracture10.1002/1097-4636(200101)54:1<87::AID-JBM10>3.0.CO;2-Z ↗
29. A study on evaluation of KIc for structural ceramics10.1299/kikaia.51.2489 ↗
30. In situ cube-corner indentation of soda-lime glass and fused silica10.1111/j.1551-2916.2004.01494.x ↗
31. Radial fracture during indentation by acute probes: I, description by an indentation wedging model10.1007/s10704-005-6034-9 ↗
32. Radial fracture during indentation by acute probes: II, Experimental observations of cube-corner and Vickers indentation10.1007/s10704-005-6033-x ↗
33. Measurement of the microstructural fracture toughness of cortical bone using indentation fracture10.1016/j.jbiomech.2007.04.020 ↗
34. Fracture toughness determination of Al2O3 using four-point-bend specimens with straight-through and chevron notches10.1111/j.1151-2916.1980.tb10725.x ↗
35. Mechanistic aspects of fracture and R-curve behavior of human cortical bone10.1016/j.biomaterials.2004.02.017 ↗
36. A fracture-mechanics analysis of indentation-induced Palmqvist crack in ceramics10.1007/BF00725625 ↗
37. Measurement of mechanical properties by ultra-low load indentation10.1016/S0921-5093(98)00724-2 ↗
38. Vickers indentation fracture toughness test. Part 1. Review of literature and formulation of standardized indentation toughness equations10.1179/mst.1989.5.9.865 ↗
39. Vickers indentation fracture toughness test. Part 2. Application and critical evaluation of standardized indentation toughness equations10.1179/mst.1989.5.10.961 ↗
40. On the Vickers indentation fracture toughness test10.1111/j.1551-2916.2006.01482.x ↗
41. Indentation brittleness of ceramics: A fresh approach10.1023/A:1018671823059 ↗
42. Variations in the individual thick lamellar properties within osteons by nanoindentation10.1016/S8756-3282(99)00163-5 ↗
43. Cyclic fatigue-crack propagation, stress-corrosion, and fracture-toughness behavior in pyrolytic carbon-coated graphite for prosthetic heart valve applications10.1002/jbm.820240206 ↗
44. Rising crack-growth-resistance behavior in cortical bone: Implication for toughness measurements10.1016/j.jbiomech.2003.11.003 ↗
45. Calculation of porosity and osteonal cement line effects on the effective fracture toughness of cortical bone in longitudinal crack growth10.1002/1097-4636(20000905)51:3<504::AID-JBM27>3.0.CO;2-I ↗