Increasing the fatigue strength of laser-powder bed fusion manufactured Ti6Al4V hip stems by means of appropriate post-treatments

Stefan Schroeder, Jens Gibmeier, Phuong Thao Mai, Maximilian C.M. Fischer, Moritz M. Innmann, Tobias Renkawitz, J. Philippe Kretzer

Abstract

Due to the lower fatigue resistance of LPBF manufactured Ti6Al4V alloy compared to wrought material, hip stems are still manufactured conventionally, despite the advantages of patient-specific joint replacements. Therefore, the aim of the study was the investigation of appropriate post-treatments to increase the fatigue resistance of LPBF manufactured Ti6Al4V alloy using a four-point bending setup and a Locati-test. The results showed that only a combination of a hot isostatic pressing process and a sufficient surface treatment can lead to similar fatigue results as wrought material. Thereby, machining, deep rolling and shot peening turned out to be suitable surface treatments. For complex geometries like hip stems, shot peening is the most sufficient surface treatment. A combined surface treatment of shot peening and polishing led to similar fatigue results as the shot peening process alone. It can be followed that a combination of shot peening with a previous hot isostatic pressing process leads to satisfying fatigue results comparable to the wrought material and can be applied on complex geometries like hip stems. In addition, shoulder and neck area of a hip stem can be polished after the HIP process and the shot peening procedure without any reduction in fatigue strength. • HIP alone after PFB-LB did not lead to sufficient fatigue results • Surface treatments alone after PFB-LB did not lead to sufficient fatigue results • Turning, deep rolling and shot peening after HIP led to sufficient fatigue results • Compressive residual stresses have higher impact on fatigue than reduced roughness • Shot peening after HIP could be used for PFB-LB manufactured hip implants
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Engineering Technology and Methodologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (55)

Show source-provided references
1. Fatigue behaviour of PBF additive manufactured TI6AL4V alloy after shot and laser peening10.1016/j.ijfatigue.2021.106536 ↗
2. Effect of HIP post-processing at 850 °C/200 MPa in the fatigue behavior of Ti-6Al-4V alloy fabricated by Selective Laser Melting10.1016/j.ijfatigue.2022.107097 ↗
3. On the effect of deep-rolling and laser-peening on the stress-controlled low- and high-cycle fatigue behavior of Ti–6Al–4V at elevated temperatures up to 550°C10.1016/j.ijfatigue.2012.03.008 ↗
4. Implant surface characteristics and their effect on osseointegration10.1038/sj.bdj.2015.171 ↗
5. The effect of post-sintering treatments on the fatigue and biological behavior of Ti-6Al-4V ELI parts made by selective laser melting10.1016/j.jmbbm.2017.03.024 ↗
6. Hot isostatic pressing (HIP) to achieve isotropic microstructure and retain as-built strength in an additive manufacturing titanium alloy (Ti-6Al-4V)10.1016/j.matlet.2019.126690 ↗
7. Hip joint contact forces during stumbling10.1007/s00423-003-0434-y ↗
8. Metallic implant biomaterials10.1016/j.mser.2014.10.001 ↗
9. Microstructure and mechanical properties of open-cell porous Ti-6Al-4V fabricated by selective laser melting10.1016/j.jallcom.2017.04.190 ↗
10. Three-dimensional printed implant for reconstruction of pelvic bone after removal of giant chondrosarcoma: a case report
11. Osseointegration of retrieved 3D-printed, off-the-shelf acetabular implants10.1302/2046-3758.107.BJR-2020-0462.R1 ↗
12. Dall'Ava · 2019
13. Fatigue performance evaluation of selective laser melted Ti–6Al–4V10.1016/j.msea.2014.01.041 ↗
14. Is there a need of custom-made prostheses for total hip arthroplasty? Gait analysis, clinical and radiographic analysis of customized femoral components10.1007/s00402-008-0717-4 ↗
15. Ueber die Berührung fester elastischer Körper10.1515/crll.1882.92.156 ↗
16. Custom made monoflange acetabular components for the treatment of paprosky type III defects10.3390/jpm11040283 ↗
17. Effects of laser shock peening on the ultra-high cycle fatigue performance of additively manufactured Ti6Al4V alloy10.1016/j.optlastec.2021.107391 ↗
18. Mid- and long-term Follow-Up efficacy analysis of 3D-Printed interbody fusion cages for anterior cervical discectomy and fusion10.1111/os.13005 ↗
19. Surface improvement of laser powder bed fusion processed Ti6Al4V for fatigue applications10.1016/j.addlet.2022.100070 ↗
20. Improved fatigue strength of additively manufactured Ti6Al4V by surface post processing10.1016/j.ijfatigue.2020.105497 ↗
21. Improvement of fatigue resistance and ductility of TiAl6V4 processed by selective laser melting10.1016/j.jmatprotec.2015.01.025 ↗
22. Patient activity after total hip arthroplasty declines with advancing age10.1007/s11999-009-0756-3 ↗
23. High cycle fatigue in selective laser melted Ti-6Al-4V10.1016/j.actamat.2020.05.041 ↗
24. 3D printing and its applications in orthopaedic trauma: a technological marvel10.1016/j.jcot.2018.07.022 ↗
25. On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: fatigue resistance and crack growth performance10.1016/j.ijfatigue.2012.11.011 ↗
26. Plasma sprayed hydroxyapatite coatings: understanding process relationships using design of experiment analysis10.1016/j.surfcoat.2015.10.044 ↗
27. Residual-stress relaxation mechanism and model description of 5052H32 Al alloy spun ellipsoidal heads during annealing treatment10.1007/s40436-021-00367-w ↗
28. A study on the residual stress during selective laser melting (SLM) of metallic powder10.1007/s00170-016-8466-y ↗
29. Effect of surface polishing treatment on the fatigue performance of shot-peened Ti–6Al–4V alloy10.1007/s40195-017-0555-x ↗
30. Multi-field coupling fatigue behavior of laser additively manufactured metallic materials: a review10.1016/j.jmrt.2022.12.112 ↗
31. The effect of laser shock peening, shot peening and their combination on the microstructure and fatigue properties of Ti-6Al-4V titanium alloy10.1016/j.ijfatigue.2021.106465 ↗
32. Influence of defects, surface roughness and HIP on the fatigue strength of Ti-6Al-4V manufactured by additive manufacturing10.1016/j.ijfatigue.2018.07.020 ↗
33. Fatigue properties of SLM-produced Ti6Al4V with various post-processing processes10.1088/1757-899X/461/1/012052 ↗
34. Optimization of selective laser melting process parameters for Ti-6Al-4V alloy manufacturing using deep learning10.1016/j.jmapro.2020.04.014 ↗
35. Understanding the effect of laser scan strategy on residual stress in selective laser melting through thermo-mechanical simulation
36. Geometrical effects on residual stress in selective laser melting
37. Surface roughness effects on the fatigue strength of additively manufactured Ti-6Al-4V10.1016/j.ijfatigue.2018.07.013 ↗
38. du Plessis · 2019
39. Hot isostatic pressing in metal additive manufacturing: X-ray tomography reveals details of pore closure
40. Microstructure and tensile properties of selectively laser-melted and of HIPed laser-melted Ti–6Al–4V10.1016/j.msea.2013.04.099 ↗
41. Improved osseointegration of 3D printed Ti-6Al-4V implant with a hierarchical micro/nano surface topography: an in vitro and in vivo study. Materials science & engineering
42. The incidence of implant fractures after total hip arthroplasty10.1007/s00264-013-2110-3 ↗
43. Effects of post-processing on cyclic fatigue response of a titanium alloy additively manufactured by electron beam melting10.1016/j.msea.2016.10.059 ↗
44. Analysis of factors affecting fatigue performance of HIP'd laser-based powder bed fusion Ti–6Al–4V coupons10.1016/j.msea.2022.144575 ↗
45. Fatigue performance of medical Ti6Al4V alloy after mechanical surface treatments10.1371/journal.pone.0121963 ↗
46. Electrocautery damage can reduce implant fatigue strength: cases and in vitro investigation
47. Fatigue of Ti6Al4V structural health monitoring systems produced by selective laser melting10.3390/ma9020106 ↗
48. Coupled experimental and computational study of residual stresses in additively manufactured Ti-6Al-4V components10.1016/j.matlet.2018.07.141 ↗
49. A comparison of biocompatibility of a titanium alloy fabricated by Electron beam melting and selective laser melting
50. Three-dimensional printing in orthopaedic surgery: current applications and future developments
51. Die Symmetrisierung unsymmetrischer Interferenzlinien mit Hilfe von Spezialblenden
52. High Cycle Fatigue (HCF) performance of Ti-6Al-4V alloy processed by selective laser melting10.4028/www.scientific.net/AMR.816-817.134 ↗
53. Fatigue performance differences between rolled and selective laser melted Ti6Al4V alloys10.1016/j.matchar.2022.111963 ↗
54. Biaxial residual stress states of plasma-sprayed hydroxyapatite coatings on titanium alloy substrate10.1016/S0142-9612(99)00272-0 ↗
55. Comparison of the microstructures and mechanical properties of Ti–6Al–4V fabricated by selective laser melting and electron beam melting10.1016/j.matdes.2015.12.135 ↗