The effect of microstructure on fatigue performance of Ti–6Al–4V alloy after EDM surface treatment for application in orthopaedics
Source abstract
Abstract
Three different microstructures--equiaxed, bi-modal and coarse lamellar--are prepared from Ti-6Al-4V alloy. Electric discharge machining (EDM) with a high peak current (29 A) is performed in order to impose surface roughness and modify the chemical composition of the surface. Detailed scanning electron microscopy (SEM) investigation revealed a martensitic surface layer and subsurface heat affected zone (HAZ). EDX measurements showed carbon enriched remnants of the EDM process on the material surface. Rotating bending fatigue tests are undertaken for EDM processed samples for all three microstructures and also for electropolished-benchmark-samples. The fatigue performance is found to be rather poor and not particularly dependent on microstructure. The bi-modal microstructure shows a slightly superior high cycle fatigue performance. This performance can be further improved by a suitable heat treatment to an endurance limit of 200 MPa.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Machining and Optimization Techniques · Advanced machining processes and optimization · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Phase transformations during cooling in α+β titanium alloys10.1016/S0921-5093(97)00802-2 ↗
2. Improvement in the morphology of Ti-based surfaces: a new process to increase in vitro human osteoblast response10.1016/S0142-9612(01)00271-X ↗
3. Boyer · 2007
4. Plasma surface modification of biomaterials10.1016/S0927-796X(02)00004-9 ↗
5. Rough surfaces of titanium and titanium alloys for implants and prostheses10.1016/j.msec.2004.08.004 ↗
6. Ti based biomaterials, the ultimate choice for orthopaedic implants — a review10.1016/j.pmatsci.2008.06.004 ↗
7. Electrical discharge machining of titanium alloy10.1016/j.apsusc.2007.05.031 ↗
8. Cellular Ti–6Al–4V structures with interconnected macro porosity for bone implants fabricate by selective beam melting10.1016/j.actbio.2008.03.013 ↗
9. Fatigue endurance of Ti–6Al–4V alloy with electro-eroded surface for improved bone in-growth
10. Surface modification by electrical discharge machining: a review10.1016/j.jmatprotec.2008.09.032 ↗
11. Fatigue and cyclic deformation behaviour of surface modified titanium in simulated physiological media10.1016/j.biomaterials.2005.08.012 ↗
12. 2003
13. Surface modification of titanium, titanium alloys and related materials for biomedical applications10.1016/j.mser.2004.11.001 ↗
14. Luetjering · 2007
15. Improving the biocompatibility of medical implants with plasma immersion ion implantation10.1016/S0257-8972(02)00085-3 ↗
16. Microstructural standards for “alpha” + “beta” titanium alloys bars. European Titanium Producers, Technical Committee (ETTC). Deutsche Titan GmbH, Essen, Germany and IMI-Titanium Ltd., Birmingham, UK. Publication 2 1979.
17. Mueller, J., Rack, H.J., Wagner, L., 2007. Effects of supra- and subtransus heat treatments on fatigue performance of Ti–6Al–4V. In: Ti-2007 Science and Technology. The Japan Institute of Metals, pp. 383–386.
18. Mechanical biocompatibilities of titanium alloys for biomedical applications
19. Long crack growth behaviour of implant material Ti-5Al-2.5Fe in air and simulated body environment related to microstructure10.1016/S0142-1123(00)00058-X ↗
20. Comparison of metal release from various metallic biomaterials in vitro10.1016/j.biomaterials.2004.02.005 ↗
21. Morphological studies on machined implants of commercially pure titanium and titanium alloy (Ti6Al4V) in the rabbit10.1002/jbm.b.31404 ↗
22. Effect of electrical discharging on formation of nanoporous biocompatible layer on titanium10.1016/j.jallcom.2009.11.197 ↗
23. Titanium alloys for biomedical applications10.1016/j.msec.2005.08.032 ↗
24. Investigation of near surface structure in order to determine process-temperatures during different machining process of Ti–6Al–4V10.1016/j.scriptamat.2003.09.023 ↗
25. Characteristics of hydroxyapatite coated titanium porous coatings on Ti–6Al–4V substrates by plasma sprayed method10.1002/jbm.b.30750 ↗