journal article·2019-02Open access

Ultra-thin occlusal veneers bonded to enamel and made of ceramic or hybrid materials exhibit load-bearing capacities not different from conventional restorations

Alexis Ioannidis, Sven Mühlemann, Mutlu Özcan, Jürg Hüsler, Christoph H.F. Hämmerle, Goran I. Benic

Abstract

The objective of this study was to test whether or not the load-bearing capacity of occlusal veneers bonded to enamel and made of ceramic or hybrid materials does differ from those of porcelain-fused-to-metal or lithium disilicate glass ceramic crowns. In 80 human molars occlusal enamel was removed without extending into the dentin in order to mimic substance defects caused by attrition. The restorations were digitally designed at a standardized thickness of either 0.5 mm or 1.0 mm. For each thickness, 4 test groups were formed each including a different restorative material: “0.5-ZIR”: 0.5 mm thick zirconia (Vita YZ HT); “1.0-ZIR”: 1.0 mm thick zirconia (Vita YZ HT); “0.5-LDC”: 0.5 mm thick lithium disilicate ceramic (IPS e.max Press); “1.0-LDC”: 1.0 mm thick lithium disilicate ceramic (IPS e.max Press); “0.5-HYC”: 0.5 mm thick PICN (Vita Enamic); “1.0-HYC”: 1.0 mm thick PICN (Vita Enamic); “0.5-COC”: 0.5 mm thick tooth shaded resin composite (Lava Ultimate) and “1.0-COC”: 1.0 mm thick tooth shaded resin composite (Lava ultimate). Each group consists of 10 specimens. Two additional groups of 10 specimens each were used as controls and exhibited conventional crown preparations. In one group the crowns were made of lithium-disilicate ceramic (“CLD”: IPS e.max CAD) and the other group consisted of porcelain-fused to metal crowns (“PFM”). All restorations were cemented onto the prepared teeth following the manufacturer's instruction of the corresponding luting cement. Subsequently, they were thermo-mechanically aged and then loaded until fracture. Load-bearing capacities (Fmax) between the groups were compared applying the Kruskal-Wallis test (p < 0.05) and pairwise group comparisons using the Dunn's method. Median values (and quartiles) for the load-bearing capacity amounted to (Fmax) 2′407 (1′670; 2′490) N for the CLD group and to 2′033 (1′869; 2′445) N for the PFM group. For the 0.5 mm thick restorations Fmax reached the highest median value in group 0.5-HYC 2′390 (1′355; 2′490) N, followed by 0.5-COC 2′200 (1′217; 2′492) N and 0.5-LDC 1′692 (1′324; 2′355) N. No results were obtained for group 0.5-ZIR due to the impracticability to fabricate ultra-thin specimens. The distribution of the values for the 1.0 mm thick restorations was 2′489 (2′426; 2′491) N for 1.0-COC, 2′299 (2′156; 2′490) N for 1.0-ZIR, 2′124 (1′245; 2′491) N for 1.0-HYC, and 1′537 (1′245; 1′783) N for 1.0-LDC. The differences of the medians between the test and the control groups did not reach statistical significance for the 0.5 mm thick specimens (KW: p = 0.6952 and p = 0.6986). Within the groups exhibiting 1.0 mm thickness, however, significant different medians were found: 1.0-LDC < 1.0-ZIR and 1.0-LDC < 1.0-COC (KW: p < 0.0209). Regarding their maximum load-bearing capacity, minimally invasive occlusal veneers made of ceramic and hybrid materials can be applied to correct occlusal tooth wear and thus replace conventional crown restorations.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Dental Erosion and Treatment · Dental Health and Care Utilization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Fracture resistance of ceramic and polymer-based occlusal veneer restorations10.1016/j.jmbbm.2017.06.013 ↗
2. Mechanical properties of resin-ceramic CAD/CAM restorative materials10.1016/j.prosdent.2015.04.016 ↗
3. Masticatory function--a review of the literature. 1. The form of the masticatory cycle10.1111/j.1365-2842.1975.tb00921.x ↗
4. Masticatory function - a review of the literature. III. Masticatory performance and efficiency10.1111/j.1365-2842.1976.tb00929.x ↗
5. The fracture resistance of a CAD/CAM Resin Nano Ceramic (RNC) and a CAD ceramic at different thicknesses10.1016/j.dental.2014.05.018 ↗
6. Mechanical properties and short-term in-vivo evaluation of yttrium-oxide-partially-stabilized zirconia10.1002/jbm.820230105 ↗
7. Characterization of a polymer-infiltrated ceramic-network material10.1016/j.dental.2014.02.019 ↗
8. An artificial oral environment for testing dental materials10.1109/10.133228 ↗
9. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
10. A comprehensive and conservative approach for the restoration of abrasion and erosion. Part II: clinical procedures and case report
11. Tooth structure removal associated with various preparation designs for anterior teeth10.1067/mpr.2002.124094 ↗
12. Tooth structure removal associated with various preparation designs for posterior teeth
13. Fracture strength of ultrathin occlusal veneer restorations made from CAD/CAM composite or hybrid ceramic materials10.1016/S1348-8643(15)00017-8 ↗
14. Mechanical properties of zirconia reinforced lithium silicate glass-ceramic10.1016/j.dental.2016.03.013 ↗
15. Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part I. Pressable and alumina glass-infiltrated ceramics10.1016/j.dental.2003.05.003 ↗
16. Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramics10.1016/j.dental.2003.05.002 ↗
17. Influence of preparation design and ceramic thicknesses on fracture resistance and failure modes of premolar partial coverage restorations10.1016/S0022-3913(13)60374-1 ↗
18. [An in vitro test procedure for evaluating dental restoration systems. 1. A computer-controlled mastication simulator]
19. Severe tooth wear: European consensus statement on management guidelines
20. Load-bearing properties of minimal-invasive monolithic lithium disilicate and zirconia occlusal onlays: finite element and theoretical analyses10.1016/j.dental.2013.04.004 ↗
21. Current status of zirconia restoration10.1016/j.jpor.2013.09.001 ↗
22. MMP inhibitors on dentin stability: a systematic review and meta-analysis10.1177/0022034514538046 ↗
23. Tooth wear: a systematic review of treatment options10.1016/j.prosdent.2014.01.018 ↗
24. Effect of three surface conditioning methods to improve bond strength of particulate filler resin composites10.1007/s10856-005-6442-4 ↗
25. Effect of surface conditioning methods on the microtensile bond strength of resin composite to composite after aging conditions10.1016/j.dental.2006.11.007 ↗
26. Clinical study on the reasons for and location of failures of metal-ceramic restorations and survival of repairs
27. Effect of thermal cycling on fracture toughness of CAD/CAM materials
28. Survival and complications of zirconia-based fixed dental prostheses: a systematic review10.1016/S0022-3913(12)60051-1 ↗
29. Influence of thermomechanical fatigue loading on the fracture resistance of all-ceramic posterior crowns
30. Fracture strength of lithium disilicate crowns compared to polymer-infiltrated ceramic-network and zirconia reinforced lithium silicate crowns10.1016/j.jmbbm.2017.06.025 ↗
31. A comparison of patterns of tooth wear with aetiological factors10.1038/sj.bdj.4805401 ↗
32. In vitro evaluation of a mechanical testing chewing simulator10.1016/j.dental.2008.09.010 ↗
33. Interpenetrating network ceramic-resin composite dental restorative materials10.1016/j.dental.2015.09.009 ↗
34. Biaxial flexural strength and indentation fracture toughness of three new dental core ceramics10.1016/S0022-3913(96)90297-8 ↗
35. Competition of fracture mechanisms in monolithic dental ceramics: flat model systems. Journal of biomedical materials research. Part B