journal article·2010-08

Effect of surface treatments on the fatigue life of titanium for biomedical applications

L. Pazos, P. Corengia, H. Svoboda

Publisher page

Abstract

Many surface treatments that are used in cementless and endosseous implants modify the topography and the roughness to increase the implant-bone contact area and thus favor bio-mechanical anchorage, shortening the period of osseointegration. Nevertheless, the effects that the surface treatments can have on the fatigue life of the material are not generally considered. In this sense, the superficial condition of the component is one of the features that affect the fatigue strength, specially the fatigue crack nucleation. The fatigue behaviour of annealed commercially pure titanium grade 4 was studied. The surface treatments used were acid etching, shot blasting and a dual treatment of blasting + acid etching. An as-machined surface condition was used as a reference. Topography, roughness, surface defects, microstructural changes and residual stresses were characterized in each case. Rotating-bending fatigue tests of each surface condition were conducted at room temperature with a frequency of 33 Hz. S-N curves and Basquin equations were obtained based on the results of these tests. Tested samples were also characterized to evaluate fatigue damage. The acid etching decreases the fatigue endurance, while the blasting and blasting + acid etching treatments showed a similar behaviour with respect to the reference condition. For acid etching, the modifications introduced (stress raisers) contributed to accelerate the nucleation of cracks. On the other hand, the treatments with a blasting stage besides generating stress raisers, introduced compressive residual stresses and superficial plastic deformation that tend to improve the fatigue endurance of the material.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · Bone Tissue Engineering Materials · Orthopaedic implants and arthroplasty

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (42)

Show source-provided references
1. Human-osteoblast proliferation and differentiation on grit-blasted and bioactive titanium for dental applications
2. Estimating the fatigue stress concentration factor of machined surfaces10.1016/S0142-1123(02)00012-9 ↗
3. Fatigue life prediction of machined components using finite element analysis of surface topography10.1016/j.ijfatigue.2005.07.031 ↗
4. Surface roughness characterization for fatigue life predictions using finite element analysis10.1016/j.ijfatigue.2008.05.020 ↗
5. ASTM Standard E112 · 2004
6. ASTM Standard E407 · 2007
7. ASTM Standard F67 · 2006
8. Surface treatments and roughness properties of Ti-based biomaterials10.1023/B:JMSM.0000042679.28493.7f ↗
9. Surface modification of titanium by etching in concentrated sulfuric acid10.1016/j.dental.2005.09.007 ↗
10. Surface roughness mediates its effects on osteoblasts via protein kinase A and phospholipase A210.1016/S0142-9612(99)00159-3 ↗
11. Visualisation of human plasma fibrinogen adsorbed on titanium implant surfaces with different roughness10.1016/S0039-6028(01)01303-6 ↗
12. The removal torque of titanium screw inserted in rabbit tibia treated by dual acid etching10.1016/S0142-9612(03)00218-7 ↗
13. Rough surfaces of titanium and titanium alloys for implants and prostheses
14. A role for surface topography in creating and maintaining bone at titanium endosseous implants10.1067/mpr.2000.111966 ↗
15. Cullity · 2001
16. Effect of surface roughness of the titanium alloy Ti–6Al–4V on human bone marrow cell response and on protein absorption10.1016/S0142-9612(00)00274-X ↗
17. Biomaterial osseointegration. Enhancement with biophysical stimulation
18. About the role of residual stresses and surface work hardening on fatigue ΔKth of a nitrided and shot peened low-alloy steel10.1016/j.surfcoat.2007.11.015 ↗
19. Ti based biomaterials, the ultimate choice for orthopaedic implants — a review10.1016/j.pmatsci.2008.06.004 ↗
20. The effect of shot blasting and heat treatment on the fatigue behavior of titanium for dental implant applications10.1016/j.dental.2006.03.003 ↗
21. Bone formation after 4 weeks around blood-plasma-modified titanium implants with varying surface topographies: an in vivo study10.1016/S0142-9612(02)00277-6 ↗
22. Quantitative and qualitative investigation of surface enlarged titanium and titanium alloy implants10.1034/j.1600-0501.1998.090101.x ↗
23. In vivo metallic biomaterials and surface modification10.1016/S0921-5093(99)00101-X ↗
24. Environmental effects on fatigue failure micromechanisms in titanium10.1016/S0921-5093(04)01018-4 ↗
25. Enhancement of fatigue and corrosion properties of pure Ti by sandblasting10.1016/j.msea.2006.04.024 ↗
26. Mechanism of creation of compressive residual stress by shot peening10.1016/S0142-1123(98)00002-4 ↗
27. Surface treatments of titanium dental implants for rapid osseointegration10.1016/j.dental.2006.06.025 ↗
28. Effect of surface structure on biomechanical properties and osseointegration
29. Biomechanical comparison of the sandblasted and acid-etched and the machined and acid-etched titanium surface for dental implants10.1002/jbm.10063 ↗
30. A comparison of the fatigue behavior of cast Ti–7.5Mo with c.p. titanium, Ti–6Al–4V and Ti–13Nb–13Zr alloys10.1016/j.biomaterials.2004.09.007 ↗
31. Response of MG63 osteoblast-like cells to titanium and titanium alloy is dependent on surface roughness and composition10.1016/S0142-9612(98)00144-6 ↗
32. Surface modification of titanium, titanium alloys, and related materials for biomedical applications10.1016/j.mser.2004.11.001 ↗
33. Titanium alloy in total joint replacement: a material science perspective10.1016/S0142-9612(97)00146-4 ↗
34. Mechanical biocompatibilities of titanium alloys for biomedical applications10.1016/j.jmbbm.2007.07.001 ↗
35. The influence of blasting and sterilization on static and time-related wettability and surface-energy properties of titanium surfaces10.1016/j.surfcoat.2007.12.021 ↗
36. Surface roughness and fatigue performance of commercially pure titanium and Ti-6Al-4V alloy after different polishing protocols10.1016/j.prosdent.2005.01.010 ↗
37. The effect on fatigue life of residual stress and surface hardness resulting from different cutting conditions of 0.45%C steel10.1016/j.ijmachtools.2004.08.002 ↗
38. Mechanical surface treatments on titanium, aluminum and magnesium alloys10.1016/S0921-5093(98)01168-X ↗
39. Residual stress distributions and their influence on fatigue lifetimes10.1016/S0142-1123(01)00133-5 ↗
40. Bone tissue response to commercially pure titanium implants blasted with fine and coarse particles of aluminium oxide
41. Torque and histomorphometric evaluation of c.p. titanium screws blasted with 25- and 75-μm-sized particles of Al2O310.1002/(SICI)1097-4636(199602)30:2<251::AID-JBM16>3.0.CO;2-P ↗
42. Fatigue crack initiation in high-purity titanium crystals10.1016/0142-1123(96)00086-2 ↗