journal article·2016-01

Effect of low-temperature degradation on the mechanical and microstructural properties of tooth-colored 3Y-TZP ceramics

K. Nakamura, A. Harada, M. Ono, H. Shibasaki, T. Kanno, Y. Niwano, E. Adolfsson, P. Milleding, U. Örtengren

Publisher page

Abstract

The aim of the present study was to evaluate the effects of low-temperature degradation (LTD) induced by autoclaving on the mechanical and microstructural properties of tooth-colored 3 mol% yttria-stabilized tetragonal zirconia polycrystals (3Y-TZP). In total, 162 disc-shaped 3Y-TZP specimens were prepared. Two-thirds of the specimens were shaded by either the infiltration or powder mixing methods while the remaining specimens were used without coloring. The specimens were autoclaved at 134 °C for 0, 10, and 100 h to induce LTD (n=18 for each group). Chemical compositions were analyzed with X-ray fluorescence spectroscopy. Biaxial flexural strength was measured using a piston-on-three-ball test. The surface fraction and penetration depth of the monoclinic phase were examined using X-ray diffraction and scanning electron microscopy, respectively. The tooth-colored 3Y-TZP specimens contained Fe2O3 and Er2O3 (infiltration technique), and Fe2O3 (powder mixing method) at concentrations of<0.5 wt%. The tooth-colored 3Y-TZP had higher strength than the non-colored material after 100 h of autoclaving. In terms of surface fraction and penetration depth, the generation of monoclinic phase was significantly lower in the tooth-colored 3Y-TZP than in the non-colored material. The tooth-colored 3Y-TZP possessed equivalent biaxial flexural strength to that of the non-colored material and higher resistance to LTD regardless of the coloring technique (infiltration technique or powder mixing method) when the coloring pigments were contained at concentrations used in the present study.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Bone Tissue Engineering Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (48)

Show source-provided references
1. ASTM Standard E 112-13: Standard test methods for determining average grain size. West Conshohocken, PA, USA, 2014.
2. Is Weibull׳s modulus really a material constant? Example case with interacting collinear cracks10.1016/j.ijsolstr.2005.08.002 ↗
3. Transformation-toughened zirconia for dental inlays, crowns and bridges: chemical stability and effect of low-temperature aging on flexural strength and surface structure10.1016/S0109-5641(01)00095-1 ↗
4. In vitro performance of full-contour zirconia single crowns10.1016/j.dental.2011.11.024 ↗
5. Colored zirconia ceramics for dental applications
6. Low-temperature aging of Y-TZP ceramics10.1111/j.1151-2916.1999.tb02055.x ↗
7. Critical effect of cubic phase on aging in 3mol% yttria-stabilized zirconia ceramics for hip replacement prosthesis10.1016/j.biomaterials.2004.01.002 ↗
8. Low-temperature degradation of zirconia and implications for biomedical implants10.1146/annurev.matsci.37.052506.084250 ↗
9. The tetragonal-monoclinic transformation in zirconia: lessons learned and future trends10.1111/j.1551-2916.2009.03278.x ↗
10. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
11. A critical comparison of methods for the determination of the aging sensitivity in biomedical grade yttria-stabilized zirconia
12. Yttria tetragonal zirconia biomaterials: kinetic investigation10.1016/S1005-0302(11)60070-4 ↗
13. Accelerated aging characteristics of three yttria-stabilized tetragonal zirconia polycrystalline dental materials10.1016/S0022-3913(12)60166-8 ↗
14. Phase analysis in zirconia systems10.1111/j.1151-2916.1972.tb11290.x ↗
15. Ceramic steel?10.1038/258703a0 ↗
16. Combining ageing and wear to assess the durability of zirconia-based ceramic heads for total hip arthroplasty10.1016/j.actbio.2013.03.030 ↗
17. A colorimetric study of coffee and tea staining of four composite resins10.1111/j.1365-2842.1977.tb00997.x ↗
18. Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic10.1016/j.jdent.2004.07.001 ↗
19. Effect of Fe2O3 doping on sintering of yttria-stabilized zirconia10.1016/j.jeurceramsoc.2012.07.035 ↗
20. Phase transformation of a zirconia ceramic head after total hip arthroplasty10.1302/0301-620X.83B7.0830996 ↗
21. Effect of shading the zirconia framework on biaxial strength and surface microhardness10.1080/00016350802247123 ↗
22. ISO6872. Dentistry – Ceramic Materials. Geneva, Switzerland, 2008.
23. Fracture strength of monolithic all-ceramic crowns made of high translucent yttrium oxide-stabilized zirconium dioxide compared to porcelain-veneered crowns and lithium disilicate crowns10.3109/00016357.2013.822098 ↗
24. Fracture statics of multiple flaw distribution
25. Production and characterization of self-colored dental zirconia blocks10.1016/j.ceramint.2012.06.056 ↗
26. Crystallography of stress-induced martensitic transformations in partially-stabilized zirconia10.1111/j.1151-2916.1986.tb07421.x ↗
27. Lattice parameters, tetragonality (c/a) and transformability of tetragonal zirconia phase in plasma-sprayed ZrO2–Er2O3 coatings10.1016/S0167-577X(96)00245-5 ↗
28. The effect of low temperature aging on the mechanical property & phase stability of Y-TZP ceramics10.4047/jap.2009.1.3.113 ↗
29. Effects of coloring agents applied during sintering on bending strength and hardness of zirconia ceramics10.4012/dmj.2013-110 ↗
30. Effect of dopants on zirconia stabilization – an X-ray-absorption study 1. Trivalent dopants10.1111/j.1151-2916.1994.tb06964.x ↗
31. Low temperature degradation – aging – of zirconia: a critical review of the relevant aspects in dentistry10.1016/j.dental.2010.04.006 ↗
32. Current status of zirconia restoration10.1016/j.jpor.2013.09.001 ↗
33. Mechanical properties and low-temperature aging of tetragonal zirconia polycrystals processed by hot isostatic pressing10.1557/JMR.2003.0337 ↗
34. Zirconia as a dental implant abutment material: a systematic review
35. Influence of grain size and veneer firing process on flexural strength of zirconia ceramics10.1111/j.1600-0722.2012.00958.x ↗
36. Fracture resistance of monolithic zirconia molar crowns with reduced thickness10.3109/00016357.2015.1007479 ↗
37. Colorimetry
38. Zirconia as a ceramic biomaterial10.1016/S0142-9612(98)00010-6 ↗
39. The biaxial flexural strength and fatigue property of Lava Y-TZP dental ceramic10.1016/j.dental.2006.09.003 ↗
40. The effect of zirconia surface treatment on flexural strength and shear bond strength to a resin cement10.1016/S0022-3913(10)60033-9 ↗
41. Richerson · 2006 · 581
42. Effect of coloring with various metal oxides on the microstructure, color, and flexural strength of 3Y-TZP10.1002/jbm.b.31107 ↗
43. Effect of in vitro aging on the flexural strength and probability to fracture of Y-TZP zirconia ceramics for all-ceramic restorations10.1016/j.dental.2014.05.033 ↗
44. Enamel wear caused by monolithic zirconia crowns after 6 months of clinical use10.1111/joor.12139 ↗
45. Strength limitations of transformation-toughened zirconia alloys10.1111/j.1151-2916.1986.tb04785.x ↗
46. Thermal and mechanical properties of Y2O3-stabilized tetragonal zirconia polycrystals
47. Strengthening of oxide ceramics by transformation-induced stresses10.1111/j.1151-2916.1987.tb04952.x ↗
48. Effect of dopant species on tetragonal (t׳)-to-monoclinic phase-transformation of arc-melted ZrO2–RO1.5 (R=Sm, Y, Er, and Sc) in water at 200°C and 100MPa pressure10.1111/j.1151-2916.1995.tb08643.x ↗