journal article·2018-01

Low temperature degradation of single layers of multilayered zirconia in comparison to conventional unshaded zirconia: Phase transformation and flexural strength

Sebastian Wille, Paul Zumstrull, Victor Kaidas, Lea Katharina Jessen, Matthias Kern

Publisher page

Abstract

Objectives The aim of this study was to evaluate the transformation of yttrium stabilized tetragonal zirconia (Y-TZP) to monoclinic phase and its change in flexural strength of the various layers of multilayered zirconia (enamel layer, transition layer 1, transition layer 2 and body layer) in comparison to two conventional zirconia ceramics. Additionally, the ball-on-three-balls test was compared with a conventional biaxial flexural strength test. Methods The crystallographic structure of the four layers of Katana Zirconia ML (Kuraray), e.max ZirCAD (Ivoclar Vivadent) and Lava Plus (3M ESPE) was investigated by x-ray-diffraction before and after hydrothermal aging in an autoclave for 5, 10, 15 and 20h. The biaxial flexural strength was examined with a piston-on-three-ball test and a ball-on-three-balls test. Results There was a significant difference of the ratio of transformation with respect to the tested materials, also between the four different layers of multilayered zirconia. After 20h of hydrothermal aging the mean ratio of monoclinic phase ranged from 9.9vol% (LAVA Plus) to 44.2vol% (Katana Zirconia ML, enamel layer). However, hydrothermal aging had no significant influence on the flexural strength of any material. Furthermore, the flexural strength measured by the ball-on-three-balls test was higher than that measured by the piston-on-three-ball test. Conclusion A ratio of 40% monoclinic phase at the surface did not significantly influence the biaxial flexural strength. Both test methods provide reliable results. However, as the ball-on-three balls test is less dependent on surface roughness, it might be preferred for investigations adapted to clinical reality.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Advanced ceramic materials synthesis · Bone Tissue Engineering Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. Air abrasion before and/or after zirconia sintering: surface characterization, flexural strength, and resin cement bond strength10.2341/14-013-LR1 ↗
2. Low-temperature degradation of a Y-TZP ceramic after surface treatments10.1002/jbm.b.32957 ↗
3. In vitro performance of full-contour zirconia single crowns10.1016/j.dental.2011.11.024 ↗
4. The ball on three balls test for strength testing of brittle discs: stress distribution in the disc10.1016/S0955-2219(01)00458-7 ↗
5. Low-temperature aging of Y-TZP ceramics10.1111/j.1151-2916.1999.tb02055.x ↗
6. Low-temperature degradation of zirconia and implications for biomedical implants10.1146/annurev.matsci.37.052506.084250 ↗
7. Effect of accelerated aging on dental zirconia-based materials10.1016/j.jmbbm.2016.08.023 ↗
8. Zirconia dental implants degradation by confocal Raman microspectroscopy: analytical simulation and experiments10.1364/BOE.4.000725 ↗
9. Effect of changes in sintering parameters on monolithic translucent zirconia10.1016/j.dental.2014.09.003 ↗
10. Factors affecting the mechanical behavior of Y-TZP10.1016/j.jmbbm.2014.05.013 ↗
11. Accelerated aging characteristics of three yttria-stabilized tetragonal zirconia polycrystalline dental materials10.1016/S0022-3913(12)60166-8 ↗
12. Influence of aging on flexural strength of translucent zirconia for monolithic restorations10.1016/j.prosdent.2016.06.010 ↗
13. Montan Universität - Institut für Struktur- und Funktionskeramik. Ball-on-3-Balls Test (B3B) – Strength Testing. 〈http://www.isfk.at/de/960/〉. (Accessed 22 September 2016).
14. Phase analysis in zirconia systems10.1111/j.1151-2916.1972.tb11290.x ↗
15. Effect of stress-induced phase transformation on the properties of polycrystalline zirconia containing metastable tetragonal phase10.1007/BF00553200 ↗
16. Effect of surface treatments on the properties and morphological change of dental zirconia10.1016/j.prosdent.2015.09.007 ↗
17. Catastrophic failure of modular zirconia-ceramic femoral head components after total hip arthroplasty10.1016/S0883-5403(05)80085-3 ↗
18. Aging resistance of surface-treated dental zirconia10.1016/j.dental.2014.11.018 ↗
19. Fracture strength of monolithic all-ceramic crowns made of high translucent yttrium oxide-stabilized zirconium dioxide compared to porcelain-veneered crowns and lithium disilicate crowns10.3109/00016357.2013.822098 ↗
20. Ageing of dental zirconia ceramics10.1016/j.jeurceramsoc.2012.02.024 ↗
21. Low temperature degradation -aging- of zirconia: a critical review of the relevant aspects in dentistry10.1016/j.dental.2010.04.006 ↗
22. The influences of accelerated aging on mechanical properties of veneering ceramics used for zirconia restorations10.4012/dmj.2015-115 ↗
23. An overview of zirconia ceramics: basic properties and clinical applications10.1016/j.jdent.2007.07.008 ↗
24. Effect of air-abrasion regimens and fine diamond bur grinding on flexural strength, Weibull modulus and phase transformation of zirconium dioxide
25. Effects of airborne-particle abrasion protocol choice on the surface characteristics of monolithic zirconia materials and the shear bond strength of resin cement10.1016/j.ceramint.2015.09.104 ↗
26. Effect of low-temperature degradation on the mechanical and microstructural properties of tooth-colored 3Y-TZP ceramics10.1016/j.jmbbm.2015.08.031 ↗
27. Translucency and low-temperature degradation of silica-doped zirconia: a pilot study10.4012/dmj.2015-274 ↗
28. Catastrophic failure of the Elite Plus total hip replacement, with a hylamer acetabulum and zirconia ceramic femoral head10.1302/0301-620X.84B5.0840631 ↗
29. Effect of air-particle abrasion protocols on the biaxial flexural strength, surface characteristics and phase transformation of zirconia after cyclic loading10.1016/j.jmbbm.2013.01.005 ↗
30. Towards long lasting zirconia-based composites for dental implants. Part I: innovative synthesis, microstructural characterization and in vitro stability10.1016/j.biomaterials.2015.01.018 ↗
31. The effect of air-abrasion and heat treatment on the fracture behavior of Y-TZP10.1016/j.dental.2015.05.008 ↗
32. Effect of low-temperature aging on the mechanical behavior of ground Y-TZP10.1016/j.jmbbm.2014.12.009 ↗
33. Low-temperature degradation of Y-TZP ceramics: a systematic review and meta-analysis10.1016/j.jmbbm.2015.10.017 ↗
34. Zirconia as a ceramic biomaterial10.1016/S0142-9612(98)00010-6 ↗
35. Flexural strength and Weibull analysis of a microhybrid and a nanofill composite evaluated by 3- and 4-point bending tests10.1016/j.dental.2007.05.013 ↗
36. The combined effect of alumina and silica co-doping on the ageing resistance of 3Y-TZP bioceramics10.1016/j.actbio.2014.09.009 ↗
37. Influence of coloring procedure on flexural resistance of zirconia blocks10.1016/j.prosdent.2015.02.001 ↗
38. Effect of in vitro aging on the flexural strength andprobability to fracture of Y-TZP zirconia ceramicsfor all-ceramic restorations10.1016/j.dental.2014.05.033 ↗
39. Fracture strength and microstructure of Y-TZP zirconia after different surface treatments10.1016/S0022-3913(13)60376-5 ↗
40. Comparison of four monolithic zirconia materials with conventional ones: contrast ratio, grain size, four-point flexural strength and two-body wear10.1016/j.jmbbm.2015.11.040 ↗
41. Effects of core-to-dentin thickness ratio on the biaxial flexural strength, reliability, and fracture mode of bilayered materials of zirconia core (Y-TZP) and veneer indirect composite resins10.1016/j.prosdent.2016.04.017 ↗
42. The effect of staining and vacuum sintering on optical and mechanical properties of partially and fully stabilized monolithic zirconia10.4012/dmj.2015-054 ↗
43. Calibration curve for quantitative analysis of the monoclinic-tetragonal ZrO2 system by x-ray diffraction10.1111/j.1151-2916.1984.tb19614.x ↗
44. Flexural strength and fracture toughness of dental core ceramics10.1016/S0022-3913(07)60045-6 ↗
45. Highly-translucent, strong and aging-resistant 3Y-TZP ceramics for dental restoration by grain boundary segregation10.1016/j.actbio.2015.01.037 ↗
46. Making yttria-stabilized tetragonal zirconia translucent10.1016/j.dental.2014.08.375 ↗