Fatigue properties of magnesium alloy AZ91 processed by severe plastic deformation
Source abstract
Abstract
Fatigue properties of cast AZ91 magnesium alloy processed by severe plastic deformation were investigated and compared with the properties of the initial cast state. The severe plastic deformation was carried out by equal channel angular pressing (ECAP). The ECAP treatment resulted in a bimodal structure. The bimodality consists in a coexistence of fine grained areas with higher content of Mg17Al12 particles and areas exhibiting larger grains and lower density of Mg17Al12 particles. Improvement of the basic mechanical properties of AZ91 (yield stress, tensile strength and ductility) by ECAP was significant. Also the improvement of the fatigue life in the low-cycle fatigue region was substantial. However the improvement of the fatigue strength in the high-cycle fatigue region was found to be negligible. The endurance limit based on 10(7) cycles for the cast alloy was 80 MPa and for the alloy processed by ECAP 85 MPa. The cyclic plastic response in both states was qualitatively similar; initial softening was followed by a long cyclic hardening. Fatigue cracks in cast alloy initiate in cyclic slip bands which were formed in areas of solid solution. In the case of severe plastic deformed material with bimodal structure two substantially different mechanisms of crack initiation were observed. Crack initiation in slip bands was a preferred process in the areas with large grains whereas the grain boundaries cracking was a characteristic mechanism in the fine grained regions.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Altwicker · 1939
2. Braszczyńska-Malik, K.N., 2011. Precipitates of γ-Mg17Al12 Phase in AZ91 Alloy. In: 〈http://cdn.intechopen.com/pdfs/12741/InTech-Precipitates_of_gamma_mg17al12_phase_in_mg_al_alloys.pdf〉.10.5772/13115 ↗
3. Equal-channel angular pressing of magnesium alloy AZ91 and its effects on microstructure and mechanical properties10.1016/j.msea.2006.10.199 ↗
4. Recent advances on the development of magnesium alloys for biodegradable implants10.1016/j.actbio.2014.07.005 ↗
5. Magnesium alloys as body implants: fracture mechanism under dynamic and static loadings in a physiological environment10.1016/j.actbio.2011.10.031 ↗
6. Effect of ECAP on microstructure and mechanical properties of cast AZ91 magnesium alloy
7. Microstructure and mechanical properties of an as-cast AZ91 Mg alloy processed by equal channel angular pressing10.1088/1757-899X/4/1/012012 ↗
8. Fatigue properties of fine grained magnesium alloys after severe plastic deformation10.1007/BF03023903 ↗
9. Influence of elevated temperatures on the cyclic deformation behaviour of the magnesium die-cast alloys AZ91D and MRI 230D10.1016/j.msea.2007.10.003 ↗
10. Cyclic deformation and fatigue behaviour of the magnesium alloy AZ9110.1016/S0921-5093(01)01105-4 ↗
11. Cyclic plastic beahavior and fatigue life of AZ91 alloy in as-cast and ultrafine-grained state
12. Microstructure and mechanical properties of iltrafine-grained magnesium AZ91 alloy10.4028/www.scientific.net/MSF.782.384 ↗
13. Corrosion fatigue behaviors of two biomedical Mg alloys-AZ91D and WE43-in simulated body fluid10.1016/j.actbio.2010.07.026 ↗
14. Gupta · 2011 · 257
15. Microstructure and corrosion properties of fine-grained Mg-based alloys10.4028/www.scientific.net/MSF.584-586.994 ↗
16. Evaluation of fatigue life of AZ31 magnesium alloy fabricated by squeeze casting10.1016/j.matdes.2012.08.079 ↗
17. Bimodal grain size distribution in UFG materials produced by SPD: their evolution and effect on mechanical properties
18. Fatigue properties of a fine-grained magnesium alloy produced by equal channel angular pressing10.1016/j.scriptamat.2004.11.007 ↗
19. Bimodal grain size distribution in UFG materials produced by SPD—their evolution and effect on the fatigue and monotonic strength properties10.4149/km_2011_1_51 ↗
20. On the thermal stability of ECAP deformed FCC metals10.4028/www.scientific.net/MSF.558-559.259 ↗
21. High cyclic fatigue characteristics of gravity cast AZ91 magnesium alloy subjected to transverse load10.1016/j.matdes.2008.10.032 ↗
22. Cyclic fatigue resistance of AZ91 magnesium alloy
23. Mechanisms of extrusion and intrusion formation in fatigued crystalline materials10.1016/j.msea.2013.12.005 ↗
24. Magnesium: an update on physiological, clinical and analytical aspects10.1016/S0009-8981(99)00258-2 ↗
25. Thermal stability of magnesium alloy AZ91 prepared by severe plastic deformation
26. Paradox of strength and ductility in metals processed by severe plastic deformation10.1557/JMR.2002.0002 ↗
27. Room temperature corrosion properties of AZ31 magnesium alloy processed by extrusion and equal channel angular pressing10.1007/s10853-013-7173-4 ↗
28. The effect of pre-processing and grain structure on the bio-corrosion and fatigue resistance of magnesium alloy AZ3110.1002/adem.200700200 ↗
29. In vitro and in vivo corrosion measurements of magnesium alloys10.1016/j.biomaterials.2005.07.037 ↗
30. Characterization of the fatigue behaviour of the magnesium alloy AZ91D by means of mechanical hysteresis and temperature measurements10.1016/j.ijfatigue.2004.04.005 ↗
31. Chemistry and biochemistry of magnesium10.1016/S0098-2997(02)00087-0 ↗
32. Improving the mechanical properties of magnesium and a magnesium alloy through severe plastic deformation10.1016/S0921-5093(00)01660-9 ↗