Influence of minimal extended firing on dimensional, optical, and mechanical properties of crystalized zirconia-reinforced lithium silicate glass ceramic
Source abstract
Abstract
This study should evaluate the influence of extended firing on the dimension, optical properties and flexural strength of a fully crystalized zirconia-reinforced lithium-silicate ceramic (ZLS) for single tooth restorations. Methods 150 ZLS (Celtra Duo) and 30 lithium disilicate (LDS, IPS e.max CAD) specimens (17 × 4 × 1 mm) were milled in a standard device (Cerec MC XL). The ZLS specimens were distributed equally to five experimental groups (polished, standard firing [IFU], and three extended firings). LDS acted as a control group. The extended firings of ZLS addressed the first glaze firing (EF1) as well as the subsequent glaze firing (EF2) by a controlled overheating of +15 °C during the holding time. Color was measured with a digital spectrophotometer (Shadepilot), and dimensions with a digital calliper, before and after firing. A color change of ΔE ≥1.5 and a volume change of ±0.5% was regarded as clinical relevant. All specimens underwent a three-point-bending test to calculate flexural strength and Weibull statistics. Results The color change after firing of ZLS (ΔE value; mean = 1.06; SD = 0.53) exceeded the perceptible threshold of ΔE ≥1.5 in 20% of IFU (mean = 1.18) and EF1+2 (mean = 0.95), 23% of EF1 (mean = 1.11), and 10% of EF2 (mean = 0.99) specimens with no statistical difference between the experimental groups. In 80% of IFU, 63% of EF2, 56% of EF1, and 33% of EF1+2 vol. change after firing exceeded ±0.5%. Characteristic Weibull strength σ0 and modulus m of polished ZLS specimen was affected by firing in IFU (σ0 = 314.35 MPa; m = 5.81), EF1 (σ0 = 324.68 MPa; m = 5.67), EF2 (σ0 = 326.4 MPa; m = 7.24), and EF1+2 (σ0 = 357.15 MPa, m = 3.69). LDS revealed σ0 = 405.7 MPa; m = 8.04, and polished ZLS σ0 = 219.3 MPa; m = 8.9 with statistical significant difference of the flexural strength between all fired ZLS experimental groups towards "as polished" as well as LDS. Conclusion Firing of ZLS led to changes in dimensions, color, and Weibull modulus. Firing increases flexural strength, but minimal temperature extension also increases materials inhomogeneity and risk of failure. The findings call for further investigations towards firing behavior of ZLS and its clinical relevance for restorations.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Bone Tissue Engineering Materials · Endodontics and Root Canal Treatments
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Extended glaze firing on ceramics for hard machining: crack healing, residual stresses, optical and microstructural aspects10.1016/j.dental.2016.12.002 ↗
2. Extended glaze firing improves flexural strength of a glass ceramic10.1016/j.dental.2015.10.012 ↗
3. Machinability of CAD-CAM materials10.1016/j.prosdent.2016.09.022 ↗
4. Damage tolerance of indirect restorative materials (including PICN) after simulated bur adjustments10.1016/j.dental.2015.03.007 ↗
5. Grinding damage assessment for CAD-CAM restorative materials10.1016/j.dental.2016.12.004 ↗
6. Mechanical properties of zirconia reinforced lithium silicate glass-ceramic10.1016/j.dental.2016.03.013 ↗
7. Impact of machining on the flexural fatigue strength of glass and polycrystalline CAD/CAM ceramics10.1016/j.dental.2017.07.019 ↗
8. Microstructural and mechanical characterization of CAD/CAM materials for monolithic dental restorations10.1111/jopr.12964 ↗
9. Effect of crystallization firing on marginal gap of CAD/CAM fabricated lithium disilicate crowns10.1111/jopr.12638 ↗
10. Generic principles of crack-healing ceramics10.1007/s40145-012-0020-2 ↗
11. Porcelain veneering of titanium--clinical and technical aspects
12. Firing temperature accuracy of four dental furnaces
13. Influence of surface defects on the biaxial strength of a silicon nitride ceramic – increase of strength by crack healing10.1016/j.jeurceramsoc.2011.07.019 ↗
14. Early complications and performance of 327 heat-pressed lithium disilicate crowns up to five years10.4047/jap.2016.8.3.194 ↗
15. Perceptibility and acceptability thresholds for colour differences in dentistry10.1016/j.jdent.2013.11.017 ↗
16. Effect of the crystallization process on the marginal and internal gaps of lithium disilicate CAD/CAM crowns
17. Complete rehabilitation of compromised full dentitions with adhesively bonded all-ceramic single-tooth restorations: long-term outcome in patients with and without amelogenesis imperfecta10.1016/j.jdent.2017.12.011 ↗
18. The dependence of sintering parameters on the surface quality and roughness of ceramic veneered PFM-restorations10.4028/www.scientific.net/KEM.240-242.875 ↗
19. Laboratory and clinical reliability of two spectrophotometers
20. Survival rates of all-ceramic systems differ by clinical indication and fabrication method10.1016/j.jebdp.2009.11.013 ↗
21. Wear, strength, modulus and hardness of CAD/CAM restorative materials10.1016/j.dental.2016.08.222 ↗
22. Influence of CAD/CAM tool and material on tool wear and roughness of dental prostheses after milling10.1016/j.prosdent.2014.12.021 ↗
23. Microstrucural evolution and physical behavior of a lithium disilicate glass-ceramic10.1016/j.dental.2015.05.003 ↗
24. The miniaturisation of the 4‐point bend test10.1111/j.1460-2695.1997.tb01514.x ↗
25. The effect of ceramic thickness and number of firings on the color of two all-ceramic systems10.1016/S0022-3913(08)60156-0 ↗
26. Color difference thresholds in dentistry
27. Color stability of dental ceramics submitted to artificial accelerated aging after repeated firings10.1016/S0022-3913(08)60282-6 ↗
28. A systematic review of the survival and complication rates of all-ceramic and metal-ceramic reconstructions after an observation period of at least 3 years. Part I: single crowns10.1111/j.1600-0501.2007.01467.x ↗
29. A practical and systematic review of Weibull statistics for reporting strengths of dental materials10.1016/j.dental.2009.09.006 ↗
30. Microstructure characterization and SCG of newly engineered dental ceramics10.1016/j.dental.2016.03.018 ↗
31. Clinical survival of chair-side generated monolithic lithium disilicate crowns:10-year results10.1007/s00784-017-2271-3 ↗
32. Impact of crystallization firing process on the microstructure and flexural strength of zirconia-reinforced lithium silicate glass-ceramics10.1016/j.dental.2018.06.010 ↗
33. Shapiro · 1965
34. CAD/CAM ceramic restorative materials for natural teeth10.1177/0022034518779759 ↗
35. Chairside CAD/CAM materials. Part 2: flexural strength testing10.1016/j.dental.2016.10.008 ↗
36. Comparative study of flexural strength test methods on CAD/CAM Y-TZP dental ceramics10.1093/rb/rbv020 ↗
37. The effect of repeated firings on the color change of dental ceramics using different glazing methods10.4047/jap.2014.6.6.427 ↗