journal article·2022-01

Synergistic effects of hybrid (HA+Ag) particles and friction stir processing in the design of a high-strength magnesium matrix bio-nano composite with an appropriate texture for biomedical applications

Foroozan Yousefpour, Roohollah Jamaati, Hamed Jamshidi Aval

Publisher page

Abstract

In this work, the effects of hybrid (HA + Ag) particles and triple-pass friction stir processing on the microstructure, texture, hardness, and tensile behavior of magnesium matrix bio-nano composite were investigated. The results showed that the mean grain size of samples was in the range of 1-5 μm owing to the occurrence of dynamic recrystallization and suppression of grain growth by second phase particles. All samples exhibited uniform dispersion of particles in the magnesium matrix caused by triple-pass FSP. However, some agglomerations were visible in the microstructure of AZ91/nHA nanocomposite. The average grain size of the AZ91/nHA/smAg sample (1.4 μm) was smaller than that of the AZ91/nHA/mAg sample (2.1 μm), which was attributed to the formation of higher content of MgxAgy precipitates in the AZ91/nHA/smAg composite. By performing the FSP, the content of Mg17Al12 was significantly decreased due to the dissolution of beta into the alpha caused by the breakup effect of mechanical stirring and temperature increase of samples. The AZ91/nHA/smAg sample had the highest texture parameter for the {101‾1} orientation as the high corrosion resistance texture. This was due to the promoting the non-basal slip caused by the dissolution of smAg particles in the magnesium matrix. After the FSP, the microhardness distribution of AZ91, AZ91/nHA, AZ91/nHA/mAg, and AZ91/nHA/smAg samples tended to be uniform and the average hardness was improved owing to the fragmentation of beta particles, grain refinement, and homogeneous dispersion of second phase particles. Compared with the AZ91/nHA/mAg sample, an increase in ultimate tensile strength (291.7 MPa), and a decrease in total elongation (5.6%) and energy absorption (12.3 J/cm3) were observed in the AZ91/nHA/smAg sample due to the formation of a higher content of the silver-rich precipitates in the AZ91/nHA/smAg sample during cooling caused by the higher solubility of silver submicron particles. The fracture surfaces of all processed samples consisted of a large number of fine equiaxed dimples (ductile fracture) owing to the grain refinement and the presence of fine second phase particles.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Magnesium Alloys: Properties and Applications · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (56)

Show source-provided references
1. Bactericidal effect of silver-reinforced carbon nanotube and hydroxyapatite composites10.1177/0885328211431856 ↗
2. Development of aluminium-based composites reinforced with steel and graphite particles: structural, mechanical and wear characterization10.1016/j.jmrt.2018.04.019 ↗
3. Effects of Ti particles and T6 heat treatment on the microstructure and mechanical properties of A356 alloy fabricated by compocasting10.1016/j.msea.2021.141443 ↗
4. Microstructure, mechanical properties, and degradation of Mg-Ag alloy after equal-channel angular pressing10.1016/j.msec.2019.110543 ↗
5. Microstructure evolution and mechanical properties of a submerged friction-stir-processed AZ91 magnesium alloy10.1007/s10853-015-8887-2 ↗
6. Achieving ultrafine grain size in Mg–Al–Zn alloy by friction stir processing10.1016/j.scriptamat.2007.04.007 ↗
7. Effect of nano-HA content on the mechanical properties, degradation and biocompatible behavior of Mg-Zn/HA composite prepared by spark plasma sintering10.1016/j.matchar.2019.03.048 ↗
8. Mechanical properties and corrosion behavior of Mg–HAP composites10.1016/j.jmbbm.2014.07.014 ↗
9. Processing and mechanical characteristics of magnesium-hydroxyapatite metal matrix biocomposites10.1016/j.jmbbm.2016.12.023 ↗
10. The significance of texture parameters in phase analysis by X-ray diffraction10.1107/S0021889869006881 ↗
11. Synthesis and evaluation of magnesium/co-precipitated hydroxyapatite based composite for biomedical application10.1016/j.jmbbm.2021.104460 ↗
12. Antimicrobial silver-hydroxyapatite composite coatings through two-stage electrochemical synthesis10.1016/j.surfcoat.2016.03.010 ↗
13. In vitro corrosion-fatigue behavior of biodegradable Mg/HA composite in simulated body fluid10.1016/j.jma.2021.03.027 ↗
14. Deformation behavior of as-cast and as-extruded Mg97Zn1Y2 alloys during compression, as tracked by in situ neutron diffraction10.1016/j.ijplas.2018.08.001 ↗
15. Microstructure, mechanical property, bio-corrosion and cytotoxicity evaluations of Mg/HA composites10.1016/j.msec.2010.03.016 ↗
16. The microstructure, mechanical properties, corrosion performance and biocompatibility of hydroxyapatite reinforced ZK61 magnesium-matrix biological composite10.1016/j.jmbbm.2021.104759 ↗
17. Electrospun PCL/HA coated friction stir processed AZ31/HA composites for degradable implant applications10.1016/j.jmatprotec.2017.10.009 ↗
18. Development of ductile magnesium composite materials using titanium as reinforcement10.1016/S0925-8388(02)00413-9 ↗
19. Domination of volumetric toughening by silver nanoparticles over interfacial strengthening of carbon nanotubes in bactericidal hydroxyapatite biocomposite10.1016/j.msec.2013.09.034 ↗
20. In-vitro biomineralization and biocompatibility of friction stir additively manufactured AZ31B magnesium alloy-hydroxyapatite composites
21. The formation mechanism and bio-corrosion properties of Ag/HA composite conversion coating on the extruded Mg-2Zn-1Mn-0.5Ca alloy for bone implant application10.1016/j.surfcoat.2017.06.023 ↗
22. Fabrication of tungsten particles reinforced aluminum matrix composites using multi-pass friction stir processing: evaluation of microstructural, mechanical and electrical behavior10.1016/j.msea.2016.07.124 ↗
23. Fabrication of tungsten particles reinforced aluminum matrix composites using multi-pass friction stir processing: evaluation of microstructural, mechanical and electrical behavior10.1016/j.msea.2016.07.124 ↗
24. Mechanical, corrosion and biocompatibility behaviour of Mg-3Zn-HA biodegradable composites for orthopaedic fixture accessories10.1016/j.jmbbm.2017.11.030 ↗
25. The influence of bioactive hydroxyapatite shape and size on the mechanical and biodegradation behaviour of magnesium based composite10.1016/j.ceramint.2020.07.202 ↗
26. Effect of alloy composition, stacking fault energy, second phase particles, initial thickness, and measurement position on deformation texture development of nanostructured FCC materials fabricated via accumulative roll bonding process10.1016/j.msea.2014.01.020 ↗
27. Texture development in Al/Al2O3 MMCs produced by anodizing and ARB processes10.1016/j.msea.2011.01.056 ↗
28. Development of texture during ARB in metal matrix composite10.1179/1743284711Y.0000000073 ↗
29. Comparison of microparticles and nanoparticles effects on deformation texture of steel-based composite and nanocomposite fabricated by the ARB process10.1016/j.msea.2014.04.007 ↗
30. Surface metal matrix nano-composite of magnesium/hydroxyapatite produced by stir-centrifugal casting10.1016/j.surfcoat.2020.126654 ↗
31. Comparative property study on extruded Mg–HAP and ZM61–HAP composites10.1016/j.msea.2010.06.031 ↗
32. Antibacterial activity of silver nanoparticles: a surface science insight10.1016/j.nantod.2015.04.002 ↗
33. Fabrication of biodegradable HA/Mg-Zn-Ca composites and the impact of heterogeneous microstructure on mechanical properties, in vitro degradation and cytocompatibility10.1016/j.bioelechem.2019.05.001 ↗
34. Mechanical properties and degradation behavior of binary magnesium-silver alloy sheets10.1016/j.jpcs.2019.05.008 ↗
35. Effect of SiC nanoparticles on the microstructure and texture of friction stir welded AA2024/AA606110.1016/j.matchar.2019.04.020 ↗
36. Antioxidant and antibacterial hydroxyapatite-based biocomposite for orthopedic applications10.1016/j.msec.2018.02.014 ↗
37. Strength retention, corrosion control and biocompatibility of Mg–Zn–Si/HA nanocomposites10.1016/j.jmbbm.2019.103584 ↗
38. Manufacture of biodegradable magnesium alloy by high speed friction stir processing10.1016/j.jmapro.2018.09.019 ↗
39. Mechanical and corrosion behaviour of hydroxyapatite reinforced Mg-Sn alloy composite by squeeze casting for biomedical applications10.1016/j.jma.2019.05.010 ↗
40. Synthesis, phase stability of hydroxyapatite–silver composite with antimicrobial activity and cytocompatibility10.1016/j.ceramint.2014.03.075 ↗
41. Friction stir processing of magnesium–nanohydroxyapatite composites with controlled in vitro degradation behavior10.1016/j.msec.2014.03.004 ↗
42. Nano-hydroxyapatite reinforced AZ31 magnesium alloy by friction stir processing: a solid state processing for biodegradable metal matrix composites10.1007/s10856-013-5127-7 ↗
43. Evidence of a novel intermetallic Mg7Ag3 phase in Mg–Ag binary alloy system10.1107/S160057671800599X ↗
44. Effect of addition of mutually soluble and insoluble metallic elements on the microstructure, tensile and compressive properties of pure magnesium10.1016/j.msea.2011.09.066 ↗
45. Aging behavior of nano SiC particles reinforced AZ91D composite fabricated via friction stir processing10.1016/j.jallcom.2019.04.280 ↗
46. Development of multi-pass processed AA6082/SiCp surface composite using friction stir processing and its mechanical and tribology characterization
47. Mechanical properties and corrosion behaviour of AZ91D-HAP surface composites fabricated by friction stir processing10.1088/2053-1591/ab1ded ↗
48. Synthesis of silver–hydroxyapatite composite with improved antibacterial properties10.1016/j.vacuum.2018.03.015 ↗
49. Titanium alloy reinforced magnesium matrix composite with improved mechanical properties10.1016/j.scriptamat.2005.09.020 ↗
50. Solute segregation assisted nanocrystallization of a cold-rolled Mg–Ag alloy during annealing10.1016/j.scriptamat.2019.10.012 ↗
51. Nickel particle embedded aluminium matrix composite with high ductility10.1016/j.matlet.2009.12.030 ↗
52. Biodegradable Mg-Cu alloy implants with antibacterial activity for the treatment of osteomyelitis: in vitro and in vivo evaluations10.1016/j.biomaterials.2016.08.031 ↗
53. Microstructure and tensile properties of Ti6Al4V/AM60B magnesium matrix composite10.1016/j.jallcom.2005.04.175 ↗
54. Effect of traverse and rotational speeds on microstructure, texture, and mechanical properties of friction stir processed AZ91 alloy10.1016/j.matchar.2021.111235 ↗
55. Water-assisted crystallization of nanoporous tin oxide formed by anodic oxidation on cold sprayed tin coating10.1016/j.jallcom.2021.160207 ↗
56. Silver-hydroxyapatite composite coatings with enhanced antimicrobial activities through heat treatment10.1016/j.surfcoat.2017.06.013 ↗