Low-temperature degradation of Y-TZP ceramics: A systematic review and meta-analysis

G.K.R. Pereira, A.B. Venturini, T. Silvestri, K.S. Dapieve, A.F. Montagner, F.Z.M. Soares, L.F. Valandro

Publisher page

Abstract

The aim of this study was to systematically review the literature to assess if low-temperature degradation (LTD) simulation in autoclave promotes deleterious impact on the mechanical properties and superficial characteristics of Y-TZP ceramics compared to the non-aged protocol. The MEDLINE via PubMed electronic database was searched with included peer-reviewed publications in English language and with no publication year limit. From 413 potentially eligible studies, 49 were selected for full-text analysis, 19 were included in the systematic review with 12 considered in the meta-analysis. Two reviewers independently selected the studies, extracted the data, and assessed the risk of bias. Statistical analysis was performed using RevMan 5.1, with random effects model, at a significance level of p<0.05. Descriptive analysis of monoclinic phase content data showed that aging in autoclave promotes an increase in m-phase content (ranging from 0% up to 13.4% before and 2.13% up to 81.4% after aging) with intensity associated to the material susceptibility and to the aging parameters (time, pressure and temperature). Risk of bias analysis showed that only 1 study presented high risk, while the majority showed medium risk. Five meta-analyzes (factor: aging×control) were performed considering global and subgroups analyzes (pressure, time, temperature and m-phase % content) for flexural strength data. In the global analysis a significant difference (p<0.05) was observed between conditions, favoring non-aging group. Subgroup analysis revealed statistical difference (p<0.05) favoring non-aging, for aging time >20h. However, for shorter aging times (≤20h), there was no difference between groups. Pressure subgroup analysis presented a statistical difference (p<0.05) only when a pressure ≥2bar was employed, favoring non-aging group. Temperature subgroup analysis showed a statistical difference (p<0.05) only when temperature=134°C was used, favoring the non-aging group. M-phase % content analysis presented statistical difference (p<0.05) when more than 50% of m-phase content was observed, favoring non-aging group. High heterogeneity was found in some comparisons. Aging in autoclave promoted low-temperature degradation, impacting deleteriously on mechanical properties of Y-TZP ceramics. However, the effect of LTD depends on some methodological parameters indicating that aging time higher than 20h; pressure ≥2bar and temperature of 134°C are ideal parameters to promote LTD effects, and that those effect are only observed when more than 50% m-phase content is observed.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Advanced ceramic materials synthesis · Recycling and utilization of industrial and municipal waste in materials production

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (58)

Show source-provided references
1. Low- temperature degradation of a Y-TZP ceramic after surface treatments10.1002/jbm.b.32957 ↗
2. Quantitative phase analysis from X-ray diffraction in Y-TZP dental ceramicas: a critical evaluation10.1016/j.jdent.2014.08.010 ↗
3. Biaxial flexure strength and low temperature degradation of Ce-TZP/Al2O3 nanocomposite and Y-TZP as dental restoratives10.1002/jbm.b.31131 ↗
4. High-strength CAD/CAM-fabricated veneering material sintered to zirconia copings—a new fabrication mode for all-ceramic restorations10.1016/j.dental.2008.04.019 ↗
5. In vitro performance of full-contour zirconia single crowns10.1016/j.dental.2011.11.024 ↗
6. Influence of hydrothermal and mechanical conditions on the strength of zirconia10.1016/j.actbio.2010.07.025 ↗
7. Long term in vivo and in vitro aging of a zirconia ceramic used in orthopaedy10.1002/jbm.820280512 ↗
8. Low temperature degradation of a Y-TZP dental ceramic10.1016/j.actbio.2010.09.020 ↗
9. Low temperature aging of Y-TZP ceramics10.1111/j.1151-2916.1999.tb02055.x ↗
10. Low-temperature degradation of zirconia and implications for biomedical implants10.1146/annurev.matsci.37.052506.084250 ↗
11. Measurement of the crystallographically transformed zone produced by fracture in ceramics containing tetragonal zirconia10.1111/j.1151-2916.1982.tb10445.x ↗
12. Current ceramic materials and systems with clinical recommendations: a systematic review10.1016/S0022-3913(07)60124-3 ↗
13. Effects of aging procedures on the topographic surface, structural stability, and mechanical strength of a ZrO2-based dental ceramic10.1016/j.dental.2014.08.380 ↗
14. Martensitic relief observation by atomic force microscopy in yttria-stabilized zirconia10.1111/j.1151-2916.2003.tb03639.x ↗
15. A critical comparison of methods for the determination of the aging sensitivity in biomedical grade yttria-stabilized zirconia10.1002/jbm.b.30123 ↗
16. Factors affecting the mechanical behaviour of Y-TZP10.1016/j.jmbbm.2014.05.013 ↗
17. Accelerated aging characteristics of three yttria-stabilized tetragonal zirconia polycrystalline dental materials10.1016/S0022-3913(12)60166-8 ↗
18. Effect of hydrothermal degradation on three types of zirconias for dental application10.1016/j.prosdent.2014.07.015 ↗
19. Phase analysis in zirconia systems10.1111/j.1151-2916.1972.tb11290.x ↗
20. Higgins, J.P.T., Green, S. (Eds.), 2011. Cochrane Handbook for Systematic Reviews of Interventions Version 5.1.0 (updated March 2011). The Cochrane Collaboration. Available from 〈www.cochrane-handbook.org〉.
21. Inhibition of low-temperature degradation of tetragonal zirconia ceramics—a review
22. Protection of yttria-stabilized zirconia for dental application by oxidic PVD coating10.1016/j.actbio.2014.09.042 ↗
23. Influence of sintering conditions on low-temperature degradation of dental zirconia10.1016/j.dental.2014.03.005 ↗
24. Aging resistance of surface-treated dental zirconia10.1016/j.dental.2014.11.018 ↗
25. ISO 13356-2008 · 2008
26. ISO 6872-2008 · 2008
27. The martensitic transformation in ceramics: its role in transformation toughening10.1016/S0079-6425(00)00005-0 ↗
28. Effect of tetravalent dopants on Raman spectra of tetragonal zirconia10.1111/j.1151-2916.1997.tb03003.x ↗
29. The effect of low temperature aging on the mechanical property and phase stability of YTZP ceramics10.4047/jap.2009.1.3.113 ↗
30. Concerns of hydrothermal degradation in CAD/CAM zirconia10.1177/0022034509354193 ↗
31. Phase change and mechanical properties of ZrO2–Y2O3 solid electrolyte after ageing10.1016/0167-2738(81)90138-7 ↗
32. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic10.1016/S0109-5641(99)00070-6 ↗
33. The effects of dental grinding and sandblasting on ageing and fatigue behavior of dental zirconia (Y-TZP) ceramics10.1016/j.jeurceramsoc.2007.09.013 ↗
34. Y-TZP ceramic processing from coprecipitated powders: a comparative study with three commercial dental ceramics10.1016/j.dental.2008.04.002 ↗
35. Effects of surface treatments on the susceptibilities of low temperature degradation by autoclaving in zirconia10.1002/jbm.b.32700 ↗
36. Phase transformation of dental zirconia following artificial aging
37. Low temperature degradation – ageing – of zirconia: a critical review of the relevant aspects in dentistry10.1016/j.dental.2010.04.006 ↗
38. Preferred reporting items for systematic reviews and meta-analyses: the prisma statement10.1371/journal.pmed.1000097 ↗
39. MMP inhibitors on dentin stability: a systematic review and meta-analysis10.1177/0022034514538046 ↗
40. Subsurface evaluation of hydrothermal degradation of zirconia10.1016/j.actamat.2010.09.047 ↗
41. The influence of low-temperature degradation and cyclic loading on the fracture resistance of monolithic zirconia crowns10.1016/j.jmbbm.2015.03.007 ↗
42. Effect of low-temperature aging on the mechanical behavior of ground Y-TZP10.1016/j.jmbbm.2014.12.009 ↗
43. Raman spectroscopic analysis of phase transformation and stress patterns in zirconia hip joints10.1117/1.1647547 ↗
44. Zirconia as a ceramic biomaterial10.1016/S0142-9612(98)00010-6 ↗
45. Full-contour Y-TZP ceramic surface roughness effect on synthetic hydroxyapatite wear10.1016/j.dental.2013.03.008 ↗
46. The role of resin cement on bond strength of glass-fiber posts (GFPs) luted into root canals: a systematic review and meta-analysis of in vitro studies10.2341/13-070-LIT ↗
47. Transformation of yttria-doped tetragonal ZrO2 polycrystals by annealing in water10.1111/j.1151-2916.1985.tb15239.x ↗
48. Significance of internal stresses for the martensitic transformation in yttria-stabilized zirconia polycrystals during degradation10.1111/j.1151-2916.1986.tb04789.x ↗
49. Stability of Y-TZP during hydrothermal treatment: neutron experiments and stability considerations10.1016/j.jeurceramsoc.2004.03.025 ↗
50. Effect of in vitro aging on the flexural strength and probability to fracture of Y-TZP zirconia ceramics for all-ceramic restorations10.1016/j.dental.2014.05.033 ↗
51. Phase stability after aging and its influence on pin-on-disk wear properties of Ce-TZP/Al2O3 nanocomposite and conventional Y-TZP10.1002/jbm.a.10006 ↗
52. Analysis of residual stresses in thermal barrier coatings10.1016/S0924-0136(99)00157-0 ↗
53. Calibration curve for quantitative analysis of the monoclinic-tetragonal ZrO2 systems by X-ray diffraction10.1111/j.1151-2916.1984.tb19614.x ↗
54. Stress fatigue: basic principles and prosthodontic implications
55. Aging performances for resisting low-temperature of three dental yttria-stabilized zirconia ceramic core materials
56. Role of H2O on the degradation process of Y-TZP10.1007/BF01756800 ↗
57. Effect of sandblasting on the long-term performance of dental ceramics
58. Fatigue of dental ceramics10.1016/j.jdent.2013.10.007 ↗