Degradation resistance of PVDF mesh in vivo in comparison to PP mesh
Source abstract
Abstract
Mesh implant has been applied in hernia repair and urogynecological reconstruction. Polypropylene (PP) is now the most widely used material for non-resorbable mesh implants. A degradation phenomenon of PP mesh, which is apparent on the mesh surface as cracking, flaking and peeling, was discovered in the 1990's. This phenomenon of mesh implant has drawn attention because of mesh-related litigations. Polyvinylidene fluoride (PVDF), due to its high biocompatible performance, has been used since 2003 as an alternative material for non-resorbable mesh implants. Till now, no such degradation phenomenon of PVDF mesh has been reported, although limited study on PVDF mesh is available. In this paper, we researched the degradation of PVDF meshes taking the degradation of PP mesh as a reference. The meshes analysed in this study were received from a previous animal experiment. To expose the surface of explanted meshes, a tissue removing method with protease was used and the result of this cleaning process was tested by X-ray Photoelectron Spectroscopy (XPS). The morphological condition of the mesh surface was compared using Scanning Electron Microscopy (SEM) and the chemical condition concerning degradation was analysed through Fourier Transform Infrared Spectroscopy (FTIR). The surface condition of PVDF mesh after 3-, 6-, 12- and 24-month implantation was illustrated and compared with two types of PP meshes. XPS revealed an absence of nitrogen, confirming the successful removal of tissue residues using protease. SEM results presented no notable morphological surface change of the PVDF mesh and progressive surface cracking processes over time of both types of PP meshes. FTIR spectra of the implanted PVDF meshes had no considerable difference from the spectrum of the pristine mesh, while FTIR spectra of both types of PP meshes had extra chemical functional groups (carbonyl (CO) and hydroxyl (-OH) groups) increasing with implantation time, indicating progressive degradation. This study highlights the morphological and chemical stability of the PVDF mesh and demonstrates that the PVDF mesh is more resistant to degradation in comparison to the other two types of PP meshes.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hernia repair and management · Aortic aneurysm repair treatments · Pelvic and Acetabular Injuries
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Foreign body reaction to biomaterials10.1016/j.smim.2007.11.004 ↗
2. Polypropylene as a reinforcement in pelvic surgery is not inert: comparative analysis of 100 explants10.1007/s00192-009-1021-8 ↗
3. Materials characterization of explanted polypropylene hernia meshes10.1002/jbm.b.30764 ↗
4. Inflammatory reaction as determinant of foreign body reaction is an early and susceptible event after mesh implantation
5. IDEAL in meshes for prolapse, urinary incontinence, and hernia repair10.1177/1553350612472987 ↗
6. Vitro study on the deterioration of polypropylene hernia repair meshes: deterioration OF polypropylene hernia meshes10.1002/jbm.b.34029 ↗
7. Oxidative stress and cardiovascular injury: Part II: animal and human studies10.1161/01.CIR.0000093661.90582.c4 ↗
8. Characterization of the degradation mechanisms of lysine-derived aliphatic poly(ester urethane) scaffolds10.1016/j.biomaterials.2010.08.108 ↗
9. A new and evolving paradigm for biocompatibility10.1002/term.4 ↗
10. Iakovlev, Vladimir V., Scott A. Guelcher, and robert Bendavid 2017 degradation of polypropylene in vivo: a microscopic analysis of meshes explanted from patients: degradation OF polypropylene IN VIVO. J. Biomed. Mater. Res. B Appl. Biomater. 105(2): 237–248.10.1002/jbm.b.33502 ↗
11. Vivo oxidative degradation of polypropylene pelvic mesh10.1016/j.biomaterials.2015.09.015 ↗
12. Adhesion formation of a polyvinylidenfluoride/polypropylene mesh for intra-abdominal placement in a rodent animal model10.1007/s00464-008-9923-y ↗
13. Comparison of long-term biocompability of PVDF and PP meshes10.3109/08941939.2011.589883 ↗
14. Polyvinylidene fluoride as a suture material: evaluation of comet tail-like infiltrate and foreign body granuloma10.1159/000371797 ↗
15. Laroche, Gaétan, Yves Marois, Erwin Schwarz, et al. 1995Polyvinylidene fluoride monofilament sutures: can they Be used safely for long-term anastomoses in the thoracic aorta? Artif. Organs 19(11): 1190–1199.10.1111/j.1525-1594.1995.tb02282.x ↗
16. Subcutaneous implants of polypropylene filaments10.1002/jbm.820100611 ↗
17. Mesh removal following transvaginal mesh placement: a case series of 104 operations10.1007/s00192-009-1050-3 ↗
18. A porous tissue engineering scaffold selectively degraded by cell-generated reactive oxygen Species10.1016/j.biomaterials.2014.01.026 ↗
19. Comparison of the in vivo behavior of polyvinylidene fluoride and polypropylene sutures used in vascular surgery10.1097/00002480-199805000-00015 ↗
20. Mohrig · 2010
21. Palleros · 2000
22. Degradation studies of some polymeric biomaterials: polypropylene (PP) and polyvinylidene difluoride (PVDF)10.4028/www.scientific.net/MSF.539-543.573 ↗
23. Sternschuss, Gina, Donald R. Ostergard, and hiren Patel 2012 post-implantation alterations of polypropylene in the human. J. Urol. 188(1): 27–32.10.1016/j.juro.2012.02.2559 ↗
24. Oxidation and degradation of polypropylene transvaginal mesh10.1080/09205063.2017.1279045 ↗
25. The failure of polypropylene surgical mesh in vivo10.1016/j.jmbbm.2018.08.041 ↗
26. Ţucureanu, Vasilica, Alina Matei, and andrei marius Avram 2016 FTIR spectroscopy for carbon family study. Crit. Rev. Anal. Chem. 46(6): 502–520.10.1080/10408347.2016.1157013 ↗
27. The myth: in vivo degradation of polypropylene-based meshes
28. Evaluation of dynamic creep properties of surgical mesh prostheses-uniaxial fatigue10.1002/jbm.b.31401 ↗
29. Comparison of mechanical properties of polyvinylidene fluoride and polypropylene monofilament sutures used for flexor tendon repair10.1054/jhsb.2000.0508 ↗
30. Microscopic mechanisms OF damage caused BY degradants
31. Human plasma ?2-macroglobulin promotesin vitro oxidative stress cracking of pellethane 2363-80a:in vivo andin vitro correlations10.1002/jbm.820270311 ↗
32. Central rupture and bulging of low-weight polypropylene mesh following recurrent incisional sublay hernioplasty10.1007/s10029-013-1197-1 ↗