Evaluation of four surface coating treatments for resin to zirconia bonding
Source abstract
Abstract
Objectives To compare the effects of four surface coating methods on resin to zirconia shear bond strength. Material and methods Eighty pre-sintered zirconia discs were prepared and randomly divided into five study groups according to the corresponding methods of surface treatments as follows: group C (control group, fully sintered without any surface treatment), group S (fully sintered and then sandblasted with silica coated alumina powder), group G (fully sintered and then coated with glazing porcelain followed by acid etching), group Si (pre-coated with silica slurry then fully sintered), and group Z (coated with zirconia particles and then fully sintered). The observation of surface morphology and elemental composition analysis were conducted by SEM and EDX. Self-adhesive resin cement stubs (diameter 3.6mm and height 3mm) were then bonded on the zirconia discs with a cylindrical shape. Both initial and artificial aged (including 30-day water storage, thermal cycling for 3000 and 6000 cycles) shear bond strengths were then evaluated. Results All the tested coating methods showed significantly higher shear bond strengths than the control group, in both dry and aged conditions. Group S produced the strongest initial zirconia/resin bonding (19.7MPa) and the control group had the lowest value (8.8MPa). However, after thermal cycling, group Z exhibited the highest mean value. All the samples in the control group failed in the thermal cycling. Both different coating methods (p<0.001) and various aging treatments (p<0.001) produced significant influence on resin-zirconia shear bond strength. Conclusions A reliable and durable resin zirconia bonding is vital for the longevity of dental restorations. Silica coating might be a reliable way in enhancing adhesion between resin and zirconia.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Endodontics and Root Canal Treatments · Dental Erosion and Treatment
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. Zirconia ceramic inlay-retained fixed dental prostheses – first clinical results with a new design10.1016/j.jdent.2010.12.005 ↗
2. Fusion sputtering for bonding to zirconia-based materials
3. Innovations in bonding to zirconia-based materials. Part II: focusing on chemical interactions10.1016/j.dental.2009.02.011 ↗
4. Effect of zirconium-oxide ceramic surface treatments on the bond strength to adhesive resin10.1016/j.prosdent.2006.03.016 ↗
5. Effect of an experimental zirconia–silica coating technique on micro tensile bond strength of zirconia in different priming conditions10.1016/j.dental.2012.04.020 ↗
6. Comparison of alternative adhesive cementation concepts for zirconia ceramic: Glaze layer vs zirconia primer
7. Effect of surface treatments on the bond strength of a zirconia-reinforced ceramic to composite resin10.1590/S1806-83242007000100002 ↗
8. Improved bonding of zirconia substructures to resin using a “glaze-on” technique10.1016/j.jdent.2011.12.011 ↗
9. Influence of surface and heat treatments on the flexural strength of y-tzp dental ceramic10.1016/j.jdent.2004.07.001 ↗
10. Effect of operating air pressure on tribochemical silica-coating10.1080/00016350701459753 ↗
11. Dental zirconia adhesion with silicon compounds using some experimental and conventional surface conditioning methods10.1007/s12633-009-9022-2 ↗
12. Insights on ceramics as dental materials. Part I: ceramic material types in dentistry10.1007/s12633-011-9078-7 ↗
13. Insights on ceramics as dental materials. Part II: chemical surface treatments.10.1007/s12633-011-9079-6 ↗
14. ISO, 2004. International organization for standardization: dentistry-polymer-based crown and bridge materials. ISO 10477, Amendment: 2004.
15. Influence of surface treatments on surface roughness, phase transformation, and biaxial flexural strength of y-tzp ceramics10.1002/jbm.b.31477 ↗
16. Resin bonding to oxide ceramics for dental restorations10.1163/156856109X432721 ↗
17. Surface conditioning influences zirconia ceramic bonding10.1177/0022034509340881 ↗
18. Bonding to zirconia ceramic: adhesion methods and their durability10.1016/S0109-5641(98)00011-6 ↗
19. Effect of an internal coating technique on tensile bond strengths of resin cements to zirconia ceramics10.4012/dmj.28.446 ↗
20. Effect of surface treatment on bond strength between an indirect composite material and a zirconia framework10.2334/josnusd.54.39 ↗
21. The effect of surface grinding and sandblasting on flexural strength and reliability of y-tzp zirconia ceramic10.1016/S0109-5641(99)00070-6 ↗
22. Strength and reliability of surface treated y-tzp dental ceramics10.1002/1097-4636(2000)53:4<304::AID-JBM4>3.0.CO;2-S ↗
23. The effect of surface grinding and sandblasting on flexural strength and reliability of y-tzp zirconia ceramic10.1016/S0109-5641(99)00070-6 ↗
24. Insights into porcelain to zirconia bonding10.1163/156856111X593586 ↗
25. A new modified laser pretreatment for porcelain zirconia bonding10.1016/j.dental.2013.03.002 ↗
26. The effect of silica-coating by sol–gel process on resin–zirconia bonding10.4012/dmj.2012-100 ↗
27. Resin bonding to silicatized zirconia with two isocyanatosilanes and a cross-linking silane. Part I: experimental10.1007/s12633-010-9044-9 ↗
28. Surface modification of silica-coated zirconia by chemical treatments10.1016/j.apsusc.2010.08.029 ↗
29. Aspects of silane coupling agents and surface conditioning in dentistry: an overview10.1016/j.dental.2012.02.009 ↗
30. An overview of zirconia ceramics: basic properties and clinical applications10.1016/j.jdent.2007.07.008 ↗
31. Bonding promotion of resin composite to silica-coated zirconia implant surface using a novel silane system10.1111/j.1600-0501.2012.02525.x ↗
32. Enhanced resin-composite bonding to zirconia framework after pretreatment with selected silane monomers10.1016/j.dental.2010.11.002 ↗
33. Microstructural changes produced by abrading y-tzp in presintered and sintered conditions10.1016/j.jdent.2012.06.009 ↗
34. Effect of surface treatment on the initial bond strength of different luting cements to zirconium oxide ceramic10.1007/s00784-008-0222-8 ↗
35. All-ceramic inlay-retained fixed partial dentures: preliminary results from a clinical study10.1016/j.jdent.2008.04.017 ↗
36. Comparison of resin cement adhesion to y-tzp ceramic following manufacturers' instructions of the cements only10.1007/s00784-007-0151-y ↗
37. Effect of surface conditioning methods on the bond strength of luting cement to ceramics10.1016/S0109-5641(03)00019-8 ↗
38. Silicoating: evaluation of a new method of bonding composite resin to metal10.1111/j.1600-0722.1988.tb01425.x ↗
39. Surface modification for enhanced silanation of zirconia ceramics10.1016/j.dental.2009.03.008 ↗
40. Zirconia as a ceramic biomaterial10.1016/S0142-9612(98)00010-6 ↗
41. The shear bond strength between luting cements and zirconia ceramics after two pre-treatments
42. CAD/CAM single retainer zirconia-ceramic resin-bonded fixed dental prostheses: clinical outcome after 5 years
43. Cooperation of phosphate monomer and silica modification on zirconia10.1177/154405910808700705 ↗
44. Evaluation of a conditioning method to improve core–veneer bond strength of zirconia restorations10.1016/S0022-3913(12)60095-X ↗
45. Adhesion/cementation to zirconia and other non-silicate ceramics: where are we now?10.1016/j.dental.2010.10.022 ↗
46. Influence of glazed zirconia on dual-cure luting agent bond strength10.2341/10-220-L ↗
47. Effect of sandblasting on the long-term performance of dental ceramics10.1002/jbm.b.30097 ↗