Magnesium-Calcium (MgCa) alloy as an emerging biodegradable implant material has received considerable attention in orthopedic fixation applications. The biodegradable MgCa alloys avoid stress shielding and secondary surgery inherent with permanent metallic implant materials. They also provide sufficient mechanical strength in load carrying applications as opposed to biopolymers. However, the key issue facing a biodegradable MgCa implant is the fast corrosion in the human body environment. The ability to adjust the degradation rate of MgCa alloys is critical in the successful development of biodegradable orthopedic materials. Burnishing as a low plastic deformation process is a promising technique to tune surface integrity of MgCa implant surface for biodegradation control. However, the poor ductility of MgCa alloys imposes a great challenge for burnishing. This study focuses on the basic understanding of surface mechanical behavior of burnished biodegradable MgCa0.8 (wt%) alloy. The effects of burnishing parameters, i.e., pressure, feed, speed, number of path, and burnishing pattern on surface integrity factors such as surface topography, roughness, microhardness, microstructure, and residual stresses are investigated. The burnished surfaces are shinier and smoother than the as-machined ones. The MgCa alloy can be safely burnished at suitable burnishing conditions since no cracks are produced at the surface and in the subsurface. The microstructure including grain size does not show a noticeable change after burnishing. The machined surfaces are harder than the burnished ones down to the deep subsurface (∼200 μm) as opposed to the shallow hardened depth (∼50 μm) in cutting. Residual stresses are highly compressive especially at low burnishing pressure.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Surface Treatment and Residual Stress · Surface Treatment and Coatings · Bone Tissue Engineering Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. Bioceramic dip-coating on Ti–6Al–4V and 316L SS implant materials10.1007/s10856-007-3304-2 ↗
2. Contribution of loading conditions and material properties to stress shielding near the tibial component of total knee replacements10.1016/j.jbiomech.2006.05.020 ↗
3. Comparative experimental study on effects of conventional and ultrasonic deep cold rolling processes on Ti–6Al–4V10.1179/174328408X302431 ↗
4. Cold surface hardening10.1016/j.cirp.2008.03.100 ↗
5. Advancing cutting technology10.1016/S0007-8506(07)60200-5 ↗
6. Denkena, B., Witte, F., Podolsky, C., Lucas, A., 2005. Degradable implants made of magnesium alloys. In: Proc. 5th Euspen Int. Conf., Montpellier, France.
7. Biocompatible magnesium alloys as absorbable implant materials-adjusted surface and subsurface properties by machining processes10.1016/j.cirp.2007.05.029 ↗
8. Development of combined manufacturing technologies for high-strength structure components10.4028/www.scientific.net/AMR.22.67 ↗
9. Disegi, J.A., Sax, C., 2009. Effect of low plasticity burnishing on the fatigue strength of spinal rods. In: Proc. of ASM Materials & Processes for Medical Devices Conf. and Expo., Minneapolis, MN.
10. Strain shielding in proximal tibia of stemmed knee prosthesis: experimental study10.1016/j.jbiomech.2007.10.006 ↗
11. Computational simulations of stress shielding and bone resorption around existing and computer-designed orthopaedic screws10.1007/BF02344213 ↗
12. Shakedown of deep cold rolling residual stresses in titanium alloys10.1088/0022-3727/41/17/174005 ↗
13. Guo, Y.B., Brooks, V., 2009. Characterization of mechanical property and microstructure of biomedical magnesium alloy. In: Proc. of ASM Materials & Processes for Medical Devices Conf. and Expo., Minneapolis, MN.
14. Process mechanics and surface integrity by high speed dry milling of biodegradable magnesium-calcium implant alloys10.1016/j.cirp.2010.03.051 ↗
15. Production and properties of small tubes made from MgCa0.8 for application as stent in biomedical science
16. Influence of alloy composition on the mechanical and electrochemical properties of binary Mg–Ca alloys and its corrosion behavior in solutions at different chloride concentrations
17. Biocorrosion of magnesium alloys: a new principle in cardiovascular implant technology10.1136/heart.89.6.651 ↗
18. Nutrition in bone health revisited: a story beyond calcium10.1080/07315724.2000.10718070 ↗
19. Mathematical modeling of stress shielding with bioresorbable materials for internal fracture fixation
20. Jayaraman, N., Hornbach, D.J., Prevey, P.S., 2007. Mitigation of fatigue and pre-cracking damage in aircraft structures through low plasticity burnishing. In: Proc. ASIP, Palm Springs, CA.
21. Effective boundary of deep-rolling treatment and its correlation with residual stress stability of Al–Mg–Mn and Al–Mg–Si–Cu alloys10.1016/j.scriptamat.2007.01.021 ↗
22. The development of binary Mg–Ca alloys for use as biodegradable materials within bone10.1016/j.biomaterials.2007.12.021 ↗
23. Influence of heat treatment on degradation behavior of bio-degradable die-cast AZ63 magnesium alloy in simulated body fluid10.1016/j.msea.2006.12.020 ↗
24. The effect of ball burnishing on heat treated steel and Inconel 718 milled surfaces10.1007/s00170-005-0402-5 ↗
25. Massalski · 1990 · 1,927
26. Stress shielding and bone resorption in shoulder arthroplasty10.1067/mse.2003.22 ↗
27. Comparison of the fatigue behavior and residual stress stability of laser-shock peened and deep rolled austenitic stainless steel AISI 304 in the temperature range 25–600 °C10.1016/j.msea.2007.02.004 ↗
28. Correlation between residual stress and plastic strain amplitude during low cycle fatigue of mechanically surface treated austenitic stainless steel AISI 304 and ferritic-pearlitic steel SAE 104510.1016/j.msea.2008.03.034 ↗
29. Residual stress relaxation of deep-rolled austenitic steel10.1016/j.scriptamat.2007.09.045 ↗
30. The influence of surface enhancement by low plasticity burnishing on the corrosion fatigue performance of AA7075-T610.1016/j.ijfatigue.2004.01.010 ↗
31. Case studies of fatigue life improvement using low plasticity burnishing in gas turbine engine applications10.1115/1.1807414 ↗
32. Controlled plasticity burnishing to improve the performance of friction stir processed Ni–Al bronze10.4028/www.scientific.net/MSF.539-543.3807 ↗
33. Prevey, P., McNulty, D., Carr, J., Sade, P., Craft, A., 2009. Fatigue strength enhancement of Ti–6Al–4V ELI femoral distal stems using low plasticity burnishing. In: Proc. of ASM Materials & Processes for Medical Devices Conf. and Expo., Minneapolis, MN.
34. Investigations on the effect of ball burnishing parameters on surface hardness and wear resistance of HSLA dual-phase steels10.1080/10426910801937306 ↗
35. Scheel, J.E., Hornbach, D.J., Prevey, P.S., 2009. Safe life conversion of aircraft aluminum structures via low plasticity burnishing for mitigation of corrosion related failures. Department of Defense Corrosion Conf., Gaylord National, Washington, DC.
36. Deep rolling of titanium rods for application in modular total hip arthroplasty
37. Low plasticity burnishing: an innovative manufacturing method for biomedical applications10.1115/1.2896121 ↗
38. Investigations on surface integrity of AISI 1045 using LPB tool10.1016/j.triboint.2008.01.003 ↗
39. Seiler · 1987
40. Control of biodegradation of biocompatible magnesium alloys10.1016/j.corsci.2007.01.001 ↗
41. A possible biodegradable magnesium implant material10.1002/adem.200600252 ↗
42. Evaluation of surface-modified Ti–6Al–4V alloy by combination of plasma-carburizing and deep-rolling10.1016/j.msea.2007.11.079 ↗
43. Effect of combined plasma-carburizing and deep rolling on notch fatigue property of Ti–6Al–4V alloy10.1016/j.msea.2008.09.008 ↗
44. Influence of different surface machining treatments of magnesium-based resorbable implants on the degradation behavior in rabbits
45. The effect of pre-processing and grain structure on the bio corrosion and fatigue resistance of magnesium alloy AZ3110.1002/adem.200700200 ↗
46. In vivo corrosion of four magnesium alloys and the associated bone response10.1016/j.biomaterials.2004.09.049 ↗