Effects of heat treatment on the microstructure, residual stress, and mechanical properties of Co–Cr alloy fabricated by selective laser melting

Kyung-Ho Ko, Hyeon-Goo Kang, Yoon-Hyuk Huh, Chan-Jin Park, Lee-Ra Cho

Publisher page

Abstract

The mechanical properties and residual stress of dental Co-Cr-Mo (CCM) alloy depend on the manufacturing and post-processing methods, which affect the prognosis of dental prostheses. Two CCM alloys manufactured by casting and selective laser melting (SLM) were compared, and the effect of heat treatment temperature for CCM alloys manufactured by SLM method was evaluated. Specimens were fabricated by casting (Cast Co-Cr) and SLM (SLM Co-Cr). SLM Co-Cr specimens were heat treated at 750, 950, and 1150 °C to compare their properties. Microstructures were analyzed via scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy (EDS), and electron backscattered diffraction (EBSD), and the residual stress was measured via x-ray diffraction (XRD). Mechanical properties were evaluated by a Vickers hardness test and a tensile test; fractography was performed after this. The SLM Co-Cr group exhibited a decrease in porosity, grain size, increase in solid solution limit, and high residual stress compared to Cast Co-Cr; the ultimate tensile strength, yield strength, and hardness were also higher. The microstructures, residual stresses, and mechanical properties differed significantly depending on the heat treatment, and the strength and hardness showed a tendency inverse to that of the elongation. Type I residual stresses mostly decreased after 750 °C heat treatment, however type II and III residual stresses remained even after 1150 °C heat treatment. SLM presented superior mechanical properties to casting. Considering the reduction of tensile residual stress and increased ductility, CCM alloys should be heat treated at a temperature of 950 °C or higher.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · Dental materials and restorations

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. Physico-mechanical properties and prosthodontic applications of Co-Cr dental alloys: a review of the literature10.4047/jap.2014.6.2.138 ↗
2. Metallurgical and interfacial characterization of PFM Co-Cr dental alloys fabricated via casting, milling or selective laser melting10.1016/j.dental.2014.01.008 ↗
3. In vitro evaluation of the bond strength between various ceramics and cobalt-chromium alloy fabricated by selective laser sintering10.4047/jap.2015.7.4.312 ↗
4. Bang · 2021 · vol. 197 · 109221
5. Bartlett · 2019 · vol. 27 · 131
6. Determination of residual stress within complex-shaped coarse-grained cobalt–chromium biomedical castings10.1080/02670836.2016.1177304 ↗
7. Fatigue performance evaluation of selective laser melted Ti–6Al–4V10.1016/j.msea.2014.01.041 ↗
8. Fitzpatrick · 2005
9. In vitro biocompatibility of CoCrMo dental alloys fabricated by selective laser melting10.1016/j.dental.2014.02.008 ↗
10. Effect of heat-treatment temperature on microstructures and mechanical properties of Co–Cr–Mo alloys fabricated by selective laser melting10.1016/j.msea.2018.04.048 ↗
11. Fatigue strength of Co-Cr-Mo alloy clasps prepared by selective laser melting10.1016/j.jmbbm.2016.02.032 ↗
12. Does the material stiffness of novel high-performance polymers for fixed partial dentures influence their biomechanical behavior?10.11607/ijp.4940 ↗
13. Microstructures and mechanical properties of Co-Cr dental alloys fabricated by three CAD/CAM-Based processing techniques10.3390/ma9070596 ↗
14. Fatigue properties of removable partial denture clasps fabricated by selective laser melting followed by heat treatment10.1016/j.jmbbm.2019.06.010 ↗
15. Challenges of Co-Cr alloy additive manufacturing methods in dentistry-the current state of knowledge (systematic review)10.3390/ma13163524 ↗
16. Selective laser melting technique of Co-Cr dental alloys: a review of structure and properties and comparative analysis with other available techniques10.1111/jopr.12268 ↗
17. Radiographic evaluation of porosities in removable partial denture castings10.1016/S0022-3913(78)80095-X ↗
18. Fast prediction and validation of Part Distortion in selective laser melting10.1016/j.promfg.2015.09.042 ↗
19. Li · 2018 · vol. 71 · 348
20. Microstructure, mechanical property and metal release of As-SLM CoCrW alloy under different solution treatment conditions10.1016/j.jmbbm.2015.10.019 ↗
21. Texture, residual stress and structural analysis of thin films using a combined X-ray analysis10.1016/j.tsf.2003.10.150 ↗
22. Effects of thermal treatments on microstructure and mechanical properties of a Co-Cr-Mo-W biomedical alloy produced by laser sintering10.1016/j.jmbbm.2015.12.045 ↗
23. Rietveld refinement and estimation of residual stress in GDC–LSCF oxygen transport membrane ceramic composites10.1016/j.ceramint.2018.03.036 ↗
24. Methods of measuring residual stresses in components
25. Sames · 2016 · vol. 61 · 315
26. Effect of heat treatment on the microstructure and fatigue strength of CoCrMo alloys fabricated by selective laser melting10.1016/j.matlet.2019.02.085 ↗
27. Residual stress measurements on AISI 316L samples manufactured by selective laser melting10.1016/j.addma.2017.07.007 ↗
28. Effect of solution heat treatment on microstructure and mechanical properties of laser powder bed fusion produced cobalt-28chromium-6molybdenum10.1016/j.msea.2019.138511 ↗
29. Microstructure and tensile properties of iron parts fabricated by selective laser melting10.1016/j.optlastec.2013.09.017 ↗
30. Fracture strength of porcelain fused to metal crowns made of cast, milled or laser-sintered cobalt-chromium10.3109/00016357.2012.757650 ↗
31. Effect of heat treatment on the anisotropic microstructural and mechanical properties of Co-Cr-Mo alloys produced by selective laser melting10.1016/j.jmbbm.2019.103496 ↗
32. CoCr alloy processed by Selective Laser Melting (SLM): effect of Laser Energy Density on microstructure, surface morphology, and hardness10.1016/j.jmapro.2020.01.052 ↗
33. Effect of annealing procedure on the bonding of ceramic to cobalt-chromium alloys fabricated by rapid prototyping10.1016/j.prosdent.2017.05.009 ↗
34. Bend testing of wrought wire removable partial denture alloys10.1016/S0022-3913(96)90019-0 ↗
35. Effects of annealing on the microstructure and mechanical properties of selective laser melted AlSi7Mg alloy10.1016/j.msea.2018.10.047 ↗
36. Microscopic residual stresses analysis and multi-objective optimization for 3D woven composites
37. Microstructures and mechanical properties of dental Co-Cr-Mo-W alloys fabricated by selective laser melting at different subsequent heat treatment temperatures10.1007/s11661-020-05719-y ↗
38. Withers · 2007 · vol. 70 · 2211
39. Metal-ceramic bond strength of Co-Cr alloy fabricated by selective laser melting10.1016/j.jdent.2012.02.006 ↗
40. Yamanaka · 2019 · vol. 6 · 100281
41. Effects of chromium and nitrogen content on the microstructures and mechanical properties of as-cast Co-Cr-Mo alloys for dental applications10.1016/j.actbio.2012.03.024 ↗
42. Comparative analysis of the microstructures and mechanical properties of Co-Cr dental alloys fabricated by different methods10.1016/j.prosdent.2017.11.015 ↗
43. Microstructure evolution and mechanical properties improvement of selective laser melted Co-Cr biomedical alloys during subsequent heat treatments10.1016/j.jallcom.2020.155664 ↗