Effect of air-particle abrasion protocols on the biaxial flexural strength, surface characteristics and phase transformation of zirconia after cyclic loading
Source abstract
Abstract
This study evaluated the effect of air-particle abrasion protocols on the biaxial flexural strength, surface characteristics and phase transformation of zirconia after cyclic loading. Disc-shaped zirconia specimens (Ø: 15mm, thickness: 1.2mm) (N=32) were submitted to one of the air-particle abrasion protocols (n=8 per group): (a) 50μm Al2O3 particles, (b) 110μm Al2O3 particles coated with silica (Rocatec Plus), (c) 30μm Al2O3 particles coated with silica (CoJet Sand) for 20s at 2.8bar pressure. Control group received no air-abrasion. All specimens were initially cyclic loaded (×20,000, 50N, 1Hz) in water at 37°C and then subjected to biaxial flexural strength testing where the conditioned surface was under tension. Zirconia surfaces were characterized and roughness was measured with 3D surface profilometer. Phase transformation from tetragonal to monoclinic was determined by Raman spectroscopy. The relative amount of transformed monoclinic zirconia (FM) and transformed zone depth (TZD) were measured using XRD. The data (MPa) were analyzed using ANOVA, Tukey's tests and Weibull modulus (m) were calculated for each group (95% CI). The biaxial flexural strength (MPa) of CoJet treated group (1266.3±158(A)) was not significantly different than that of Rocatec Plus group (1179±216.4(A,B)) but was significantly higher than the other groups (Control: 942.3±74.6(C); 50μm Al2O3: 915.2±185.7(B,C)). Weibull modulus was higher for control (m=13.79) than those of other groups (m=4.95, m=5.64, m=9.13 for group a, b and c, respectively). Surface roughness (Ra) was the highest with 50μm Al2O3 (0.261μm) than those of other groups (0.15-0.195μm). After all air-abrasion protocols, FM increased (15.02%-19.25%) compared to control group (11.12%). TZD also showed increase after air-abrasion protocols (0.83-1.07μm) compared to control group (0.59μm). Air-abrasion protocols increased the roughness and monoclinic phase but in turn abrasion with 30μm Al2O3 particles coated with silica has increased the biaxial flexural strength of the tested zirconia.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Bone Tissue Engineering Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (53)
Show source-provided references
1. Effect of conditioning methods on the microtensile bond strength of phosphate monomer-based cement on zirconia ceramic in dry and aged conditions10.1002/jbm.b.30908 ↗
2. Effect of cleaning methods after reduced-pressure air abrasion on bonding to zirconia ceramic
3. What future for zirconia as a biomaterial?10.1016/j.biomaterials.2005.07.034 ↗
4. The influence of simulated masticatory loading regimes on the biaxial flexure strength and reliability of a Y-TZP dental ceramic10.1016/j.jdent.2005.07.009 ↗
5. The influence of surface modification techniques on the performance of a Y-TZP dental ceramic10.1016/j.jdent.2005.06.006 ↗
6. Crack growth resistance of alumina, zirconia and zirconia toughened alumina ceramics for joint prostheses10.1016/S0142-9612(01)00206-X ↗
7. Characterization and surface treatment effects on topography of a glass-infiltrated alumina/zirconia-reinforced ceramic10.1016/j.dental.2006.06.043 ↗
8. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
9. Influence of surface finish and residual stresses on the ageing sensitivity of biomedical grade zirconia10.1016/j.biomaterials.2005.11.021 ↗
10. Flexural strength of an infused ceramic, glass ceramic, and feldspathic porcelain10.1016/S0022-3913(05)80067-8 ↗
11. Strength, reliability and mode of fracture of bilayered porcelain/zirconia (Y-TZP) dental ceramics10.1016/j.biomaterials.2004.02.036 ↗
12. Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramic10.1016/j.dental.2003.05.002 ↗
13. Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic10.1016/j.jdent.2004.07.001 ↗
14. Rocatec system—adhesion by tribochemical coating
15. Effect of sintering time on biaxial strength of zirconium dioxide10.1016/j.dental.2008.05.011 ↗
16. Modeling of water absorption induced cracks in resin-based composite supported ceramic layer structures10.1002/jbm.b.30852 ↗
17. International Organization for Standardization, 1998. Dental Ceramic: Amendment 1, ISO 6872. Geneva: ISO.
18. Effect of mechanical cycling on the flexural strength of densely sintered ceramics10.1016/j.dental.2005.11.025 ↗
19. Perspectives on strength10.1016/0109-5641(95)80043-3 ↗
20. Stabilized zirconia as a structural ceramic: an overview10.1016/j.dental.2007.05.005 ↗
21. Bonding to zirconia ceramic: adhesion methods and their durability10.1016/S0109-5641(98)00011-6 ↗
22. Resin bonding to oxide ceramics for dental restorations10.1163/156856109X432721 ↗
23. Determination of transformation depths in ceramics containing tetragonal ZrO210.1111/j.1151-2916.1981.tb10285.x ↗
24. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic10.1016/S0109-5641(99)00070-6 ↗
25. Strength and reliability of surface treated Y-TZP dental ceramics10.1002/1097-4636(2000)53:4<304::AID-JBM4>3.0.CO;2-S ↗
26. Fracture strength of four-unit Y-TZP FPD cores designed with varying connector diameter. An in-vitro study10.1111/j.1365-2842.2007.01770.x ↗
27. Fatigue of dental ceramics in a simulated oral environment10.1177/00220345860650071901 ↗
28. Qualitative and quantitative fracture analyses of high-strength ceramics10.1111/j.1600-0722.2008.00607.x ↗
29. Fracture load and marginal fit of shrinkage-free ZrSiO4 all-ceramic crowns after chewing simulation10.1111/j.1365-2842.2006.01637.x ↗
30. A brief history and current status of metal-and ceramic surface-conditioning concepts for resin bonding in dentistry
31. Evaluation of alternative intra-oral repair techniques for fractured ceramic-fused-to-metal restorations10.1046/j.1365-2842.2003.01037.x ↗
32. Effect of surface conditioning methods on the bond strength of luting cement to ceramics10.1016/S0109-5641(03)00019-8 ↗
33. In vitro evaluation of low-temperature aging effects and finishing procedures on the flexural strength and structural stability of Y-TZP dental ceramics10.1016/j.prosdent.2006.08.004 ↗
34. The biaxial flexural strength and fatigue property of LavaTM Y-TZP dental ceramic10.1016/j.dental.2006.09.003 ↗
35. Randomized clinical trial on single retainer all-ceramic resin-bonded fixed partial dentures: influence of the bonding system after up to 55 months10.1016/j.jdent.2012.05.009 ↗
36. Mechanical properties of dental zirconia ceramics changed with sandblasting and heat treatment10.4012/dmj.27.408 ↗
37. Transverse strength of aluminous and feldspathic porcelain10.1177/00220345740530032801 ↗
38. Fatigue of zirconia under cyclic loading in water and its implications for the design of dental bridges10.1016/j.dental.2005.12.008 ↗
39. Cyclic fatigue in water of veneer-framework composites for all-ceramic dental bridges10.1016/j.dental.2006.01.011 ↗
40. Fracture resistance of all-ceramic zirconia bridges with differing phase stabilizers and quality of sintering10.1016/j.dental.2005.11.006 ↗
41. Adhesion/cementation to zirconia and other non-silicate ceramics: where are we now?10.1016/j.dental.2010.10.022 ↗
42. Calibration curve for quantitative analysis of the monoclinic-tetragonal ZrO2 system by x-ray diffraction10.1111/j.1151-2916.1984.tb19614.x ↗
43. Y-TZP zirconia runs against highly crosslinked UHMWPE tibial inserts: Knee simulator wear and phase-transformation studies10.1002/jbm.b.30999 ↗
44. Fracture strength of two oxide ceramic crown systems after cyclic pre-loading and thermocycling10.1111/j.1365-2842.2005.01604.x ↗
45. Flexural strength of a layered zirconia and porcelain dental all-ceramic system10.1016/j.prosdent.2005.05.007 ↗
46. Four-year clinical results of fixed dental prostheses with zirconia substructures (Cercon): end abutments vs. cantilever design10.1111/j.1600-0722.2009.00693.x ↗
47. Influence of air-abrasion on zirconia ceramic bonding using an adhesive composite resin10.1016/j.dental.2009.08.008 ↗
48. Flexural strength and fracture toughness of dental core ceramics10.1016/S0022-3913(07)60045-6 ↗
49. Flexure tests on dental ceramics
50. Fatigue sensitivity of Y-TZP to microscale sharp-contact flaws10.1002/jbm.b.30174 ↗
51. Effect of sandblasting on the long-term performance of dental ceramics10.1002/jbm.b.30097 ↗
52. Damage accumulation and fatigue life of particle-abraded ceramics
53. Contact damage in an yttria stabilized zirconia: implications