journal article·2016-09

Fretting-corrosion behavior in hip implant modular junctions: The influence of friction energy and pH variation

Dmitry Royhman, Megha Patel, Maria J. Runa, Markus A. Wimmer, Joshua J. Jacobs, Nadim J. Hallab, Mathew T. Mathew

Publisher page

Abstract

Background Recently, there has been increasing concern in the orthopedic community over the use of hip implant modular devices due to an increasing number of reports of early failure, failure that has been attributed to fretting-corrosion at modular interfaces. Much is still unknown about the electrochemical and mechanical degradation mechanisms associated with the use of such devices. Purpose Accordingly, the purpose of our study was to develop a methodology for testing the fretting-corrosion behavior of modular junctions. Methods A fretting-corrosion apparatus was used to simulate the fretting-corrosion conditions of a CoCrMo hip implant head on a Ti6Al4V hip implant stem. The device features two perpendicularly-loaded CoCrMo pins that articulated against a Ti6Al4V rod. A sinusoidal fretting motion was applied to the rod at various displacement amplitudes (25, 50, 100, 150 and 200μm) at a constant load of 200N. Bovine calf serum at two different pH levels (3.0 and 7.6) was used to simulate the fluid environment around the joint. Experiments were conducted in two modes of electrochemical control - free-potential and potentiostatic. Electrochemical impedance spectroscopy tests were done before and after the fretting motion to assess changes in corrosion kinetics. Results In free potential mode, differences were seen in change in potential as a function of displacement amplitude. In general, VDrop (the drop in potential at the onset of fretting), VFretting, (the average potential during fretting), ΔVFretting (the change in potential from the onset of fretting to its termination) and VRecovery (the change in potential from the termination of fretting until stabilization) appeared linear at both pH levels, but showed drastic deviation from linearity at 100μm displacement amplitude. Subsequent EDS analysis revealed a large number of Ti deposits on the CoCrMo pin surfaces. Potentiostatic tests at both pH levels generally showed increasing current with increasing displacement amplitude. Electrochemical impedance spectroscopy measurements from free potential and potentiostatic tests indicated increased levels of resistance of the system after induction of the fretting motion. In free potential tests, the largest increase in impedance was found for the 100μm group. Conclusions We conclude that the 100µm group exhibits deviations from linearity for several parameters, and this was most likely due to adhesive wear between Ti6Al4V and CoCrMo surfaces. Overall, the degradation of the system was dominated by wear at all pH levels, and displacement amplitudes.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Orthopaedic implants and arthroplasty · Titanium Alloys Microstructure and Properties · Bone Tissue Engineering Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (48)

Show source-provided references
1. A tribo-electrochemical apparatus for in vitro investigation of fretting–corrosion of metallic implant materials10.1016/S0043-1648(02)00027-3 ↗
2. Influence of fretting regimes on the tribocorrosion behaviour of Ti6Al4V in 0.9wt% sodium chloride solution10.1016/j.wear.2003.11.003 ↗
3. Characterization of modified Ti6Al4V alloy after fretting-corrosion tests using near-field microscopy10.1016/j.surfcoat.2012.09.034 ↗
4. Fretting corrosion accelerates crevice corrosion of modular hip tapers10.1002/jab.770060104 ↗
5. In vitro studies of fretting corrosion of orthopaedic materials10.1002/jor.1100060415 ↗
6. In vivo and in vitro considerations of corrosion testing
7. Design, development, and testing of a compact tribocorrosion apparatus for biomedical applications
8. Tribocorrosion of passive metals in the mixed lubrication regime: theoretical model and application to metal-on-metal artificial hip joints10.1016/j.wear.2014.12.003 ↗
9. Tribo-corrosion of materials: interplay between chemical, electrochemical, and mechanical reactivity of surfaces10.1016/j.wear.2006.03.027 ↗
10. Evaluation of the fretting corrosion behavior of the proximal pad taper of a modular hip design10.1016/S0043-1648(99)00110-6 ↗
11. Wear and corrosion of modular interfaces in total hip replacements10.1097/00003086-199401000-00013 ↗
12. Pseudotumour formation due to tribocorrosion at the taper interface of large diameter metal on polymer modular total hip replacements10.1016/j.arth.2013.02.009 ↗
13. Adverse local tissue reaction arising from corrosion at the femoral neck-body junction in a dual-taper stem with a cobalt-chromium modular neck10.2106/JBJS.L.01042 ↗
14. Dufils, J., Laurent, M., Kunze, J., Royhman, D., Mathew, M., Fridrici, V., et al., 2015. A Servo-electric Apparatus with Potentiostat to Study the Fretting Corrosion of Cobalt- Chromium – Titanium Alloy Couples. In: Greenwald, A.S., Kurtz, S.M., Lemons, J.E., Mihalko, W.H. (eds.), Modularity and Tapers in Total Joint Replacement Devices. West Conshohocken, PA: ASTM International, pp. 303–320. (ATSM STP1591).10.1520/STP159120140143 ↗
15. Analysis of sliding behaviour for fretting loadings: determination of transition criteria10.1016/0043-1648(94)06582-9 ↗
16. Application of an energy wear approach to quantify fretting contact durability: Introduction of a wear energy capacity concept10.1016/j.triboint.2007.02.011 ↗
17. Friction–corrosion of AISI 316L/bone cement and AISI 316L/PMMA contacts: Ionic strength effect on tribological behaviour10.1016/j.wear.2008.12.087 ↗
18. Fretting-corrosion of materials used as orthopaedic implants10.1016/j.wear.2004.11.027 ↗
19. In vivo corrosion of modular hip prosthesis components in mixed and similar metal combinations. The effect of crevice, stress, motion, and alloy coupling10.1002/jbm.820271210 ↗
20. Fretting crevice corrosion of stainless steel stem–CoCr femoral head connections: comparisons of materials, initial moisture, and offset length10.1002/jbm.b.31164 ↗
21. The electrochemical and mechanical behavior of passivated and TiN/AlN-coated CoCrMo and Ti6Al4V alloys10.1016/S0142-9612(03)00606-9 ↗
22. Crevice corrosion of titanium in aqueous salt solutions10.5006/0010-9312-24.4.96 ↗
23. In vitro reactivity to implant metals demonstrates a person-dependent association with both T-cell and B-cell activation
24. Metal sensitivity in patients with orthopaedic implants10.2106/00004623-200103000-00017 ↗
25. Passive and transpassive behaviour of CoCrMo in simulated biological solutions10.1016/j.electacta.2003.12.043 ↗
26. Presence of corrosion products and hypersensitivity-associated reactions in periprosthetic tissue after aseptic loosening of total hip replacements with metal bearing surfaces10.1016/j.actbio.2008.07.032 ↗
27. Investigation of wear and corrosion of a high-carbon stellite alloy for hip implants10.1007/s11665-014-0887-x ↗
28. Corrosion at the head-neck taper as a cause for adverse local tissue reactions after total hip arthroplasty10.2106/JBJS.K.01352 ↗
29. Corrosion of a hip stem with a modular neck taper junction: a retrieval study of 16 cases10.1016/j.arth.2008.09.009 ↗
30. Impact of the economic downturn on total joint replacement demand in the United States10.2106/JBJS.M.00285 ↗
31. Electrochemical methods in tribocorrosion: a critical appraisal10.1016/S0013-4686(01)00679-X ↗
32. Electrochemical impedance spectroscopy characterization of passive film formed on implant Ti–6Al–7Nb alloy in Hank׳s solution
33. Crevice corrosion in orthopedic implant metals10.1002/jbm.820110410 ↗
34. Wear-rate transitions and their relationship to wear mechanisms10.1016/0001-6160(87)90016-2 ↗
35. Wear-corrosion synergism in a CoCrMo hip bearing alloy is influenced by proteins10.1007/s11999-012-2563-5 ↗
36. Mathew, M.T., Patel, M., Royhman, D., Runa, M.J., Jacobs, J.J., Wimmer, M., et al., 2015. Tribocorrosion in Hip Modular Taper Junctions: Load-Triggered Transitions in Electrochemical and Mechanical Behavior. In: Greenwald, A.S., Kurtz, S.M., Lemons, J.E., Mihalko, W.H. (eds.), Modularity and Tapers in Total Joint Replacement Devices. West Conshohocken, PA: ASTM International, pp. 283–302. (ATSM STP1591).10.1520/STP159120140147 ↗
37. Triboelectrochemical techniques and interpretation methods in tribocorrosion: a comparative evaluation10.1016/j.triboint.2007.11.003 ↗
38. Low amplitude oscillating sliding wear on chemically vapour deposited diamond coatings10.1016/0925-9635(93)90243-U ↗
39. Fretting of CoCrMo and Ti6Al4V alloys in modular prostheses10.1179/1751584X15Y.0000000014 ↗
40. Pourbaix, M., 1974. Atlas of electrochemical equilibria in aqueous solutions. NACE, 644 [Internet] [cited 12.03.13]; Available from: 〈http://www.csa.com/partners/viewrecord.php?requester=gs&collection=TRD&recid=943388CO〉
41. In vivo severe corrosion and hydrogen embrittlement of retrieved modular body titanium alloy hip-implants10.1002/jbm.b.31171 ↗
42. Fretting-corrosion in hip implant modular junctions: new experimental set-up and initial outcome10.1016/j.triboint.2015.04.032 ↗
43. An electrochemical investigation of TMJ implant metal alloys in an artificial joint fluid environment: the influence of pH variation10.1016/j.jcms.2014.01.029 ↗
44. Tribocorrosive behaviour of commonly used temporomandibular implants in a synovial fluid-like environment: Ti–6Al–4V and CoCrMo10.1088/0022-3727/46/40/404002 ↗
45. Mapping erosion-corrosion of carbon steel in oil exploration conditions: Some new approaches to characterizing mechanisms and synergies10.1016/j.triboint.2010.01.005 ↗
46. Fretting corrosion of CoCrMo and Ti6Al4V interfaces10.1016/j.biomaterials.2012.04.015 ↗
47. Adverse local tissue reactions in metal-on-polyethylene total hip arthroplasty due to trunnion corrosion the risk of misdiagnosis10.1302/0301-620X.97B8.34682 ↗
48. The effect of contact load on CoCrMo wear and the formation and retention of tribofilms10.1016/j.wear.2015.02.013 ↗