journal article·2017-11

Fatigue strength of yttria-stabilized zirconia polycrystals: Effects of grinding, polishing, glazing, and heat treatment

Camila Pauleski Zucuni, Luís Felipe Guilardi, Marilia Pivetta Rippe, Gabriel Kalil Rocha Pereira, Luiz Felipe Valandro

Publisher page

Abstract

This study aimed to evaluate and compare the effect of different surface post-processing treatments (polishing, heat treatment, glazing, polishing + heat treatment and polishing + glazing) on the superficial characteristics (micromorphology and roughness), phase transformation and fatigue strength of a Y-TZP ceramic ground with diamond bur. Discs of Y-TZP ceramic were manufactured (ISO:6872-2015; final dimensions of 15mm in diameter and 1.2 ± 0.2mm in thickness) and randomly allocated according to the surface condition: Ctrl - as-sintered; Gr - ground with coarse diamond bur; Gr+HT - ground and subjected to the heat treatment; Gr+Pol - ground and polished; Gr+Pol+HT - ground, polished and heat treated; Gr+Gl - ground and glazed; Gr+Pol+Gl - ground, polished and glazed. The following analyses were performed: roughness (n = 25), surface topography (n = 2), phase transformation (n = 2) and fatigue strength by staircase method (n = 20). All treatments influenced to some extent the surface characteristics of Y-TZP, being that polishing reduced the surface roughness, the m-phase content and improved the fatigue strength; glazing led to the lowest roughness values (Ra and Rz), although it showed the worst fatigue strength; heat treatment showed limited effect on surface roughness, led to complete reversion of the existing m-phase content to t-phase, without enhancing fatigue performance. Thus, a polishing protocol after clinic adjustment (grinding) of monolithic restorations based on polycrystalline zirconia material is mandatory for surface characteristics and fatigue performance improvements.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Dental Research and COVID-19

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Anusavice · 2003
2. Low-temperature degradation of a Y-TZP ceramic after surface treatments10.1002/jbm.b.32957 ↗
3. Extended glaze firing on ceramics for hard machining: crack healing, residual stresses, optical and microstructural aspects10.1016/j.dental.2016.12.002 ↗
4. Flexural strength and failure modes of layered ceramic structures10.1016/j.dental.2011.09.008 ↗
5. The effect of sandblasting, Er:YAG laser, and heat treatment on the mechanical properties of different zirconia cores10.1089/pho.2015.3980 ↗
6. The tetragonal-monoclinic transformation in zirconia: lessons learned and future trends10.1111/j.1551-2916.2009.03278.x ↗
7. Collins · 1992
8. Emerging ceramic-based materials for dentistry10.1177/0022034514553627 ↗
9. Influence of surface finish and residual stresses on the ageing sensitivity of biomedical grade zirconia10.1016/j.biomaterials.2005.11.021 ↗
10. Effects of non-planarity on the mixed mode fracture resistance of biomaterial interfaces10.1016/0001-6160(89)90017-5 ↗
11. Loading frequencies up to 20Hz as an alternative to accelerate fatigue strength tests in a Y-TZP ceramic10.1016/j.jmbbm.2016.01.008 ↗
12. Phase analysis in zirconia systems10.1111/j.1151-2916.1972.tb11290.x ↗
13. The effects of finishing and polishing techniques on surface roughness and color stability of nanocomposites10.1016/j.jdent.2012.07.005 ↗
14. A technique for introducing surface compression into zirconia ceramics10.1111/j.1151-2916.1983.tb10543.x ↗
15. Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic10.1016/j.jdent.2004.07.001 ↗
16. Surface micro-morphology, phase transformation, and mechanical reliability of ground and aged monolithic zirconia ceramic10.1016/j.jmbbm.2016.10.008 ↗
17. Strengthening by surface damage in metastable tetragonal zirconia10.1111/j.1151-2916.1980.tb10671.x ↗
18. Transformation toughening in zirconia-containing ceramics10.1111/j.1151-2916.2000.tb01221.x ↗
19. Evaluation of efficiency of manual polishing over autoglazed and overglazed porcelain and its effect on plaque accumulation10.4047/jap.2012.4.4.179 ↗
20. Comparison of different grinding procedures on the flexural strength of Zirconia10.1016/S0022-3913(12)60081-X ↗
21. ISO 4287. Geometrical product specifications (GPS) – surface texture: profile method, terms definitions and surface texture parameters. International Organ Stand, 1997.
22. ISO 6872. Dentistry—Ceramic Materials. International Organ Stand, 2015.
23. ISO 13356. Implants for Surgery – Ceramic Materials Based on Yttria-stabilizes Tetragonal Zirconia (Y-TZP). International Organ Stand, 2008.
24. Surface phase transformation during grinding of Y-TZP10.1111/j.1551-2916.2007.01739.x ↗
25. The effect of low temperature aging on the mechanical property & phase stability of Y-TZP ceramics10.4047/jap.2009.1.3.113 ↗
26. Concerns of hydrothermal degradation in CAD/CAM zirconia10.1177/0022034509354193 ↗
27. Phase change and mechanical properties of ZrO2–Y2O3 solid electrolyte after ageing10.1016/0167-2738(81)90138-7 ↗
28. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic10.1016/S0109-5641(99)00070-6 ↗
29. Y-TZP ceramic processing from coprecipitated powders: a comparative study with three commercial dental ceramics10.1016/j.dental.2008.04.002 ↗
30. Effect of grain size on the monoclinic transformation, hardness, roughness, and modulus of aged partially stabilized zirconia10.1016/j.dental.2015.09.014 ↗
31. Complete and partial contour zirconia designs for crowns and fixed dental prostheses: a clinical report10.1016/S0022-3913(11)60112-1 ↗
32. A review of dental CAD/CAM: current status and future perspectives from 20 years of experience10.4012/dmj.28.44 ↗
33. Fracture resistance of monolithic zirconia molar crowns with reduced thickness10.3109/00016357.2015.1007479 ↗
34. In vitro evaluation of low-temperature aging effects and finishing procedures on the flexural strength and structural stability of Y-TZP dental ceramics10.1016/j.prosdent.2006.08.004 ↗
35. Effect of grinding with diamond-disc and-bur on the mechanical behavior of a Y-TZP ceramic10.1016/j.jmbbm.2014.05.010 ↗
36. The effect of grinding on the mechanical behavior of Y-TZP ceramics: a systematic review and meta-analyses10.1016/j.jmbbm.2016.06.028 ↗
37. Mechanical behavior of a Y-TZP ceramic for monolithic restorations: effect of grinding and low-temperature aging10.1016/j.msec.2016.02.049 ↗
38. Fatigue limit of polycrystalline zirconium oxide ceramics: effect of grinding and low-temperature aging10.1016/j.jmbbm.2016.01.006 ↗
39. Low-temperature degradation of Y-TZP ceramics: a systematic review and meta-analysis10.1016/j.jmbbm.2015.10.017 ↗
40. Zirconia as a ceramic biomaterial, a review10.1016/S0142-9612(98)00010-6 ↗
41. Mechanical behavior of yttria-stabilized tetragonal zirconia polycristalline ceramic after different zirconia surface treatments10.1016/j.msec.2017.03.299 ↗
42. Wear performance of dental ceramics after grinding and polishing treatments10.1016/j.jmbbm.2012.03.002 ↗
43. Wear performance of monolithic dental ceramics with different surface treatments
44. Surface properties of monolithic zirconia after dental adjustment treatments and in vitro wear simulation10.1016/j.jdent.2014.08.011 ↗
45. Effect of grinding and heat treatment on the mechanical behavior of zirconia ceramic
46. Clinical evaluation and patient satisfaction of single zirconia-based and high-noble alloy porcelain-fused-to-metal crowns in the esthetic area: a retrospective cohort study10.1111/jopr.12344 ↗
47. Calibration curve for quantitative analysis of the monoclinic tetragonal ZrO2 system by X-rays diffraction10.1111/j.1151-2916.1984.tb19715.x ↗
48. Effects of two grading techniques of zirconia material on the fatigue limit of full-contour 3-unit fixed dental prostheses10.1016/j.dental.2016.12.010 ↗
49. Crack suppression in strongly bonded homogeneous/heterogeneous laminates: a study on glass/glass-ceramic bilayers10.1111/j.1151-2916.1996.tb07922.x ↗
50. Making yttria-stabilized tetragonal zirconia translucent10.1016/j.dental.2014.08.375 ↗