journal article·2016-03

Retrieval analysis of titanium nitride (TiN) coated prosthetic femoral heads articulating with polyethylene

Łukasz Łapaj, Justyna Wendland, Jacek Markuszewski, Adrian Mróz, Tomasz Wiśniewski

Publisher page

Abstract

Data regarding in vivo performance of titanium nitride (TiN) coated prosthetic femoral heads is scarce, and available studies of older generations of implants demonstrated coating wear in vivo. That is why we conducted a retrieval analysis of 11 femoral heads (articulating in vivo for 1-56 months) with TiN film formed using physical vapor deposition (PVD), to verify if coating failure is a problem in contemporary implants. Retrieved implants were examined using scanning electron microscope, coating roughness was evaluated with a contact profilometer and adhesion was tested using a Rockwell HRC test according to VDI 3824 guideline. Although no gross failure of the TiN coating was observed in our retrievals, all implants had defects typical for PVD coatings, such as pinholes, small titanium droplets and blisters with delaminated coating. In some heads the coating was contaminated with small niobium (Nb) droplets uniformly scattered on the entire surface of the film. Presence of Nb contamination was associated with an increased number and area of other types of defects and poorer coating adhesion. In one component, subjected to multiple dislocations we found severe delamination and cracking of the coating, increased roughness and the presence of third bodies. Our results indicate, that although wear of the coating is lower than seen in older generations of implants, inconsistent quality of the TiN film among different implants indicates the need for strict monitoring of the manufacturing process.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Orthopaedic implants and arthroplasty · Metal and Thin Film Mechanics · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Effect of target frequency, bias voltage and bias frequency on microstructure and mechanical properties of pulsed DC CFUBM sputtered TiN coating10.1016/j.surfcoat.2010.04.047 ↗
2. Buechel F.F., Sr., Buechel F.F., Jr., Helbig T.E., D’Alessio J. and Pappas M.J., Two-to 12-year evaluation of cementless Buechel‐PappasBuechel–Pappas total hip arthroplasty, The Journal of arthroplasty.J. Arthroplast. 19 (8), 2004, 1017–102710.1016/j.arth.2004.06.030 ↗
3. Antibacterial properties and cytocompatibility of tantalum oxide coatings10.1016/j.surfcoat.2014.03.061 ↗
4. DOT GmbH (Rostock, Germany), 2015. Optimised protection against allergic reactions and wear through the use of durable ceramic coatings. 〈http://www.dot-coating.de/1/coatings/ortho/pvd-coating/tin/〉 (last entry 05-NOV-2015).
5. The effect of the sputter cleaning of steel substrates with neutral molecule source on the adhesion of TiN films10.1016/S0257-8972(97)00189-8 ↗
6. Surface damage to an oxinium femoral head prosthesis after dislocation10.1302/0301-620X.89B4.17557 ↗
7. Abrasion resistance of oxidized zirconium in comparison with CoCrMo and titanium nitride coatings for artificial knee joints10.1002/jbm.b.31581 ↗
8. Potential for adhesive wear in friction couples of UHMWPE running against oxidized zirconium, titanium nitride coatings, and cobalt–chromium alloys10.1002/jbm.b.31604 ↗
9. Thermal characterization of commercially pure titanium for dental applications10.1590/S1516-14392007000300004 ↗
10. Tribological examination of lumbar intervertebral disc implants10.3103/S1068366613040041 ↗
11. The effect of roughness on the tribological behavior of the prosthetic pair UHMWPE/TiN-coated stainless steel10.1002/jbm.b.30849 ↗
12. The electrochemical and mechanical behavior of passivated and TiN/AlN-coated CoCrMo and Ti6Al4V alloys10.1016/S0142-9612(03)00606-9 ↗
13. Polyethylene particles of a “critical size” are necessary for the induction of cytokines by macrophages in vitro10.1016/S0142-9612(98)00140-9 ↗
14. PIRAC Ti nitride coated Ti–6Al–4V head against UHMWPE acetabular cup–hip wear simulator study
15. Wear analysis of a retrieved hip implant with titanium nitride coating10.1016/S0883-5403(97)90164-9 ↗
16. Reducing the macroparticle content of cathodic arc evaporated TiN coatings10.1016/j.surfcoat.2003.08.086 ↗
17. The fretting corrosion resistance of PVD surface-modified orthopedic implant alloys10.1002/1097-4636(2001)58:2<156::AID-JBM1002>3.0.CO;2-H ↗
18. Surface roughness of ceramic femoral heads after in vivo transfer of metal: correlation to polyethylene wear
19. Damage of oxinium femoral heads subsequent to hip arthroplasty dislocation: three retrieval case studies10.1016/j.arth.2006.07.005 ↗
20. The influence of TiN coatings properties on cavitation erosion resistance10.1016/j.surfcoat.2009.07.014 ↗
21. Potential of coatings in total hip replacement. Clinical orthopaedics and related research
22. The role of the growth defects on the corrosion resistance of CrN/NbN superlattice coatings deposited at low temperatures10.1016/j.tsf.2005.08.375 ↗
23. Tribological and electrochemical performance of PVD TiN coatings on the femoral head of Ti–6Al–4V artificial hip joints10.1016/S0257-8972(02)00630-8 ↗
24. Comparison of surface characteristics of retrieved cobalt–chromium femoral heads with and without ion implantation10.1016/j.arth.2011.03.009 ↗
25. Design and performance of the microdroplet filtering system used in cathodic arc coating deposition10.1016/S1288-3255(00)01021-2 ↗
26. Quantification of third-body damage and its effect on UHMWPE wear with different types of femoral head10.1302/0301-620X.80B5.0800894 ↗
27. Radiographic and retrieval wear analyses of the first generation highly cross-linked polyethylene cup against a ceramic femoral head10.1002/jbm.b.32929 ↗
28. Growth defects in PVD hard coatings10.1016/j.vacuum.2009.05.018 ↗
29. Quantitative evaluation of the prosthetic head damage induced by microscopic third-body particles in total hip replacement10.1002/jbm.1039 ↗
30. The current state of bearing surfaces in total hip replacement10.1302/0301-620X.96B2.31920 ↗
31. High power pulsed magnetron sputtering: a review on scientific and engineering state of the art10.1016/j.surfcoat.2009.11.013 ↗
32. A comparative study of titanium nitrides, TiN, TiNbN and TiCN, as coatings for biomedical applications10.1016/j.surfcoat.2009.06.010 ↗
33. What’s next? Alternative materials for articulation in total joint replacement10.1016/j.actbio.2012.03.029 ↗
34. Numerical and experimental study of the circular cracks observed at the contact edges of the indentations of coated systems with soft substrates10.1016/S0043-1648(01)00778-5 ↗
35. The in-vivo wear performance of prosthetic femoral heads with titanium nitride coating10.1016/S0142-9612(99)00246-X ↗
36. VDI (The Association of German Engineers), 2001-08. VDI 3824 Part 4: Quality assurance of PVD and CVD hard coating - Inspection planning of hard coatings.
37. The VDI 3198 indentation test evaluation of a reliable qualitative control for layered compounds10.1016/S0924-0136(03)00300-5 ↗
38. Effect of femoral head surface roughness on the wear of ultrahigh molecular weight polyethylene acetabular cups10.1016/S0883-5403(98)80002-8 ↗