Static and fatigue mechanical behavior of three dental CAD/CAM ceramics
Source abstract
Abstract
Purpose The aim of this study was to measure the mechanical properties and fatigue behavior of three contemporary used dental ceramics, zirconia Cercon(®) (ZC), lithium disilicate e.max(®) CAD (LD), and polymer-infiltrated ceramic Enamic(®) (PIC). Methods Flexural strength of each CAD/CAM ceramic was measured by three point bending (n=15) followed by Weibull analysis. Elastic modulus was calculated from the load-displacement curve. For cyclic fatigue loading, sinusoidal loading with a frequency of 8Hz with minimum load 3N were applied to these ceramics (n=24) using three point bending from 10(3) to 10(6) cycles. Fatigue limits of these ceramics were predicted with S-N fatigue diagram. Fracture toughness and Vickers hardness of the ceramics were measured respectively by single edge V-notch beam (SEVNB) and microindentation (Hv 0.2) methods. Chemical compositions of the materials׳ surfaces were analyzed by EDS, and microstructural analysis was conducted on the fracture surfaces by SEM. One-way ANOVA was performed and the level of significance was set at 0.05 to analyze the numerical results. Results The mean flexural strength of ZC, LD, and PIC was respectively 886.9, 356.7, and 135.8MPa. However, the highest Weibull modulus belonged to PIC with 19.7 and the lowest was found in LD with 7.0. The fatigue limit of maximum load for one million cycles of ZC, LD, and PIC was estimated to be 500.1, 168.4, and 73.8GPa. The mean fracture toughness of ZC, LD, and PIC was found to be respectively 6.6, 2.8, and 1.4MPam(1/2), while the mean Vickers hardness was 1641.7, 676.7, and 261.7Hv. Fracture surfaces followed fatigue loading appeared to be smoother than that after monotonic loading. Conclusions Mechanical properties of ZC were substantially superior to the two other tested ceramics, but the scattering of data was the least in PIC. The fatigue limit was found to be approximately half of the mean flexural strength for all tested ceramics.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (62)
Show source-provided references
1. Selective infiltration-etching technique for a strong and durable bond of resin cements to zirconia-based materials10.1016/S0022-3913(07)60123-1 ↗
2. Askeland · 2006
3. Mechanical properties of resin-ceramic CAD/CAM restorative materials10.1016/j.prosdent.2015.04.016 ↗
4. Beer · 2006
5. Mechanical fatigue degradation of ceramics versus resin composites for dental restorations10.1016/j.dental.2014.01.003 ↗
6. Fatigue and subcritical crack growth in ZrO2–bioglass ceramics10.1016/j.ceramint.2012.08.093 ↗
7. Cameron · 1996 · 19
8. Fatigue resistance of CAD/CAM complete crowns with a simplified cementation process10.1016/j.prosdent.2013.09.020 ↗
9. The fracture resistance of a CAD/CAM Resin Nano Ceramic (RNC) and a CAD ceramic at different thicknesses10.1016/j.dental.2014.05.018 ↗
10. Damage tolerance of indirect restorative materials (including PICN) after simulated bur adjustments10.1016/j.dental.2015.03.007 ↗
11. In-vitro strength degradation of dental ceramics and novel PICN material by sharp indentation10.1016/j.jmbbm.2013.05.004 ↗
12. Craig · 2002
13. Characterization of a polymer-infiltrated ceramic-network material10.1016/j.dental.2014.02.019 ↗
14. Della Bona · 2014
15. Ceramics for dental applications: a review10.3390/ma3010351 ↗
16. Effect of elasticity on stress distribution in CAD/CAM dental crowns: glass ceramic vs. polymer–matrix composite10.1016/j.jdent.2015.01.008 ↗
17. Fracture strength of ultrathin occlusal veneer restorations made from CAD/CAM composite or hybrid ceramic materials10.1016/S1348-8643(15)00017-8 ↗
18. EN843-5, 2006. Advanced Technical Ceramics – Mechanical Properties of Monolithic Ceramics at Room Temperature
19. Experimental and FE shear-bonding strength at core/veneer interfaces in bilayered ceramics10.1016/j.dental.2011.03.001 ↗
20. Single edge-crack stress intensity factor solutions10.1016/j.engfracmech.2005.09.003 ↗
21. Green · 1998
22. All-ceramic systems: laboratory and clinical performance10.1016/j.cden.2011.01.005 ↗
23. Monolithic CAD/CAM lithium disilicate versus veneered Y-TZP crowns: comparison of failure modes and reliability after fatigue
24. Materials Science and Technology
25. A novel polymer infiltrated ceramic dental material10.1016/j.dental.2011.02.002 ↗
26. Fatigue resistance of denture teeth10.1016/j.jmbbm.2015.08.034 ↗
27. IPS e.max® CAD, 2011. Ivoclar Vivadent AG, Scientific Documentation.
28. ISO 6872, 2008. Dentistry – Ceramic Materials.
29. Fracture strength and fatigue resistance of dental resin-based composites10.1016/j.dental.2009.06.013 ↗
30. Influence of cyclic fatigue in water on the load-bearing capacity of dental bridges made of zirconia10.1016/j.actbio.2008.04.012 ↗
31. Use of contact testing in the characterization and design of all-ceramic crownlike layer structures: a review10.1067/mpr.2001.119581 ↗
32. Comparison of mechanical properties of three machinable ceramics with an experimental fluorophlogopite glass ceramic10.1016/j.prosdent.2015.02.024 ↗
33. Ceramic dental biomaterials and CAD/CAM technology: state of the art10.1016/j.jpor.2014.07.003 ↗
34. Evaluation of sub-critical fatigue crack propagation in a restorative composite10.1016/j.dental.2004.04.005 ↗
35. Load-bearing properties of minimal-invasive monolithic lithium disilicate and zirconia occlusal onlays: finite element and theoretical analyses10.1016/j.dental.2013.04.004 ↗
36. In vitro fatigue resistance of CAD/CAM composite resin and ceramic posterior occlusal veneers10.1016/S0022-3913(10)60111-4 ↗
37. Wear behavior of dental Y-TZP ceramic against natural enamel after different finishing procedures10.1016/j.dental.2012.04.010 ↗
38. Montgomery · 2003
39. Fatigue of the resin-dentin interface: a new approach for evaluating the durability of dentin bonds10.1016/j.dental.2013.01.008 ↗
40. In vitro fatigue behavior of human dentin with implications for life prediction10.1002/jbm.a.10553 ↗
41. On the in vitro fatigue behavior of human dentin: effect of mean stress10.1177/154405910408300305 ↗
42. Factors affecting enamel and ceramic wear: a literature review10.1067/mpr.2002.123851 ↗
43. Quinn · 2007
44. A practical and systematic review of Weibull statistics for reporting strengths of dental materials10.1016/j.dental.2009.09.006 ↗
45. Influence of microstructure and chemistry on the fracture toughness of dental ceramics10.1016/S0109-5641(03)00002-2 ↗
46. Mechanisms of fatigue-crack propagation in ductile and brittle solids10.1023/A:1018655917051 ↗
47. Mechanics and mechanisms of fatigue damage and crack growth in advanced materials10.1016/S0020-7683(99)00096-7 ↗
48. Evaluation of bond strength of resin cements using different general-purpose statistical software packages for two-parameter Weibull statistics10.1016/j.dental.2012.04.013 ↗
49. Sakaguchi · 2012
50. Fatigue behavior in water of Y-TZP zirconia ceramics after abrasion with 30μm silica-coated alumina particles10.1016/j.dental.2010.10.003 ↗
51. Schijve · 2009
52. Shinya · 2014
53. Occlusal geometrical considerations in all-ceramic pre-molar crown failure testing10.1016/j.dental.2011.08.005 ↗
54. Evaluation of mechanical and optical behavior of current esthetic dental restorative CAD/CAM composites10.1016/j.jmbbm.2015.10.004 ↗
55. In vitro lifetime of dental ceramics under cyclic loading in water10.1016/j.biomaterials.2006.12.033 ↗
56. VITA ENAMIC®, 2013. VITA Zahnfabrik, Technical and Scientific Documentation.
57. Fracture strength of two oxide ceramic crown systems after cyclic pre-loading and thermocycling10.1111/j.1365-2842.2005.01604.x ↗
58. Watchman · 2009
59. Fatigue of the resin-enamel bonded interface and the mechanisms of failure10.1016/j.jmbbm.2013.02.017 ↗
60. Effect of fatigue on biaxial flexural strength of bilayered porcelain/zirconia (Y-TZP) dental ceramics10.1016/j.dental.2011.03.019 ↗
61. Fatigue of dental ceramics10.1016/j.jdent.2013.10.007 ↗
62. Zirconia Cercon®, 2006. DeguDent GmbH, Instruction for Use.