journal article·2016-06

3D analysis of thermal and stress evolution during laser cladding of bioactive glass coatings

Michal Krzyzanowski, Szymon Bajda, Yijun Liu, Andrew Triantaphyllou, W. Mark Rainforth, Malcolm Glendenning

Publisher page

Abstract

Thermal and strain-stress transient fields during laser cladding of bioactive glass coatings on the Ti6Al4V alloy basement were numerically calculated and analysed. Conditions leading to micro-cracking susceptibility of the coating have been investigated using the finite element based modelling supported by experimental results of microscopic investigation of the sample coatings. Consecutive temperature and stress peaks are developed within the cladded material as a result of the laser beam moving along the complex trajectory, which can lead to micro-cracking. The preheated to 500°C base plate allowed for decrease of the laser power and lowering of the cooling speed between the consecutive temperature peaks contributing in such way to achievement of lower cracking susceptibility. The cooling rate during cladding of the second and the third layer was lower than during cladding of the first one, in such way, contributing towards improvement of cracking resistance of the subsequent layers due to progressive accumulation of heat over the process.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Bone Tissue Engineering Materials · High Entropy Alloys Studies · Additive Manufacturing Materials and Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (56)

Show source-provided references
1. 〈http://www.engineeringtoolbox.com/emissivity-coefficients-d_447.html〉
2. Bioactive sol-gel scaffolds with dual porosity for tissue engineering
3. Arstila H., Vedel E., Hupa L., Hupa M. Predicting physical and chemical properties of bioactive glasses from chemical composition. Part 2: devitrification characteristics, Glass Technology: European Journal of Glass Science and Technology, Part A, 49(6), 260–265.
4. Silicon in living organisms and new generation biocomposite materials (review)10.1007/s10717-009-9136-4 ↗
5. Bioglass thin films for biomimetic implants10.1016/j.apsusc.2008.08.020 ↗
6. Studies on a novel bioactive glass and composite coating with hydroxyapatite on titanium based alloys: effect of γ-sterilization on coating10.1016/j.jeurceramsoc.2009.02.013 ↗
7. Microstructural and in vitro characterisation of high-velocity suspension flame sprayed (HVSFS) bioactive glass coatings10.1016/j.jeurceramsoc.2009.01.032 ↗
8. Chassaing G., Pougis A., Philippon S., Lipinski P., Meriaux J. Experimental and numerical study of frictional heating during rapid interactions of a Ti6Al4V tribopair, Wear, 〈doi:10.1016/j.wear.2015.09.013〉10.1016/j.wear.2015.09.013 ↗
9. Synthesis of Fe–Cr–C–W using laser cladding technique10.1007/BF00376268 ↗
10. Laser cladding of bioactive glass coatings10.1016/j.actbio.2009.08.010 ↗
11. Three-dimentional bioactive glass implants fabricated by rapid prototyping based on CO2 laser cladding10.1016/j.actbio.2011.05.023 ↗
12. Electrophoretic deposition: from traditional ceramics to nanotechnology10.1016/j.jeurceramsoc.2007.12.011 ↗
13. Pulsed laser ablation and deposition of bioactive glass as coating material for biomedical applications10.1016/S0169-4332(98)00610-2 ↗
14. Numerical contribution to the comprehension of saw-toothed Ti6Al4V chip formation in orthogonal cutting10.1016/j.ijmecsci.2014.02.017 ↗
15. Preparation and characterisation of sol-gel bioactive glass coating for improvement of biocompatibility of human body implant10.1016/j.msea.2007.05.041 ↗
16. Bioactive glass nanopowder and bioglass coating for biocompatibility improvement of metallic implant10.1016/j.jmatprotec.2008.03.051 ↗
17. Functionally graded bioactive coatings: reproducibility and stability of the coating under cell culture conditions10.1016/j.actbio.2005.12.003 ↗
18. Fixation of hip prostheses by hydroxyapatite ceramic coatings10.1302/0301-620X.73B5.1654336 ↗
19. Bioactive glass coating: physicochemical aspects and biological findings10.1016/0142-9612(95)91123-G ↗
20. Bioactive and protective sol-gel coatings on metals for orthopaedic prostheses10.1023/A:1011257516468 ↗
21. Bioactive glass and glass–ceramic scaffolds for bone tissue engineering10.3390/ma3073867 ↗
22. Additive manufacturing of bioactive glasses and silicate bioceramics
23. Bioactive® glass coatings with hydroxyapatite and bioglass particles on Ti-based implants. 1. Processing10.1016/S0142-9612(99)00131-3 ↗
24. Bioceramics: from concept to clinic10.1111/j.1151-2916.1991.tb07132.x ↗
25. Biomaterials: a forecast for the future10.1016/S0142-9612(98)00133-1 ↗
26. Genetic design of bioactive glass10.1016/j.jeurceramsoc.2008.08.002 ↗
27. Hench · 1993
28. Thermal spray: current status and future trends10.1557/mrs2000.119 ↗
29. Mediation of bone ingrowth in porous hydroxyapatite bone graft substitutes10.1002/jbm.a.10050 ↗
30. Comparison of bioactive glasses in vitro and in vivo
31. Some aspects of laser surface-cladding in the turbine industry10.1016/S0257-8972(00)00735-0 ↗
32. High-velocity suspention flame spraying (HVSFS), a new approach for spraying nanoparticles with hypersonic speed10.1016/j.surfcoat.2006.04.034 ↗
33. Surface bio-modification of titanium implants by an enamel process
34. Formation of a high-strength bioactive glass-ceramic in the system MgO-CaO-SiO2-P2O510.1007/BF01145520 ↗
35. Laser induced porosity and crystallinity modification of a bioactive glass coating on titanium substrates10.1115/1.4029566 ↗
36. Preparation and charcterisation of macroporous sol-gel bioglass10.1016/j.ceramint.2004.05.011 ↗
37. Bioactive glass coatings for orthopaedic metallic implants10.1016/S0955-2219(03)00303-0 ↗
38. Production of calcium phosphate coatings on Ti6Al4V obtained by Nd:yttrium-aluminum-garnet laser cladding10.1063/1.1402975 ↗
39. Calcium phosphate coatings obtained by Nd:YAG laser cladding: physico-chemical and biological properties10.1002/jbm.a.10440 ↗
40. Main characteristics of calcium phosphate coatings obtained by laser cladding10.1016/j.apsusc.2005.01.134 ↗
41. Effective thermal conductivity of soda-lime silicate glassmelts with different iron contents between 1100°C and 1500°C10.1111/jace.12768 ↗
42. Biocompatable and bioactive nanostructured glass coatings synthesized by pulsed laser deposition: in vitro biological tests10.1016/j.apsusc.2008.10.031 ↗
43. Laser cladding and erosive wear of Co–Mo–Cr–Si coatings10.1016/S0257-8972(99)00563-0 ↗
44. Mathematical modelling and integration of micro-scale residual stresses into axisymmetric FE models of Ti6Al4V alloy in turning10.1016/j.cirpj.2011.03.002 ↗
45. In vitro behavior of silicate glass coatings on Ti6Al4V10.1016/S0142-9612(02)00109-6 ↗
46. Laser cladding of aerospace materials10.1016/S0924-0136(01)01121-9 ↗
47. Shabnam Hosseini, 2012. Fatigue of Ti-6Al-4V, Biomedical Engineering – Technical Applications in Medicine, Dr. Radovan Hudak (Ed.), ISBN: 978-953-51-0733-0, InTech, DOI: 10.5772/45753. Available from: 〈http://www.intechopen.com/books/biomedical-engineering-technical-applications-in-medicine/fatigue-of-ti-6al-4v〉10.5772/45753 ↗
48. Bioactive glass coatings: a review10.1179/1743294410Y.0000000008 ↗
49. Elastic properties of substituted 45S5 bioactive glasses and glass–ceramics
50. Nanomechanical properties evaluation of bioactive glass coatings on titanium alloy substrate
51. Thermally assisted hydroxyapatite obtained by pulse-laser deposition on titanium substrates10.1016/0040-6090(93)90183-P ↗
52. Vedel E., Arstila H., Ylänen H., Hupa L., Hupa M. Predicting physical and chemical properties of bioactive glasses from chemical composition. Part 1: viscosity characteristics. Glass Technology: European Journal of Glass Science and Technology, Part A, 49(6), 251–259.
53. Synthethis and characterization of porous silica gels for biomedical applications
54. In situ synthesis of hydroxyapatite coating by laser cladding10.1016/j.colsurfb.2008.06.003 ↗
55. 2011
56. Experimental investigation and 3D finite element prediction of the heat affected zone during laser assisted machining of Ti6Al4V alloy10.1016/j.jmatprotec.2010.08.007 ↗