journal article·2015-11

A statistical approach to understand the role of inclusions on the fatigue resistance of superelastic Nitinol wire and tubing

Scott W. Robertson, Maximilien Launey, Oren Shelley, Ich Ong, Lot Vien, Karthike Senthilnathan, Payman Saffari, Scott Schlegel, Alan R. Pelton

Publisher page

Abstract

Superelastic wires and diamond-shaped stent surrogates were manufactured from Nitinol rods and tubing, respectively, from five different mill product suppliers - Standard VAR, Standard VIM, Standard VIM+VAR, Process-Optimized VIM+VAR, and High-Purity VAR. High-cycle fatigue tests up to 10(7) cycles were conducted under tension-tension conditions for wires and bending conditions for diamonds. These materials were compared under both testing methods at 37°C with 6% prestrain and 3% mean strain (unloading plateau) with a range of alternating strains. The High-Purity VAR material outperformed all alloys tested with a measured 10(7)-fatigue alternating strain limit of 0.32% for wire and 1.75% for diamonds. Process-Optimized VIM+VAR material was only slightly inferior to the High Purity VAR with a diamond alternating bending strain limit of 1.5%. These two "second generation" Nitinol alloys demonstrated approximately a 2× increase in 10(7)-cycle fatigue strain limit compared to all of the Standard-grade Nitinol alloys (VAR, VIM, and VIM+VAR) that demonstrated virtually indistinguishable fatigue performance. This statistically-significant increase in fatigue resistance in the contemporary alloys is ascribed to smaller inclusions in the Process-Optimized VIM+VAR material, and both smaller and fewer inclusions in the High-Purity VAR Nitinol.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Shape Memory Alloy Transformations · Orthopaedic implants and arthroplasty · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. ASTM F136-13, Standard specification for wrought titanium–6aluminum–4vanadium ELI (Extra Low Interstitial) alloy for surgical implant applications (UNS R56401), Book of Standards Volume 13.01, Subcommittee F04.12, 2013.
2. ASTM F2004-05, Standard test method for transformation temperature of nickel–titanium alloys by thermal analysis, Book of Standards Volume 13.01, Subcommittee F04.15, 2005.
3. ASTM F2063-12, Standard specification for wrought nickel–titanium shape memory alloys for medical devices and surgical implants. ASTM Book of Standards Volume 13.01, Subcommittee F04.12, 2012.
4. ASTM F2082-06, Standard test method for determination of transformation temperature of nickel–titanium shape memory alloys by bend and free recovery, Book of Standards Volume 13.01, Subcommittee F04.15, 2006.
5. ASTM F2516-07e2, Standard test method for tension testing of nickel–titanium superelastic materials, ASTM Book of Standards Volume 13.2, Subcommmittee F04.15, 2007.
6. Effect of microstructure on the fatigue of hot-rolled and cold-drawn NiTi shape memory alloys10.1016/j.msea.2007.11.033 ↗
7. Hosmer · 1989
8. Bard recovery filter: evaluation and management of vena cava limb perforation, fracture, and migration10.1016/j.jvir.2008.09.032 ↗
9. Influence of microstructural purity on the bending fatigue behavior of VAR-melted superelastic Nitinol10.1016/j.jmbbm.2014.02.008 ↗
10. Nitinol fatigue investigation on Stent-finish specimens using tension–tension method10.1007/s11665-010-9792-0 ↗
11. Nitinol fatigue life for variable strain amplitude fatigue10.1007/s11665-012-0387-9 ↗
12. Macherauch · 2002
13. Nitinol fatigue: a review of microstructures and mechanisms
14. Fatigue and durability of Nitinol stents10.1016/j.jmbbm.2007.08.001 ↗
15. Rotary-bending fatigue characteristics of medical-grade Nitinol wire10.1016/j.jmbbm.2013.06.003 ↗
16. Development of the Z specimen for tensile–tensile, tensile–compression, compression–compression wire testing10.1007/s11665-010-9766-2 ↗
17. Impurity levels and fatigue lives of pseudoelastic NiTi shape memory alloys10.1016/j.actamat.2013.02.054 ↗
18. A fracture-mechanics-based approach to fracture control in biomedical devices manufactured from superelastic Nitinol tube10.1002/jbm.b.30840 ↗
19. Mechanical fatigue and fracture of Nitinol10.1179/1743280411Y.0000000009 ↗
20. Fatigue performance of Nitinol round wire with varying cold work reductions10.1007/s11665-009-9363-4 ↗
21. Prevalence and clinical impact of stent fractures after femoropopliteal stenting10.1016/j.jacc.2004.11.026 ↗
22. Tolomeo, D., Davidson, S., Santinoranout, M., 2000. Cyclic properties of superelastic Nitinol: design implications. In: Proceedings of the International Conference on Shape Memory and Superelastic Technologies. SMST. Pacific Grove, CA, USA, pp. 409–417.
23. Wick, A., et al., 2004. Bending fatigue characteristics of Nitinol. In: Proceedings of the ASM Materials & Processes for Medical Devices Conference. Minneapolis, MN, USA. ASM International. pp. 15–20.