Fatigue limit of polycrystalline zirconium oxide ceramics: Effect of grinding and low-temperature aging
Source abstract
Abstract
The following study aimed to evaluate the effect of grinding and low-temperature aging on the fatigue limit of Y-TZP ceramics for frameworks and monolithic restorations. Disc specimens from each ceramic material, Lava Frame (3M ESPE) and Zirlux FC (Ivoclar Vivadent) were manufactured according to ISO:6872-2008 and assigned in accordance with two factors: (1) "surface treatment"-without treatment (as-sintered, Ctrl), grinding with coarse diamond bur (181µm; Grinding); and (2) "low-temperature aging (LTD)" - presence and absence. Grinding was performed using a contra-angle handpiece under constant water-cooling. LTD was simulated in an autoclave at 134°C under 2-bar pressure for 20h. Mean flexural fatigue limits (20,000 cycles) were determined under sinusoidal loading using stair case approach. For Lava ceramic, it was observed a statistical increase after grinding procedure and different behavior after LTD stimuli (Ctrl<Grinding; Ctrl<Ctrl Ltd; Grinding=Grinding Ltd); while for Zirlux, grinding and low-temperature aging promoted a statistical increase in the fatigue limit (Ctrl<Grinding; Ctrl<Ctrl Ltd; Grinding<Grinding Ltd). An important increase was observed in m-phase content after both stimuli (grinding and LTD), although with different intensities. Additionally, fatigue test did not promote increase of m-phase content. Thus, tested grinding and low temperature aging did not damage the fatigue limit values significantly for both materials evaluated, even though those conditions promoted increase in m-phase.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (56)
Show source-provided references
1. Bridging the gap between clinical failure and laboratory fracture strength tests using a fractographic approach10.1016/j.dental.2008.09.001 ↗
2. Low-temperature degradation of a Y-TZP ceramic after surface treatments10.1002/jbm.b.32957 ↗
3. Biaxial flexure strength and low temperature degradation of Ce-TZP/ Al2O3 nanocomposite and Y-TZP as dental restoratives10.1002/jbm.b.31131 ↗
4. Prospective study of zirconia-based restorations: 3-year clinical results
5. In vitro performance of full-contour zirconia single crowns10.1016/j.dental.2011.11.024 ↗
6. Biofilm and saliva affect the biomechanical behavior of dental implants10.1016/j.jbiomech.2015.02.004 ↗
7. Low-temperature degradation of zirconia and implications for biomedical implants10.1146/annurev.matsci.37.052506.084250 ↗
8. A clinical comparison of zirconia, metal and alumina fixed-prosthesis frameworks veneered with layered or pressed ceramic: a three-year report10.14219/jada.archive.2010.0076 ↗
9. Collins · 1992
10. Effects of aging procedures on the topographic surface, structural stability, and mechanical strength of a ZrO2-based dental ceramic10.1016/j.dental.2014.08.380 ↗
11. Emerging ceramic-based materials for dentistry10.1177/0022034514553627 ↗
12. Factors affecting the mechanical behaviour of Y-TZP10.1016/j.jmbbm.2014.05.013 ↗
13. Accelerated aging characteristics of three yttria-stabilized tetragonal zirconia polycrystalline dental materials10.1016/S0022-3913(12)60166-8 ↗
14. Effect of hydrothermal degradation on three types of zirconias for dental application10.1016/j.prosdent.2014.07.015 ↗
15. Phase analysis in zirconia systems10.1111/j.1151-2916.1972.tb11290.x ↗
16. Slow crack growth and reliability of dental ceramics10.1016/j.dental.2010.10.025 ↗
17. Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic10.1016/j.jdent.2004.07.001 ↗
18. Transformation toughening in zirconia-containing ceramics10.1111/j.1151-2916.2000.tb01221.x ↗
19. A review of the strength properties of dental ceramics10.1016/0022-3913(92)90602-7 ↗
20. Influence of sintering conditions on low temperature degradation of dental zirconia10.1016/j.dental.2014.03.005 ↗
21. Aging resistance of surface-treated dental zirconia10.1016/j.dental.2014.11.018 ↗
22. ISO, 6872, 2008. Dentistry – dental ceramics. Int. Organ. Stand.
23. Clinically relevant approach to failure testing of all-ceramic restorations10.1016/S0022-3913(99)70103-4 ↗
24. Dental ceramics: current thinking and trends10.1016/j.cden.2004.01.003 ↗
25. Development of clinically validated bulk failure test for ceramic crowns10.1016/S0022-3913(10)60129-1 ↗
26. The effect of low temperature aging on the mechanical property and phase stability of YTZP ceramics10.4047/jap.2009.1.3.113 ↗
27. Phase change and mechanical properties of ZrO2–Y2O3 solid electrolyte after ageing10.1016/0167-2738(81)90138-7 ↗
28. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic10.1016/S0109-5641(99)00070-6 ↗
29. The effects of dental grinding and sandblasting on ageing and fatigue behavior of dental zirconia (Y-TZP) ceramics10.1016/j.jeurceramsoc.2007.09.013 ↗
30. Y-TZP ceramic processing from coprecipitated powders: a comparative study with three commercial dental ceramics10.1016/j.dental.2008.04.002 ↗
31. Phase transformation in Y2O3-partially-stabilized ZrO2 polycrystals of various grain sizes during low-temperature aging in water10.1111/j.1151-2916.1998.tb02677.x ↗
32. Phase transformation of dental zirconia following artificial aging10.1002/jbm.b.33334 ↗
33. Effect of grain size on the monoclinic transformation, hardness, roughness, and modulus of aged partially stabilized zirconia10.1016/j.dental.2015.09.014 ↗
34. Subcritical crack growth behavior and life data analysis of two types of dental Y-TZP ceramics10.1016/j.dental.2011.03.010 ↗
35. Clinical evaluation of tooth-supported Zirconia-based fixed dental prostheses: a retrospective cohort study from the AIOP Clinical Research Group10.11607/ijp.4023 ↗
36. Hydrothermal degradation of ground 3Y TZP10.1016/j.jeurceramsoc.2011.08.029 ↗
37. The influence of low-temperature degradation and cyclic loading on the fracture resistance of monolithic zirconia crowns10.1016/j.jmbbm.2015.03.007 ↗
38. In vitro evaluation of low-temperature aging effects and finishing procedures on the flexural strength and structural stability of Y-TZP dental ceramics10.1016/j.prosdent.2006.08.004 ↗
39. Effect of grinding with diamond-disc and -bur on the mechanical behavior of a Y-TZP ceramic10.1016/j.jmbbm.2014.05.010 ↗
40. Effect of low-temperature aging on the mechanical behavior of ground Y-TZP10.1016/j.jmbbm.2014.12.009 ↗
41. Low-temperature degradation of Y-TZP ceramics: a systematic review and meta-analysis10.1016/j.jmbbm.2015.10.017 ↗
42. Zirconia as a ceramic biomaterial10.1016/S0142-9612(98)00010-6 ↗
43. Surface properties of monolithic zirconia after dental adjustment treatments and in vitro wear simulation10.1016/j.jdent.2014.08.011 ↗
44. On the nature of machining cracks in ground ceramics: Part I: SRBSN strengths and fractographic analysis10.1081/MST-200059038 ↗
45. NIST recommended practice guide: fractography of ceramics and glasses
46. The efficacy of posterior three-unit zirconium-oxide-based ceramic fixed partial dental prostheses: a prospective clinical pilot study10.1016/j.prosdent.2006.08.010 ↗
47. Full-contour Y-TZP ceramic surface roughness effect on synthetic hydroxiapatite wear10.1016/j.dental.2013.03.008 ↗
48. Five-year clinical results of zirconia frameworks for posterior fixed partial dentures
49. A systematic review of the survival and complication rates of all-ceramic and metal–ceramic reconstructions after an observation period of at least 3 years. Part II: fixed dental prostheses10.1111/j.1600-0501.2007.01468.x ↗
50. Control of the tetragonal to monoclinic phase transformation of yttria partially stabilized in hot water10.1007/BF00552389 ↗
51. Calibration curve for quantitative analysis of the monoclinic tetragonal ZrO2 system by X-rays diffraction10.1111/j.1151-2916.1984.tb19715.x ↗
52. Evaluation of hardness and fracture toughness, coupled with microstructural analysis, of zirconia ceramics stored in environments with different pH values10.4012/dmj.2012-005 ↗
53. Biaxial flexure tests of ceramic substrates
54. Stress fatigue: basic principles and prosthodontic implications
55. Role of H2O on the degradation process of Y-TZP10.1007/BF01756800 ↗
56. Zhang Y, Sailer I, Lawn BR. Fatigue of dental ceramics. J Dent, 2013;41(12):1135-1147.10.1016/j.jdent.2013.10.007 ↗