journal article·2017-11

Influence of various bonding techniques on the fracture strength of thin CAD/CAM-fabricated occlusal glass-ceramic veneers

Christine Yazigi, Matthias Kern, Mohamed Sad Chaar

Publisher page

Abstract

Objectives To evaluate the efficiency of immediate dentin sealing and the effects of different bonding protocols on the fracture strength of CAD/CAM occlusal veneers bonded to exposed dentin. Methods Ninety-six extracted maxillary premolars were initially divided into three main groups with 32 specimens each: without immediate dentin sealing, immediate dentin sealing/total etching and immediate dentin sealing/selective etching. Teeth were identically prepared in the dentin to receive occlusal veneers of 0.8mm thickness, milled from lithium disilicate ceramic blocks (IPS e.max CAD). Each main group was later subdivided, according to the pre-cementation surface etching protocol (total/selective), into two subgroups with 16 specimens each. All restorations were adhesively bonded using a resin cement (Variolink Esthetic). Half of the specimens of each subgroup were subjected to thermo-dynamic loading in a chewing simulator with 1,200,000 cycles at 10kg load. The other half and the surviving specimens were subjected to quasi-static loading until failure. Statistical analysis was performed using three-way ANOVA and Tukey's post-hoc tests. Results All specimens except one survived the artificial aging. A significantly higher fracture strength of restorations (p ≤ 0.001) was obtained when immediate dentin sealing was followed regardless of the etching method with values ranging from a minimum of 1122 ± 336N to a maximum of 1853 ± 333N. Neither the pre-cementation treatment nor the artificial aging had a statistical significant effect on the fracture strength. Significance Immediate dentin sealing protocol is recommended whenever dentin is exposed during the preparation for thin glass-ceramic occlusal veneers.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Endodontics and Root Canal Treatments · Dental Research and COVID-19

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (67)

Show source-provided references
1. Guidelines for the preparation of CAD/CAM ceramic inlays and partial crowns
2. Fracture resistance of ceramic and polymer-based occlusal veneer restorations10.1016/j.jmbbm.2017.06.013 ↗
3. Influence of cyclic loading and luting agents on the fracture load of two all-ceramic crown systems10.1016/j.prosdent.2004.09.002 ↗
4. Dual application of dentin bonding agents: effect on bond strength
5. Digital dentistry: an overview of recent developments for CAD/CAM generated restorations10.1038/sj.bdj.2008.350 ↗
6. Non- and minimally invasive full-mouth rehabilitation of patients with loss of vertical dimension of occlusion using CAD/CAM: an innovative concept demonstrated with a case report
7. Survival rates for porcelain laminate veneers with special reference to the effect of preparation in dentin: a literature review10.1111/j.1708-8240.2012.00517.x ↗
8. Dentin contamination protection after mechanical preparation for veneering
9. Dynamic fatigue and fracture resistance of non-retentive all-ceramic full-coverage molar restorations. Influence of ceramic material and preparation design10.1016/j.dental.2010.01.011 ↗
10. Bonding of an auto-adhesive luting material to enamel and dentin10.1016/j.dental.2004.03.002 ↗
11. A critical review of the durability of adhesion to tooth tissue: methods and results10.1177/154405910508400204 ↗
12. Development of an artificial oral environment for the testing of dental restoratives: bi-axial force and movement control10.1177/00220345830620010801 ↗
13. In vitro evaluation of marginal and internal adaptation of class II resin composite restorations after thermal and occlusal stressing
14. Tooth structure removal associated with various preparation designs for posterior teeth
15. Comparison of fracture strength and failure mode of different ceramic implant abutments10.1016/j.prosdent.2016.06.018 ↗
16. Tensile bond strength of so-called universal primers and universal multimode adhesives to zirconia and lithium disilicate ceramics
17. Bond strength of self-etch adhesives to pre-etched enamel10.1016/j.dental.2009.04.004 ↗
18. Influence of different conditioning methods on immediate and delayed dentin sealing10.1016/j.prosdent.2013.10.028 ↗
19. Effect of selective enamel etching on clinical performance of CAD/CAM partial ceramic crowns luted with a self-adhesive resin cement10.1007/s00784-013-1173-2 ↗
20. Selective enamel etching reconsidered: better than etch-and-rinse and self-etch?
21. Clinical results of lithium-disilicate crowns after up to 9 years of service10.1007/s00784-012-0700-x ↗
22. Effect of immediate and delayed dentin sealing on the fracture strength, failure type and Weilbull characteristics of lithiumdisilicate laminate veneers10.1016/j.dental.2016.01.001 ↗
23. Attrition, abrasion, corrosion and abfraction revisited: a new perspective on tooth surface lesions10.14219/jada.archive.2004.0369 ↗
24. Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part I. Pressable and alumina glass-infiltrated ceramics10.1016/j.dental.2003.05.003 ↗
25. Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramics10.1016/j.dental.2003.05.002 ↗
26. Influence of preparation design and ceramic thicknesses on fracture resistance and failure modes of premolar partial coverage restorations10.1016/S0022-3913(13)60374-1 ↗
27. Prospective clinical split-mouth study of pressed and CAD/CAM all-ceramic partial-coverage restorations: 7-year results10.11607/ijp.3043 ↗
28. Effect of storage media on microleakage of five dentin bonding agents10.1016/0109-5641(93)90119-B ↗
29. Effect of priming time on tensile bond strength to bovine teeth and morphologic structure of interfaces created by self-etching primers
30. Restorative therapy of erosion10.1159/000093364 ↗
31. Efficacy of a resin coating on bond strengths of resin cement to dentin10.1111/j.1708-8240.2003.tb00325.x ↗
32. Fracture strength of all-porcelain, resin-bonded bridges after testing in an artificial oral environment10.1016/0300-5712(93)90160-R ↗
33. Wear of composite resin veneering materials in a dual-axis chewing simulator10.1046/j.1365-2842.1999.00416.x ↗
34. Kern · 2017
35. Adhesive luting of indirect restorations
36. The effect of three variables on shear bond strength when luting a resin inlay to dentin10.2341/08-82 ↗
37. Ask the expert. Will ceramic restorations be challenged in the future?10.14219/jada.archive.2001.0024 ↗
38. Effects of thickness, processing technique, and cooling rate protocol on the flexural strength of a bilayer ceramic system10.1016/j.dental.2013.07.019 ↗
39. The wear and tear of teeth10.1159/000367976 ↗
40. Immediate dentin sealing: a fundamental procedure for indirect bonded restorations10.1111/j.1708-8240.2005.tb00103.x ↗
41. Porcelain veneers: dentin bonding optimization and biomimetic recovery of the crown
42. Immediate dentin sealing improves bond strength of indirect restorations10.1016/j.prosdent.2005.10.010 ↗
43. Immediate dentin sealing supports delayed restoration placement10.1016/S0022-3913(07)60052-3 ↗
44. The case for moderate "guided prep" indirect porcelain veneers in the anterior dentition. The pendulum of porcelain veneer preparations: from almost no-prep to over-prep to no-prep
45. Survival of Dicor glass-ceramic dental restorations over 16 years. Part III: effect of luting agent and tooth or tooth-substitute core structure10.1067/mpr.2001.119415 ↗
46. Dentine bonding--the effect of pre-curing the bonding resin10.1038/sj.bdj.4808447 ↗
47. Effects of cyclic loading on the strength of all-ceramic materials
48. Dentin bond strengths of two ceramic inlay systems after cementation with three different techniques and one bonding system10.1067/mpr.2003.37 ↗
49. Measuring the residual stress in dental composites using a ring slitting method10.1016/j.dental.2005.03.006 ↗
50. Aggressiveness of contemporary self-etching adhesives. Part II: etching effects on unground enamel10.1016/S0109-5641(00)00104-4 ↗
51. Dentin permeability: sealing the dentin in crown preparations
52. The dual bonding technique: a modified method to improve adhesive luting procedures
53. Porcelain veneers: a review of the literature10.1016/S0300-5712(99)00066-4 ↗
54. Three-year clinical effectiveness of a two-step self-etch adhesive in cervical lesions10.1111/j.1600-0722.2005.00256.x ↗
55. Compressive fracture resistance of porcelain laminates bonded to enamel or dentin with four adhesive systems10.1111/j.1532-849X.2007.00227.x ↗
56. Long-term bond between dual-polymerizing cementing agents and human hard dental tissue10.1016/j.dental.2006.01.012 ↗
57. A systematic review of ceramic inlays in posterior teeth: an update
58. Performance of dental ceramics: challenges for improvements10.1177/0022034510391795 ↗
59. Influence of restoration thickness and dental bonding surface on the fracture resistance of full-coverage occlusal veneers made from lithium disilicate ceramic10.1016/j.dental.2015.04.017 ↗
60. Novel-design ultra-thin CAD/CAM composite resin and ceramic occlusal veneers for the treatment of severe dental erosion10.1016/S0022-3913(11)60035-8 ↗
61. Simplified treatment of severe dental erosion with ultrathin CAD-CAM composite occlusal veneers and anterior bilaminar veneers10.1016/j.prosdent.2016.02.013 ↗
62. The effect of phosphoric acid pre-etching and thermocycling on self-etching adhesive enamel bonding10.1016/S0022-3913(12)60033-X ↗
63. Influence of cavity preparation design on fracture resistance of posterior Leucite-reinforced ceramic restorations10.1016/j.prosdent.2006.03.022 ↗
64. Investigation of the dry and wet fatigue properties of three all-ceramic crown systems
65. Fracture resistance of lithium disilicate-, alumina-, and zirconia-based three-unit fixed partial dentures: a laboratory study
66. Bond strength of a mild self-etch adhesive with and without prior acid-etching10.1016/j.jdent.2005.04.001 ↗
67. A randomized, controlled trial evaluating the three-year clinical effectiveness of two etch & rinse adhesives in cervical lesions