journal article·2023-05

In-vitro performance of subtractively and additively manufactured resin-based molar crowns

Martin Rosentritt, Angelika Rauch, Sebastian Hahnel, Michael Schmidt

Publisher page

Abstract

Purpose To compare the in-vitro performance and wear behavior of additively or subtractively fabricated resin-based composite molar crowns for temporary and permanent application. Materials and methods Identical molar crowns (n = 8 per group) were manufactured from materials for temporary or permanent application (3x temporary additive fabrication, 3x additive permanent fabrication, 1x temporary subtractive fabrication, 1x permanent subtractive fabrication). All crowns were adhesively bonded (Calibra Universal, Dentsply Sirona, USA) on standardized resin-based composite molars (FDI 46, P Pro temporary Crown & Bridge). Thermal cycling and mechanical loading (2 × 3000 × 5°C/55 °C, 2min, H20 dist., 1.2 × 106 force 50N) were performed and fracture force was determined (v = 1 mm/min, Z010, Zwick, Germany). Mean wear, maximum wear, and roughness were investigated on polished (P1200) specimens (n = 8 per group, d = 8 mm) in a pin-on-block test (50N; 120000 cycles; 1.6Hz; H2O). Statistics were performed by using one-way ANOVA, Bonferroni post-hoc-tests, and Pearson-correlation (α = 0.05). Results All crowns survived TCML without failures. Fracture forces ranged from 1362.4 ± 182.4N to 2354.1 ± 373.3N for the additive temporary crowns, from 1680.4.4 ± 525.1N to 2601.6 ± 403.7N for the additive permanent crowns, and reached values of 2988.5 ± 604.7N for subtractive temporary crowns and 3092.0 ± 307.6 N for subtractive permanent crowns. Significant (p < 0.001) differences were identified between the various additively manufactured systems, but not for the subtractively fabricated systems (p = 0.673). Mean wear of the additive temporary crowns ranged between 114.5 ± 25.8 μm and 163.8 ± 21.4 μm without significant differences (p = 0.061). Mean wear of the additive permanent crowns ranged between 120.0 ± 27.5 μm and 171.3 ± 31.8 μm with significant differences (p = 0.004). No statistically significant differences were identified between temporary and permanent subtractively manufactured specimens, with mean wear ranging between 140.5 ± 51.1 μm and 176.6 ± 26.8 μm (p = 0.673). Maximum wear of additive temporary specimens ranged between 221.4.5 ± 53.3 μm and 322.1 ± 50.6 μm; significant differences were identified between the groups (p = 0.016). Maximum wear of additive permanent specimens ranged between 246.3 ± 47.3 μm and 337.4 ± 61.4 μm, and significant differences were identified between the groups (p = 0.006). Mean wear of the subtractive group (permanent and temporary) showed no differences in maximum wear from 277.9 ± 79.7.1 μm to 316.4 ± 58.1 μm (p = 0.288). Ra roughness ranged from 0.7 ± 0.2 μm to 3.6 ± 1.3 μm with significant differences (p < 0.001) and Rz reference between 65.9 ± 26.2 μm and 16.8 ± 6.3 μm. Conclusion Temporary and permanent molar crowns provided at least acceptable in-vitro performance and fracture force for clinical mid-term application. Laboratory wear stability of the resin-based materials appeared sufficient, but should be verified under clinical conditions.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Erosion and Treatment · Endodontics and Root Canal Treatments

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Comparison between direct chairside and digitally fabricated temporary crowns10.4012/dmj.2017-315 ↗
2. Assessment of effect of accelerated aging on interim fixed dental materials using digital technologies10.4047/jap.2022.14.6.360 ↗
3. Effect of printing layer thickness and postprinting conditions on the flexural strength and hardness of a 3D-printed resin10.1155/2022/8353137 ↗
4. Dependence of the survival of 3D-printed temporary materials on the filler content
5. Influence of different postcuring parameters on mechanical properties and biocompatibility of 3D printed crown and bridge resin for temporary restorations10.1016/j.jmbbm.2022.105127 ↗
6. Chairside CAD/CAM materials. Part 1: measurement of elastic constants and microstructural characterization10.1016/j.dental.2016.10.009 ↗
7. Effect of material thickness on the fracture resistance and failure pattern of 3D-printed composite crowns
8. Does artificial aging affect mechanical properties of CAD/CAM composite materials10.1016/j.jpor.2017.06.001 ↗
9. The occlusal precision of milled versus printed provisional crowns10.1016/j.jdent.2021.103924 ↗
10. Printable and machinable dental restorative composites for CAD/CAM application-comparison of mechanical properties, fractographic, texture and fractal dimension analysis10.3390/ma14174919 ↗
11. The effect of artificial aging on Martens hardness and indentation modulus of different dental CAD/CAM restorative materials10.1016/j.jmbbm.2018.06.028 ↗
12. Effects of the washing time and washing solution on the biocompatibility and mechanical properties of 3D printed dental resin materials10.3390/polym13244410 ↗
13. Physical and mechanical properties of 3D-printed provisional crowns and fixed dental prosthesis resins compared to CAD/CAM milled and conventional provisional resins: a systematic review and meta-analysis10.3390/polym14132691 ↗
14. In silico non-linear dynamic analysis reflecting in vitro physical properties of CAD/CAM resin composite blocks10.1016/j.jmbbm.2020.103697 ↗
15. 3D and 4D printing in dentistry and maxillofacial surgery: printing techniques, materials, and applications10.1016/j.actbio.2020.12.044 ↗
16. Influence of hydrolysis degradation of silane coupling agents on mechanical performance of CAD/CAM resin composites: in silico multi-scale analysis10.4012/dmj.2019-223 ↗
17. Quantitative evaluation of the degradation amount of the silane coupling layer of CAD/CAM resin composites by water absorption10.2186/jpr.JPR_D_21_00236 ↗
18. The impact of cement mixing and storage errors on the risk of failure of glass-ceramic crowns10.1007/s00784-008-0215-7 ↗
19. Polishing effects and wear performance of chairside CAD/CAM materials10.1007/s00784-018-2473-3 ↗
20. The potential of additive manufacturing technologies and their processing parameters for the fabrication of all-ceramic crowns: a review10.1111/jerd.12535 ↗
21. A review of dental CAD/CAM: current status and future perspectives from 20 years of experience10.4012/dmj.28.44 ↗
22. Short-term and long-term release of monomers from newly developed resin-modified ceramics and composite resin CAD-CAM blocks10.1016/j.prosdent.2019.01.012 ↗
23. Wear of 3D printed and CAD/CAM milled interim resin materials after chewing simulation10.4047/jap.2021.13.3.144 ↗
24. Influence of fused deposition method 3D printing on thermoelastic effect10.1007/s12206-019-1013-7 ↗
25. Evaluation of the mechanical properties and degree of conversion of 3D printed splint material10.1016/j.jmbbm.2020.104254 ↗
26. Strength-limiting damage and its mitigation in CAD-CAM zirconia-reinforced lithium-silicate ceramics machined in a fully crystallized state10.1016/j.dental.2020.09.012 ↗
27. Influence of resilient support of abutment teeth on fracture resistance of all-ceramic fixed partial dentures: an in vitro study
28. Approach for valuating the influence of laboratory simulation10.1016/j.dental.2008.08.009 ↗
29. Approach for valuating the significance of laboratory simulation10.1016/j.jdent.2008.09.001 ↗
30. Fracture force of CAD/CAM resin composite crowns after in vitro aging10.1007/s00784-019-03099-1 ↗
31. In-vitro performance of CAD/CAM crowns with insufficient preparation design10.1016/j.jmbbm.2018.10.002 ↗
32. Thermoanalytical investigations on the influence of storage time in water of resin-based CAD/CAM materials10.3390/biomedicines9121779 ↗
33. Resin-composite blocks for dental CAD/CAM applications10.1177/0022034514553976 ↗
34. Impact of the occlusal contact pattern and occlusal adjustment on the wear and stability of crowns10.1016/j.jdent.2022.104364 ↗
35. Wear behavior of materials for additive manufacturing after simulated occlusion of deciduous dentition10.1016/j.jmbbm.2022.105627 ↗
36. Influence of root embedment material and periodontal ligament simulation on fracture resistance tests10.1590/S1806-83242005000100003 ↗
37. 3D printing with polymers: challenges among expanding options and opportunities10.1016/j.dental.2015.09.018 ↗
38. Evaluation of mechanical and optical behavior of current esthetic dental restorative CAD/CAM composites10.1016/j.jmbbm.2015.10.004 ↗
39. Effect of molar preparation axial height on retention of adhesively-luted CAD-CAM ceramic crowns
40. Chairside CAD/CAM materials. Part 2: flexural strength testing10.1016/j.dental.2016.10.008 ↗
41. Fracture origin and crack propagation of CAD/CAM composite crowns by combining of in vitro and in silico approaches10.1016/j.jmbbm.2020.104083 ↗