journal article·2012-09

Shear bond strength comparison between conventional porcelain fused to metal and new functionally graded dental restorations after thermal–mechanical cycling

B. Henriques, S. Gonçalves, D. Soares, F.S. Silva

Publisher page

Abstract

Objectives The aim of this study was to evaluate the effect of thermo-mechanical cycling on the metal-ceramic bond strength of conventional porcelain fused to metal restorations (PFM) and new functionally graded metal-ceramic dental restorations (FGMR). Methods Two types of specimens were produced: PFM and FGMR specimens. PFM specimens were produced by conventional PFM technique. FGMR specimens were hot pressed and prepared with a metal/ceramic composite interlayer (50 M, vol%) at the metal-ceramic interface. They were manufactured and standardized in cylindrical format and then submitted to thermal (3000, 6000 and 12,000 cycles; between 5 °C and 60 °C; dwell time: 30s) and mechanical (25,000, 50,000 and 100,000 cycles under a load of 50 N; 1.6 Hz) cycling. The shear bond strength tests were performed in a universal testing machine (crosshead speed: 0.5mm/min), using a special device to concentrate the tension at the metal-ceramic interface and the load was applied until fracture. The metal-ceramic interfaces were examined with SEM/EDS prior to and after shear tests. The Young's modulus and hardness were measured across the interfaces of both types of specimens using nanoindentation tests. Data was analyzed with Shapiro-Wilk test to test the assumption of normality. The 2-way ANOVA was used to compare shear bond strength results (p<0.05). Results FGMR specimens showed significantly (p<0.001) higher shear bond strength results than PFM specimens, irrespective of fatigue conditions. Fatigue conditions significantly (p<0.05) affected the shear bond strength results. The analysis of surface fracture revealed adhesive fracture type for PFM specimens and mixed fracture type for FGMR specimens. Nanoindentation tests showed differences in mechanical properties measured across the metal-ceramic interface for the two types of specimens, namely Young's Modulus and hardness. Significance This study showed significantly better performance of the new functionally graded restorations relative to conventional PFM restorations, under fatigue testing conditions and for the materials tested.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. Anusavice · 2006
2. Comparative evaluation of ceramic–metal bond tests using finite element stress analysis10.1177/00220345800590030901 ↗
3. Comparison of the bond strength of laser-sintered and cast base metal dental alloys to porcelain10.1016/j.dental.2008.03.001 ↗
4. Bond strengths of three chemical adhesive cements adhered to a nickel–chromium alloy for direct bonded retainers10.1016/0022-3913(90)90096-U ↗
5. Craig · 2002
6. Evaluation of two methods for assessing marginal leakage10.1016/0022-3913(81)90334-6 ↗
7. Shear bond strengths of a ceramic system to alternative alloys10.1016/j.prosdent.2004.10.017 ↗
8. Preparation, microstructure and mechanical properties of metal-particulate/glass-matrix composites10.1016/S0266-3538(96)00102-9 ↗
9. Porcelain-fused-to-metal (PFM) alternatives10.1111/j.1708-8240.2008.00222.x ↗
10. Shear bond strength of metal–ceramic repair systems10.1016/j.prosdent.2006.07.002 ↗
11. A clinical evaluation of cobalt-chromium metal ceramic fixed partial dentures and crowns: A three-to seven-year retrospective study10.1016/S0022-3913(07)60032-8 ↗
12. Effect of chromium interlayer on the shear bond strength between porcelain and pure titanium10.1016/j.dental.2010.04.004 ↗
13. Influence of chromium interlayer on the adhesion of porcelain to machined titanium as determined by the strain energy release rate10.1016/j.jdent.2010.05.003 ↗
14. The effect of thermal cycling on metal–ceramic bond strength10.1016/j.jdent.2009.03.014 ↗
15. Corrosion of gold and amalgam placed in contact with each other10.1177/00220345630420051301 ↗
16. Optimization of FGM TBC and their thermal cycling stability10.4028/www.scientific.net/MSF.492-493.9 ↗
17. Thermal cycling procedures for laboratory testing of dental restorations10.1016/S0300-5712(98)00037-2 ↗
18. A qualitative study for the bond and color of ceramometals — Part I.10.1016/S0022-3913(96)90244-9 ↗
19. Designs of bond strength tests for metal–ceramic complexes: Review of the literature10.1016/S0022-3913(96)90244-9 ↗
20. Evaluation of an experimental dental porcelain10.1016/j.jmbbm.2010.07.011 ↗
21. Optimization of bond strength between gold alloy and porcelain through a composite interlayer obtained by powder metallurgy10.1016/j.msea.2010.10.054 ↗
22. Shear bond strength of a Hot Pressed Au-Pd-Pt alloy-porcelain dental composite. J. Mech. Behav
23. Bioinspired design of dental multilayers
24. The influence of opaque application methods on the bond strength and final shade of PFM restorations10.1016/j.jdent.2010.08.016 ↗
25. In vitro study of the effect of thermo- and load-cycling on the bond strength of porcelain repair system10.1046/j.1365-2842.1999.00346.x ↗
26. Fatigue life and failure modes of crowns systems with a modified framework design10.1016/j.jdent.2010.04.011 ↗
27. Fractures of the fixture component of an osseointegrated implant
28. Longevity of fixed metal ceramic bridge prostheses: a clinical follow-up study10.1046/j.1365-2842.2002.00833.x ↗
29. Evaluation of thermal cycling and mechanical loading on bond strength of a self-etching primer system to dentin10.1016/S0109-5641(01)00048-3 ↗
30. Bio-inspired design of dental multilayers: Experiments and model10.1016/j.jmbbm.2008.10.009 ↗
31. Influence of thermal and mechanical cycling on the flexural strength of ceramics with titanium or gold alloy frameworks10.1016/j.dental.2007.06.008 ↗
32. A systematic review of the survival and complication rates of fixed partial dentures after an observation period of at least 5 years10.1111/j.1600-0501.2004.01119.x ↗
33. Three-point bending strength of ceramics fused to cast titanium10.1111/j.1600-0722.1996.tb00083.x ↗
34. The current status of composite materials and adhesive systems. Part 4. Some clinically related research
35. Indentation fracture toughness and dynamic elastic moduli for commercial feldspathic dental porcelain materials10.1016/S0109-5641(03)00092-7 ↗
36. The influence of the resilient support of abutment teeth on the fracture resistance of all-ceramic fixed dental prostheses: An in vitro study
37. Approach for valuating the influence of laboratory simulation10.1016/j.dental.2008.08.009 ↗
38. Shear bond strength between metal alloy and a ceramic system, submitted to different thermocycling immersion times
39. Mechanical properties of dental implants submitted to fluoride ions action
40. Monotonic flexure and fatigue strength of composites for provisional and definitive restorations10.1016/S0022-3913(03)00174-4 ↗
41. Comparative strength of metal–ceramic and metal–composite bonds after extended thermocycling10.1111/j.1365-2842.2004.01391.x ↗
42. Characterization of dental-ceramic interfaces immersed in artificial saliva after substructural mechanical metallization with titanium10.1016/j.surfcoat.2010.07.116 ↗
43. Suresh · 1998
44. Graded materials for resistance to contact deformation and damage10.1126/science.1059716 ↗
45. The effect of thermal cycling on the bond strength of low-fusing porcelain to commercially pure titanium and titanium-aluminium-vanadium alloy10.1016/S0109-5641(03)00027-7 ↗
46. Corrosion of alloys used in dentistry: A review10.1016/j.msea.2006.05.003 ↗
47. Van Noort · 2007
48. Mechanical and Thermal Cycling Effects on the flexural of glass Ceramics Fused to Titanium10.4012/dmj.27.7 ↗
49. Evaluation of interface characterization and adhesion of glass ceramics to commercially pure titanium and gold alloys after thermal- and mechanical-loading10.1016/j.dental.2008.07.002 ↗
50. Color related to ceramic and zirconia restorations: A review10.1016/j.dental.2010.10.018 ↗
51. Effect of interfacial variables on metal-porcelain bonding10.1002/jbm.820270414 ↗
52. Six year follow-up of titanium and high-gold porcelain-fused-to-metal fixed partial dentures10.1046/j.1365-2842.1999.00373.x ↗
53. The effect of oxidation heat treatment on porcelain bond strength in selected base metal alloys10.1016/0022-3913(91)90502-N ↗
54. From porcelain-fused-to-metal to zirconia: Clinical and experimental considerations10.1016/j.dental.2010.10.024 ↗