journal article·2025-12Open access

Impact of different post-polymerization protocols on the material properties of three printed dental resins

Sophie Gekle, Felicitas Mayinger, Ursula Kreitmair, Marcel Reymus, Moritz Hoffmann, Bogna Stawarczyk

Abstract

To investigate the influence of different post-polymerization protocols (PP) on polymerization depth and resultant degree of conversion (DC), Martens hardness (HM), flexural strength (FS) and elastic modulus (EM) of 3D-printed specimens with and without aging regimes. Specimens of a specific geometry (N = 720) were 3D printed from two resins for permanent applications (VAR=Varseo Smile Crown plus , BEGO Medical; CRO= Crowntec, Saremco Dental), and one resin for temporary applications (FRE=Freeprint temp, Detax). They underwent five PP's, divided into three LED-groups (PP 1: 385 nm, 76 mW/cm 2 , 180 s; PP 2: 400 nm, 77 mW/cm 2 , 180 s; PP 3: 460 nm, 49 mW/cm 2 , 180 s) and two flash curing groups (PP 4: 37 mW/cm 2 , ten flashes per second, pulse duration 100 μs, curing period 2000 flashes/200 ms; PP 5: 90 mW/cm 2 , ten flashes per second, pulse duration 100 μs, curing period 2000 flashes/200 ms). DC, HM, FS and EM were tested initially and after thermal cycling (10.000x, 5/55 °C) and within three different depths (0 mm, 2 mm, 4 mm). Data were analyzed with Kolmogorov-Smirnov, Kruskal-Wallis, Mann-Whitney-U test, Wilcoxon signed-rank test and Spearman's correlation (p < 0.05). PP 5 consistently showed high values for both aging regimes, while PP 3 presented the lowest results. Artificial aging increased the properties for most groups, some decreased. For DC 25/30 PP-groups and HM 27/30 PP-groups showed higher values for 0 mm depths in comparison with 2 mm and 4 mm depths. Post-polymerization enhances the properties of the tested specimens intended for fixed dental prostheses (FDPs). PP 5 is recommended because it consistently resulted in highest DC, HM, FS, and EM across most groups, especially when combined with depths of 0 mm for DC and HM. Depths of 2 mm and 4 mm mostly resulted in lower values. Among LED groups, wavelengths of 385 nm and 400 nm are recommended for all materials, while wavelength of 460 nm seems not advisable. • PP 5 consistently yielded in high values for both aging regimes. • PP 3 consistently showed lowest results. • Artificial aging increased the properties for most groups, some decreased. • For DC 25/30 PP-groups and HM 27/30 PP-groups showed higher values for 0 mm depths in comparison with 2 mm and 4 mm depths.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Additive Manufacturing and 3D Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Marginal adaptation and fracture resistance of 3D-printed and CAD/CAM-milled definitive resin matrix ceramic crowns
2. Effects of postcuring temperature on the mechanical properties and biocompatibility of three-dimensional printed dental resin material10.3390/polym13081180 ↗
3. Influence of different postcuring parameters on mechanical properties and biocompatibility of 3D printed crown and bridge resin for temporary restorations10.1016/j.jmbbm.2022.105127 ↗
4. Comparing the mechanical properties of pressed, milled, and 3D-printed resins for occlusal devices10.1016/j.prosdent.2019.10.024 ↗
5. Fracture resistance of additively or subtractively manufactured resin-based definitive crowns: effect of restorative material, resin cement, and cyclic loading10.1016/j.dental.2024.05.020 ↗
6. Influence of different post-processing methods on the dimensional accuracy of 3D-printed photopolymers for dental crown applications - a systematic review10.1016/j.jmbbm.2023.106314 ↗
7. Additive manufacturing by digital light processing: a review
8. Resin composite—State of the art10.1016/j.dental.2010.10.020 ↗
9. The effect of resin formulation on the degree of conversion and mechanical properties of dental restorative resins10.1002/jbm.820200111 ↗
10. Factors affecting flexural strength of 3D-printed resins: a systematic review10.1111/jopr.13640 ↗
11. Water sorption, solubility, and translucency of 3D-Printed denture base resins10.3390/dj10030042 ↗
12. Raman spectroscopy as spectral tool for assessing the degree of conversion after curing of two resin-based materials used in restorative dentistry10.3390/diagnostics12081993 ↗
13. The effect of artificial aging on martens hardness and indentation modulus of different dental CAD/CAM restorative materials10.1016/j.jmbbm.2018.06.028 ↗
14. Effects of post-processing parameters on 3D-Printed dental appliances: a review10.3390/polym16192795 ↗
15. Physical and mechanical properties of 3D-Printed provisional crowns and fixed dental prosthesis resins compared to CAD/CAM milled and conventional provisional resins: a systematic review and meta-analysis10.3390/polym14132691 ↗
16. 3D/4D printing of polymers: fused deposition modelling (FDM), selective laser sintering (SLS), and stereolithography (SLA)10.3390/polym13183101 ↗
17. Effects of post-curing light intensity on the mechanical properties and three-dimensional printing accuracy of interim dental material10.3390/ma15196889 ↗
18. Three-body wear of 3D printed temporary materials10.1016/j.dental.2019.10.005 ↗
19. The effect of filler loading and morphology on the mechanical properties of contemporary composites10.1067/mpr.2002.125179 ↗
20. Effects of post-curing time on the mechanical and color properties of three-dimensional printed crown and bridge materials10.3390/polym12112762 ↗
21. Post-polymerization of three-dimensional printing resin using a dental light curing unit10.1016/j.jds.2023.07.028 ↗
22. Effect of different post-curing methods on the degree of conversion of 3D-Printed resin for models in dentistry10.3390/polym16040549 ↗
23. The photoinitiators used in resin based dental Composite-A review and future perspectives10.3390/polym13030470 ↗
24. Evaluating the accuracy (trueness and precision) of interim crowns manufactured using digital light processing according to post-curing time: an in vitro study10.4047/jap.2021.13.2.89 ↗
25. Photoinitiator type and applicability of exposure reciprocity law in filled and unfilled photoactive resins10.1016/j.dental.2010.09.011 ↗
26. Postpolymerization of a 3D-printed denture base polymer: impact of post-curing methods on surface characteristics, flexural strength, and cytotoxicity10.1016/j.jdent.2021.103856 ↗
27. Are polywave light-emitting diodes more effective than monowave ones in the photoactivation of resin-based materials containing alternative photoinitiators? A systematic review10.1016/j.jmbbm.2023.105905 ↗
28. Temporary 3D printed fixed dental prosthesis materials: impact of post printing cleaning methods on degree of conversion as well as surface and mechanical properties10.11607/ijp.7048 ↗
29. Manufacturing accuracy, intaglio surface adaptation, and survival of additively and subtractively manufactured definitive resin crowns after cyclic loading: an in vitro study10.11607/ijp.8976 ↗
30. Influence of the rinsing postprocessing procedures on the manufacturing accuracy of vat-polymerized dental model material10.1111/jopr.13288 ↗
31. Effects of printing orientation and artificial ageing on martens hardness and indentation modulus of 3D printed restorative resin materials10.1016/j.dental.2024.05.005 ↗
32. Evaluation of the mechanical properties and degree of conversion of 3D printed splint material10.1016/j.jmbbm.2020.104254 ↗
33. Influence of different postpolymerization strategies and artificial aging on hardness of 3D-Printed resin materials: an in vitro study10.11607/ijp.6634 ↗
34. In vitro study on the influence of postpolymerization and aging on the martens parameters of 3D-printed occlusal devices10.1016/j.prosdent.2019.12.026 ↗
35. 3D-printed material for temporary restorations: impact of print layer thickness and post-curing method on degree of conversion
36. Refractive index mismatch and monomer reactivity influence composite curing depth10.1177/154405910808700115 ↗
37. The influence of filler load in 3D printing resin-based composites10.1016/j.dental.2024.05.016 ↗
38. Zguris · 2016 · 1