Abstract
The study aims to evaluate the effect of finishing and polishing protocol after CAD/CAM grinding and surface treatments of bonding surface on the topographical characteristics and fatigue behavior of 4YSZ adhesively luted to an epoxy resin substrate. Ninety 4YSZ discs (IPS e.max ZirCAD MT, Ivoclar AG) (Ø = 10 mm, thickness = 1 mm) were obtained, submitted to in-lab simulation with a CAD/CAM system bur, and randomly allocated into six groups (n = 15) based on 'Surface condition' (with or without finishing and polishing) and 'Surface treatments' (no treatment, air abrasion with 45 μm aluminum oxide and glaze spray application). The surface roughness of all samples was measured, and the discs were luted with resin cement onto an epoxy resin substrate to be tested under cyclic fatigue (step-stress approach: 20 Hz, 5,000 cycles for piston accommodation in the first step, followed by 10,000 cycles per step with a step size of 100 N, starting at 100 N until failure). The results indicated that surface roughness (Ra and Rz) decreased in the groups with polishing and finishing protocol, with no significant differences between surface treatments in groups without finishing and polishing. The air abrasion groups (whit and without finishing and polishing) showed superior fatigue performance, comparable to no treatment with polishing and finishing. While the groups no treatment without finishing and polishing, treated with glaze spray without finishing and polishing and treated with glaze spray with finishing and polishing exhibited inferior fatigue behavior. In conclusion, while the finishing and polishing protocol can minimize defects and influence the fatigue behavior of 4YSZ, its effect is not significant when combined with surface treatments. The surface treatment, particularly air abrasion, plays a more decisive role in improving fatigue performance, proving to be the most effective approach.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Additive Manufacturing and 3D Printing Technologies · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Transient thermal stresses developed during speed sintering of 3 mol% yttria-stabilized tetragonal zirconia polycrystals10.1016/j.dental.2023.04.004 ↗
2. Load-bearing capacity under fatigue of bonded-yttria tetragonal zirconia polycrystals and -yttria-stabilized zirconia: effects of the viscosity of a dual-cured resin cement10.1016/j.jmbbm.2023.106233 ↗
3. The effect of extended glaze firing on the flexural fatigue strength of hard-machined ceramics10.1016/j.prosdent.2018.01.030 ↗
4. A 3-dimensional accuracy analysis of chairside CAD/CAM milling processes10.1016/j.prosdent.2014.05.012 ↗
5. Fatigue performance of fully-stabilized zirconia polycrystals monolithic restorations: the effects of surface treatments at the bonding surface10.1016/j.jmbbm.2020.103962 ↗
6. Surface treatments and its effects on the fatigue behavior of a 5% mol yttria partially stabilized zirconia material10.1016/j.jmbbm.2021.104543 ↗
7. In-lab simulation of CAD/CAM grinding and intaglio surface treatments of 4YSZ monolithic restorations: effect on its load-bearing capacity under fatigue10.1016/j.jmbbm.2022.105417 ↗
8. Grinding and polishing of the inner surface of monolithic simplified restorations made of zirconia polycrystals and lithium disilicate glass-ceramic: effects on the load-bearing capacity under fatigue of the bonded restorations: grinding and polishing on10.1016/j.jmbbm.2021.104833 ↗
9. Recent advances in dental zirconia: 15 years of material and processing evolution10.1016/j.dental.2024.02.026 ↗
10. The fracture resistance of a CAD/CAM Resin Nano Ceramic (RNC) and a CAD ceramic at different thicknesses10.1016/j.dental.2014.05.018 ↗
11. Phase transformation and subsurface damage in 3Y-TZP after sandblasting10.1016/j.dental.2013.03.005 ↗
12. Microstructural analysis and reliability of monolithic zirconia after simulated adjustment protocols10.1016/j.dental.2017.04.024 ↗
13. Influence of CAD-CAM diamond bur deterioration on surface roughness and maximum failure load of Y-TZP-based restorations
14. Cyclic fatigue vs static loading for shear bond strength test of lithium disilicate and dentin substrates: a comparison of resin cement viscosities10.1016/j.dental.2022.09.008 ↗
15. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
16. Fatigue strength of bilayered ceramics under cyclic loading as a function of core veneer thickness ratios10.1016/j.prosdent.2015.09.017 ↗
17. Impact of machining on the flexural fatigue strength of glass and polycrystalline CAD/CAM ceramics10.1016/j.dental.2017.07.019 ↗
18. Guilardi · 2020 · vol. 103
19. Fracture resistance of computer-aided design/computer-aided manufacturing-generated composite resin-based molar crowns10.1111/eos.12173 ↗
20. Perspectives on strength10.1016/0109-5641(95)80043-3 ↗
21. ADM guidance-ceramics: fatigue principles and testing10.1016/j.dental.2017.09.006 ↗
22. Fracture surface analysis of dental ceramics: clinically failed restorations
23. A study of the antagonist tooth wear, hardness, and fracture toughness of three different generations of zirconia10.5005/jp-journals-10015-2276 ↗
24. Effect of Al2O3 sandblasting particle size on the surface topography and residual compressive stresses of three different dental zirconia grades
25. Phase transformations and subsurface changes in three dental zirconia grades after sandblasting with various Al2O3 particle sizes
26. Effect of different surface treatment methods on bond strength of dental ceramics to dental hard tissues: a systematic review
27. Complete and partial contour zirconia designs for crowns and fixed dental prostheses: a clinical report10.1016/S0022-3913(11)60112-1 ↗
28. In vitro 2D and 3D roughness and spectrophotometric and gloss analyses of ceramic materials after polishing with different prophylactic pastes10.1016/j.prosdent.2020.05.040 ↗
29. Effect of air-particle abrasion protocols on the biaxial flexural strength, surface characteristics and phase transformation of zirconia after cyclic loading10.1016/j.jmbbm.2013.01.005 ↗
30. Effect of surface conditioning methods on the bond strength of luting cement to ceramics10.1016/S0109-5641(03)00019-8 ↗
31. High-versus low-viscosity resin cements: its effect on the load-bearing capacity under fatigue of a translucent zirconia10.1016/j.jmbbm.2023.105829 ↗
32. Mechanical reliability, fatigue strength and survival analysis of new polycrystalline translucent zirconia ceramics for monolithic restorations10.1016/j.jmbbm.2018.05.029 ↗
33. Fatigue behavior in water of Y-TZP zirconia ceramics after abrasion with 30μm silica-coated alumina particles10.1016/j.dental.2010.10.003 ↗
34. ADM guidance—ceramics: guidance to the use of fractography in failure analysis of brittle materials10.1016/j.dental.2017.03.004 ↗
35. Ceramic strengthening by tuning the elastic moduli of resin-based luting agents10.1016/j.dental.2017.01.002 ↗
36. Strengthening of porcelain provided by resin cements and flowable composites10.2341/15-025-L ↗
37. Three generations of zirconia: from veneered to monolithic. Part I
38. A brief review on fatigue test of ceramic and some related matters in Dentistry10.1016/j.jmbbm.2022.105607 ↗
39. Influence of glazed zirconia on dual-cure luting agent bond strength10.2341/10-220-L ↗
40. Evaluation of resin bond strength to yttria-stabilized tetragonal zirconia and framework marginal fit: comparison of different surface conditionings10.2341/12-269-L ↗
41. Accelerated loading frequency does not influence the fatigue behavior of polymer infiltrated ceramic network or lithium disilicate glass-ceramic restorations10.1016/j.jmbbm.2020.103905 ↗
42. Biaxial flexure tests of ceramic substrates
43. Trueness analysis of zirconia crowns fabricated with 3-dimensional printing10.1016/j.prosdent.2018.04.012 ↗
44. Influence of alumina air-abrasion for highly translucent partially stabilized zirconia on flexural strength, surface properties, and bond strength of resin cement10.1590/1678-7757-2019-0371 ↗
45. Making yttria-stabilized tetragonal zirconia translucent10.1016/j.dental.2014.08.375 ↗
46. Effect of sandblasting on the long‐term performance of dental ceramics10.1002/jbm.b.30097 ↗
47. Does the bond strength of highly translucent zirconia show a different dependence on the airborne-particle abrasion parameters in comparison to conventional zirconia?10.1016/j.jpor.2019.04.008 ↗
48. CAD/CAM machining vs pre-sintering in-lab fabrication techniques of Y-TZP ceramic specimens: effects on their mechanical fatigue behavior10.1016/j.jmbbm.2017.03.013 ↗
49. Fatigue strength of yttria-stabilized zirconia polycrystals: effects of grinding, polishing, glazing, and heat treatment10.1016/j.jmbbm.2017.06.016 ↗