journal article·2016-07Open access

Effects of thermal treatments on microstructure and mechanical properties of a Co–Cr–Mo–W biomedical alloy produced by laser sintering

P. Mengucci, G. Barucca, A. Gatto, E. Bassoli, L. Denti, F. Fiori, E. Girardin, P. Bastianoni, B. Rutkowski, A. Czyrska-Filemonowicz

Abstract

Direct Metal Laser Sintering (DMLS) technology based on a layer by layer production process was used to produce a Co-Cr-Mo-W alloy specifically developed for biomedical applications. The alloy mechanical response and microstructure were investigated in the as-sintered state and after post-production thermal treatments. Roughness and hardness measurements, and tensile and flexural tests were performed to study the mechanical response of the alloy while X-ray diffraction (XRD), electron microscopy (SEM, TEM, STEM) techniques and microanalysis (EDX) were used to investigate the microstructure in different conditions. Results showed an intricate network of ε-Co (hcp) lamellae in the γ-Co (fcc) matrix responsible of the high UTS and hardness values in the as-sintered state. Thermal treatments increase volume fraction of the ε-Co (hcp) martensite but slightly modify the average size of the lamellar structure. Nevertheless, thermal treatments are capable of producing a sensible increase in UTS and hardness and a strong reduction in ductility. These latter effects were mainly attributed to the massive precipitation of an hcp Co3(Mo,W)2Si phase and the contemporary formation of Si-rich inclusions.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. Precipitates in as-cast and heat-treated ASTM F75 Co-Cr-Mo-C alloys containing Si and/or Mn10.1007/s11661-011-0604-4 ↗
2. Metallurgical and interfacial characterization of PFM Co–Cr dental alloys fabricated via casting, milling or selective laser melting10.1016/j.dental.2014.01.008 ↗
3. Corrosion fatigue of biomedical metallic alloys: Mechanisms and mitigation10.1016/j.actbio.2011.09.012 ↗
4. Characterization of Co-Cr-Mo alloy after a thermal treatment for high wear resistance10.1016/j.msec.2012.05.003 ↗
5. Structural characterization of biomedical Co–Cr–Mo components produced by direct metal laser sintering10.1016/j.msec.2014.12.009 ↗
6. Joining mechanisms and mechanical properties of PA composites obtained by selective laser sintering10.1108/13552541211212087 ↗
7. Investigation into the failure of inconel exhaust collector produced by laser consolidation10.1016/j.engfailanal.2013.03.025 ↗
8. Craig · 2004
9. Metal additive manufacturing: a review10.1007/s11665-014-0958-z ↗
10. Microstructural characterization of as-cast biocompatible Co–Cr–Mo alloys10.1016/j.matchar.2010.10.011 ↗
11. Microstructural evolution during solution treatment of Co–Cr–Mo–C biocompatible alloys10.1016/j.matchar.2012.03.006 ↗
12. Additive manufacturing: a transformational advanced manufacturing technology
13. In vitro biocompatibility of CoCrMo dental alloys fabricated by selective laser melting10.1016/j.dental.2014.02.008 ↗
14. Microstructure and corrosion behaviour in biological environments of the new forged low-Ni Co–Cr–Mo alloys10.1016/j.biomaterials.2005.01.028 ↗
15. Strain-induced martensitic transformation near twin boundaries in a biomedical Co–Cr–Mo alloy with negative stacking fault energy10.1016/j.actamat.2012.11.041 ↗
16. Investigation on the microstructure, mechanical property and corrosion behavior of the selective laser melted CoCrW alloy for dental application10.1016/j.msec.2015.01.023 ↗
17. Toxicology of wear particles of cobalt-chromium alloy metal-on-metal hip implants Part I: Physicochemical properties in patient and simulator studies10.1016/j.nano.2014.12.005 ↗
18. Carbide formation and dissolution in biomedical Co-Cr-Mo alloys with different carbon contents during solution treatment10.1007/s11661-010-0227-1 ↗
19. Role of strain-induced martensitic transformation on extrusion and intrusion formation during fatigue deformation of biomedical Co–Cr–Mo–N alloys10.1016/j.actamat.2014.08.039 ↗
20. A comparison of the effects of prosthetic and commercially pure metals on retrieved human fibroblasts: The role of surface elemental composition10.1016/j.actbio.2009.07.006 ↗
21. High density selective laser melting of Waspaloy10.1016/j.jmatprotec.2007.04.117 ↗
22. Precipitates in biomedical Co–Cr alloys
23. Nishiyama · 1978
24. Effect of solution treatments on the fcc/hcp isothermal martensitic transformation in Co–27Cr–5Mo–0.05C aged at 800°C10.1016/S1359-6462(98)00489-8 ↗
25. Formation of hcp martensite during the isothermal ageing of an fcc Co–27Cr–5Mo–0.05C orthopaedic implant alloy10.1007/s11661-999-0267-6 ↗
26. Temperature effects on the lattice constants and crystal structure of a Co–27Cr–5Mo low-carbon alloy10.1007/s11661-006-0232-6 ↗
27. Microstructural effects on the wear resistance of wrought and as-cast Co–Cr–Mo–C implant alloys10.1002/jbm.a.30392 ↗
28. Structural integrity of direct metal laser sintered parts subjected to thermal and finishing treatments10.1016/j.jmatprotec.2013.06.013 ↗
29. Direct laser sintering of metal powders: mechanism, kinetics and microstructural features10.1016/j.msea.2006.04.117 ↗
30. Stadelmann, P., 2007. JEMS: Java Electron Microscopy Software. Available from: 〈〈http://cimeepfl.ch〉〉.
31. The development of a scanning strategy for the manufacture of porous biomaterials by selective laser melting10.1007/s10856-009-3763-8 ↗
32. Development of athermal ε-martensite in atomized Co–Cr–Mo–C implant alloy powders10.1016/j.actbio.2006.04.003 ↗
33. Microstructures and mechanical properties of Co–29Cr–6Mo alloy fabricated by selective laser melting process for dental applications10.1016/j.jmbbm.2013.01.021 ↗
34. Internal fit evaluation of crowns prepared using a new dental crown fabrication technique: laser-sintered Co–Cr crowns10.1016/S0022-3913(09)60165-7 ↗
35. Alloys for prosthodontic restorations10.1067/mpr.2002.123817 ↗
36. In vitro biocompatibility of Co–Cr alloy fabricated by selective laser melting or traditional casting techniques10.1016/j.matlet.2012.08.032 ↗
37. Surface characteristics and corrosion properties of selective laser melted Co–Cr dental alloy after porcelain firing10.1016/j.dental.2013.11.013 ↗
38. Inorganic materials database for exploring the nature of material10.1143/JJAP.50.11RH02 ↗
39. Nanoarchitectured Co–Cr–Mo orthopedic implant alloys: Nitrogen enhanced nanostructural evolution and its effect on phase stability10.1016/j.actbio.2012.12.013 ↗
40. Local strain evolution due to athermal γ-ε martensitic transformation in biomedical Co–Cr–Mo alloys10.1016/j.jmbbm.2013.12.019 ↗
41. ssessment of precipitation behaviour in dental castings of a Co–Cr–Mo alloy10.1016/j.jmbbm.2015.06.020 ↗
42. Effects of chromium and nitrogen content on the microstructures and mechanical properties of as-cast Co–Cr–Mo alloys for dental applications10.1016/j.actbio.2012.03.024 ↗
43. Effect of isothermal aging on the microstructural evolution of Co–Cr–Mo–C alloy10.1016/j.msea.2010.06.081 ↗