Fracture load of ultrathin occlusal veneers: Effect of thickness and surface conditioning
Source abstract
Abstract
Objective This in-vitro study is planned to analyze the effect of different thicknesses of ceramic occlusal veneers and different surface treatments on fracture resistance. Materials and methods A total of 48 sound mandibular molars are anatomically prepared from the occlusal surface with two different thicknesses (1.0 and 0.5 mm). CAD/CAM zirconia-reinforced glass ceramic blocks (Vita Suprinity) are used for fabricating occlusal veneers. The teeth are randomly divided into two primary groups A and B (n=24) according to occlusal veneer thickness. Each group is subdivided according to surface conditioning into three equal subgroups (n=8)-subgroup HF: etching with hydrofluoric acid and ceramic primer application; subgroup APF: etching with acidulated phosphate fluoride and ceramic primer application; subgroup EP: conditioning with etch and prime only. Dual-cure adhesive resin cement (Multilink Automix) is utilized to adhesively bond the veneers. All specimens are subjected to 240,000 cycles of dynamic load aging prior to the fracture resistance test. The fracture resistance is measured in Newton (N). The Failure mode patterns are analyzed and categorized using a scanning electron microscope (SEM). The results are analyzed using a two-way ANOVA with Bonferroni's Post-Hoc test, followed by a one-way ANOVA for each factor. That is in addition to one-way ANOVA for surface treatment under each thickness, each followed by Bonferroni's Post-Hoc test. Then, a T-test is used to compare the two thicknesses under each surface treatment. All tests are set at 0.05 significance level. Results The two-way ANOVA test revealed that restoration thickness and surface treatment both significantly affect the fracture resistance values (p<0.05). The highest fracture resistance mean (2672±216N) is obtained from HF at 1.0 mm thickness, while the lowest mean (2104±299N) is obtained from APF at 0.5 mm thickness. Conclusion All test groups, regardless of thickness, demonstrated fracture resistance values that exceeded both normal and parafunctional bite forces. The veneers that bonded after hydrofluoric acid etching followed by ceramic primer application showed more favourable fracture patterns.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Dental Research and COVID-19 · Endodontics and Root Canal Treatments
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (64)
Show source-provided references
1. Fracture resistance of ceramic and polymer-based occlusal veneer restorations10.1016/j.jmbbm.2017.06.013 ↗
2. Influence of thermomechanical fatigue on the fracture strength of CAD-CAM-fabricated occlusal veneers10.1016/j.prosdent.2018.07.019 ↗
3. Laboratory study of micro-shear bond strength of two resin cements to leucite ceramics using different ceramic primers10.5005/jp-journals-10024-2357 ↗
4. Influence of material type, thickness and storage on fracture resistance of CAD/CAM occlusal veneers10.1016/j.jmbbm.2021.104485 ↗
5. Effect of different computer-aided design/computer-aided manufacturing (CAD/CAM) materials and thicknesses on the fracture resistance of occlusal veneers10.2341/17-131-L ↗
6. Fracture load of composite resin and feldspathic all-ceramic CAD/CAM crowns10.1016/j.prosdent.2005.11.014 ↗
7. Fracture strength of all-ceramic crowns luted using two bonding methods10.1016/j.prosdent.2003.12.005 ↗
8. Influence of cyclic loading and luting agents on the fracture load of two all-ceramic crown systems10.1016/j.prosdent.2004.09.002 ↗
9. Acid etching as surface treatment method for luting of glass-ceramic restorations, part 1: acids, application protocol and etching effectiveness10.3889/oamjms.2018.147 ↗
10. Influence of ceramic thickness and ceramic materials on fracture resistance of posterior partial coverage restorations10.2341/12-459-L ↗
11. Zirconia-reinforced lithium silicate crowns: effect of thickness on survival and failure mode10.1016/j.dental.2019.04.007 ↗
12. Strength and fracture pattern of monolithic CAD/CAM-generated posterior crowns10.1016/j.dental.2005.02.007 ↗
13. Effect of different acid treatments on a porcelain surface10.1046/j.1365-2842.2001.00626.x ↗
14. Current aspects on bonding effectiveness and stability in adhesive dentistry10.1111/j.1834-7819.2011.01294.x ↗
15. Dynamic fatigue and fracture resistance of non-retentive all-ceramic full-coverage molar restorations. Influence of ceramic material and preparation design10.1016/j.dental.2010.01.011 ↗
16. Influence of adhesive type and placement technique on postoperative sensitivity in posterior composite restorations10.2341/16-010-C ↗
17. Microstructure, composition, and etching topography of dental ceramics
18. Effect of ceramic surface treatment on tensile bond strength to a resin cement
19. Novel ceramic primer vs. conventional treatment methods: effects on roughness and bond strength of all-ceramic restorations
20. Tooth structure removal associated with various preparation designs for posterior teeth
21. Self-etching ceramic primer versus hydrofluoric acid etching: etching efficacy and bonding performance10.1016/j.jpor.2017.06.002 ↗
22. Mechanical properties of zirconia reinforced lithium silicate glass-ceramic10.1016/j.dental.2016.03.013 ↗
23. Influence of thickness and surface conditioning on fracture resistance of occlusal veneer10.1186/s12903-023-02932-0 ↗
24. Influence of acid concentration and etching time on composite cement adhesion to lithium-silicate glass ceramics
25. Effect of tooth preparation design on fracture resistance of zirconia-reinforced lithium silicate overlays10.1111/jopr.13160 ↗
26. Statistical power analyses using G*Power 3.1: tests for correlation and regression analyses10.3758/BRM.41.4.1149 ↗
27. Posterior minimally invasive full-veneers: effect of ceramic thicknesses, bonding substrate, and preparation designs on failure-load and -mode after fatigue10.1111/jerd.12861 ↗
28. Marginal discrepancies and leakage of all-ceramic crowns: influence of luting agents and aging conditions
29. Influence of preparation design and ceramic thicknesses on fracture resistance and failure modes of premolar partial coverage restorations10.1016/S0022-3913(13)60374-1 ↗
30. Effect of microstructure on the mechanical properties of lithium disilicate glass-ceramics10.1016/j.jmbbm.2018.02.032 ↗
31. Indirect restorations for severe tooth wear: fracture risk and layer thickness10.1016/j.jdent.2013.10.003 ↗
32. Relevance of in vitro tests of adhesive and composite dental materials. A review in 3 parts. Part 3: in vitro tests of adhesive systems
33. Microtensile bond strength test and failure analysis to assess bonding characteristics of different adhesion approaches to ground versus unground enamel10.1590/S0103-64402011000200006 ↗
34. Effect of preparation design on the fracture behavior of ceramic occlusal veneers in maxillary premolars10.1016/j.jdent.2020.103346 ↗
35. Ultra-thin occlusal veneers bonded to enamel and made of ceramic or hybrid materials exhibit load-bearing capacities not different from conventional restorations10.1016/j.jmbbm.2018.09.041 ↗
36. Fracture strength of CAD/CAM composite and composite-ceramic occlusal veneers10.1016/j.jpor.2014.01.001 ↗
37. Effect of hydrofluoric acid surface treatments on surface roughness and three-point flexural strength of suprinity ceramic
38. Severe tooth wear: European consensus statement on management guidelines
39. Aspects of silane coupling agents and surface conditioning in dentistry: an overview10.1016/j.dental.2012.02.009 ↗
40. The case for moderate "guided prep" indirect porcelain veneers in the anterior dentition. The pendulum of porcelain veneer preparations: from almost no-prep to over-prep to no-prep
41. Fatigue failure load of two resin-bonded zirconia-reinforced lithium silicate glass-ceramics: effect of ceramic thickness10.1016/j.dental.2018.03.004 ↗
42. Lithium disilicate restorations fatigue testing parameters: a systematic review10.1111/jopr.12376 ↗
43. Color match of machinable lithium disilicate ceramics: effects of foundation restoration10.1016/j.prosdent.2013.09.004 ↗
44. Bonding effectiveness of luting composites to different CAD/CAM materials
45. Clinical outcomes of lithium disilicate single crowns and partial fixed dental prostheses: a systematic review10.1016/j.prosdent.2014.01.005 ↗
46. Different surface treatment strategies on etchable CAD-CAM materials: Part II-Effect on the bond strength
47. Ceramic surface treatment with a single-component primer: resin adhesion to glass ceramics
48. Effect of etching with distinct hydrofluoric acid concentrations on the flexural strength of a lithium disilicate-based glass ceramic10.1002/jbm.b.33619 ↗
49. Bonding to silicate ceramics: conventional technique compared with a simplified technique
50. Approach for valuating the influence of laboratory simulation10.1016/j.dental.2008.08.009 ↗
51. Resin-matrix ceramics for occlusal veneers: effect of thickness on reliability and stress distribution10.1016/j.dental.2020.11.002 ↗
52. Influence of restoration thickness and dental bonding surface on the fracture resistance of full-coverage occlusal veneers made from lithium disilicate ceramic10.1016/j.dental.2015.04.017 ↗
53. Influence of the preparation design on the survival probability of occlusal veneers10.1016/j.dental.2022.02.003 ↗
54. Shen · 2022
55. New single-bottle ceramic primer: 6-month case report and laboratory performance10.5005/jp-journals-10024-1977 ↗
56. CAD/CAM ceramic restorative materials for natural teeth10.1177/0022034518779759 ↗
57. The effect of hydrofluoric acid concentration on the bond strength and morphology of the surface and interface of glass ceramics to a resin cement10.2341/14-133-L ↗
58. Posterior indirect adhesive restorations: updated indications and the Morphology Driven Preparation Technique
59. Comparison between hydrofluoric acid and single-component primer as conditioners on resin cement adhesion to lithium silicate and lithium disilicate glass ceramics10.3390/ma14226776 ↗
60. Enamel and dentin bond strengths of a new self-etch adhesive system10.1111/j.1708-8240.2011.00465.x ↗
61. Influence of various bonding techniques on the fracture strength of thin CAD/CAM-fabricated occlusal glass-ceramic veneers10.1016/j.jmbbm.2017.08.016 ↗
62. Biomimetic aspects of restorative dentistry biomaterials10.3390/biomimetics5030034 ↗
63. Load capacity of occlusal veneers of different restorative CAD/CAM materials under lateral static loading10.1016/j.jmbbm.2020.104290 ↗
64. Comparison of fracture load and surface wear of microhybrid composite and ceramic occlusal veneers10.1111/jopr.13156 ↗