Effect of grinding with diamond-disc and -bur on the mechanical behavior of a Y-TZP ceramic
Source abstract
Abstract
This study compared the effects of grinding on the surface micromorphology, phase transformation (t→m), biaxial flexural strength and structural reliability (Weibull analysis) of a Y-TZP (Lava) ceramic using diamond-discs and -burs. 170 discs (15×1.2mm) were produced and divided into 5 groups: without treatment (Ctrl, as-sintered), and ground with 4 different systems: extra-fine (25µm, Xfine) and coarse diamond-bur (181µm, Coarse), 600-grit (25µm, D600) and 120-grit diamond-disc (160µm, D120). Grinding with burs was performed using a contra-angle handpiece (T2-Revo R170, Sirona), while for discs (Allied) a Polishing Machine (Ecomet, Buehler) was employed, both under water-cooling. Micromorphological analysis showed distinct patterns generated by grinding with discs and burs, independent of grit size. There was no statistical difference for characteristic strength values (MPa) between smaller grit sizes (D600 - 1050.08 and Xfine - 1171.33), although they presented higher values compared to Ctrl (917.58). For bigger grit sizes, a significant difference was observed (Coarse - 1136.32>D120 - 727.47). Weibull Modules were statistically similar between the tested groups. Within the limits of this study, from a micromorphological point-of-view, the treatments performed did not generate similar effects, so from a methodological point-of-view, diamond-discs should not be employed to simulate clinical abrasion performed with diamond-burs on Y-TZP ceramics.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Advanced ceramic materials synthesis · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Bridging the gap between clinical failure and laboratory fracture strength tests using a fractographic approach10.1016/j.dental.2008.09.001 ↗
2. Resin-ceramic bonding: a review of the literature10.1067/mpr.2003.50 ↗
3. Flexural strenght and failures modes of layered ceramic structures10.1016/j.dental.2011.09.008 ↗
4. Low-temperature degradation of zirconia and implications for biomedical implants10.1146/annurev.matsci.37.052506.084250 ↗
5. Crespo · 1997
6. Fracture toughness versus micro-tensile bond strength testing of adhesive–dentin interfaces10.1016/j.dental.2013.03.010 ↗
7. Weibull analysis and flexural strength of hot-pressed core and veneered ceramic structures10.1016/S0109-5641(03)00010-1 ↗
8. Characterizing ceramics and interfacial adhesion to resin: I – the relationship of microstructure, composition, properties and fractography10.1590/S1678-77572005000100002 ↗
9. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
10. Influence of surface finish and residual stresses on the ageing sensitivity of biomedical grade zirconia10.1016/j.biomaterials.2005.11.021 ↗
11. Martensitic transformation in zirconia. Part II. Martensitic growth
12. Phase analysis in Zirconia systems10.1111/j.1151-2916.1972.tb11290.x ↗
13. The phenomena of rupture and flow in solids10.1098/rsta.1921.0006 ↗
14. Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic10.1016/j.jdent.2004.07.001 ↗
15. Influence of clenching intensity on bite force balance, occlusal contact area, and average bite pressure10.1177/00220345990780070801 ↗
16. Inhibition of low-temperature degradation of tetragonal zirconia ceramics—a review
17. ISO 6872, 2008. Dentistry—Ceramic Materials. Int. Organ. Stand.
18. Effect of ceramic surface treatments on the bond of four resin luting agents to a ceramic material10.1016/S0022-3913(98)70170-2 ↗
19. The effect of low temperature aging on the mechanical property & phase stability of YTZP ceramics10.4047/jap.2009.1.3.113 ↗
20. Concerns of hydrothermal degradation in CAD/CAM zirconia10.1177/0022034509354193 ↗
21. Phase change and mechanical properties of ZrO2–Y2O3 solid electrolyte after ageing10.1016/0167-2738(81)90138-7 ↗
22. The strength and hydrothermal stability of Y-TZP ceramics for dental applications10.1111/j.1744-7402.2007.02124.x ↗
23. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic10.1016/S0109-5641(99)00070-6 ↗
24. The effects of dental grinding and sandblasting on ageing and fatigue behavior of dental zirconia (Y-TZP) ceramics10.1016/j.jeurceramsoc.2007.09.013 ↗
25. X-Ray determination of transformation depths in ceramics containing tetragonal ZrO210.1111/j.1151-2916.1981.tb10285.x ↗
26. Review of low temperature degradation in Y-TZPs
27. Correlation of in vitro fatigue data and in vivo clinical performance of a glassceramic material10.1016/j.dental.2007.01.011 ↗
28. Low temperature degradation – ageing – of zirconia: a critical review of the relevant aspects in dentistry10.1016/j.dental.2010.04.006 ↗
29. In vitro evaluation of low-temperature aging effects and finishing procedures on the flexural strength and structural stability of Y-TZP dental ceramics10.1016/j.prosdent.2006.08.004 ↗
30. Zirconia as a ceramic biomaterial, a review10.1016/S0142-9612(98)00010-6 ↗
31. Task-dependence of activity/bite-force relations and its impact on estimation of chewing force from EMG10.1177/154405910208100706 ↗
32. On the nature of machining cracks in ground ceramics: part I: SRBSN strengths and fractographic analysis10.1081/MST-200059038 ↗
33. Design data for engineering ceramics: a review of the flexure test10.1111/j.1151-2916.1991.tb08259.x ↗
34. Quinn, G.D., 2007. NIST Recommended Practice Guide: Fractography of Ceramics and Glasses. Nat. Inst. Stand. Technol.10.6028/NBS.SP.960-16 ↗
35. A practical and systematic review of Weibull statistics for reporting strengths of dental materials10.1016/j.dental.2009.09.006 ↗
36. Control of the tetragonal to monoclinic phase transformation of yttria partially stabilized in hot water10.1007/BF00552389 ↗
37. Significance of internal stresses for the martensitic transformation in yttria-stabilized tetragonal zirconia polycrystals during degradation10.1111/j.1151-2916.1986.tb04789.x ↗
38. In vitro lifetime of dental ceramics under cyclic loading in water10.1016/j.biomaterials.2006.12.033 ↗
39. Structural reliability of alumina-, feldspar-leucite-, mica- and zirconia-based ceramics10.1016/S0300-5712(00)00030-0 ↗
40. Calibration curve for quantitative analysis of the monoclinic tetragonal ZrO2 system by X-rays diffraction10.1111/j.1151-2916.1984.tb19614.x ↗
41. Biaxial flexure tests of ceramic substrates
42. A statistical distribution function of wide applicability10.1115/1.4010337 ↗
43. Abrasive machining of porcelain and zirconia with a dental handpiece10.1016/S0043-1648(03)00195-9 ↗
44. An overview of in vitro abrasive finishing & CAD/CAM of bioceramics in restorative dentistry10.1016/j.ijmachtools.2005.07.045 ↗
45. Role of H2O on the degradation process of Y-TZP10.1007/BF01756800 ↗