journal article·2018-02

Effect of adding support structures for overhanging part on fatigue strength in selective laser melting

Yuka Kajima, Atsushi Takaichi, Takayuki Nakamoto, Takahiro Kimura, Nuttaphon Kittikundecha, Yusuke Tsutsumi, Naoyuki Nomura, Akira Kawasaki, Hidekazu Takahashi, Takao Hanawa, Noriyuki Wakabayashi

Publisher page

Abstract

Selective laser melting (SLM) technology was recently introduced to fabricate dental prostheses. However, the fatigue strength of clasps in removable partial dentures prepared by SLM still requires improvement. In this study, we attempted to improve the fatigue strength of clasps by adding support structures for overhanging parts, which can generally be manufactured at an angle to be self-supporting. The results show that the fatigue strength of the supported specimens was more than twice that of unsupported specimens. Electron back-scattered diffraction analysis revealed that the supported specimens exhibited lower kernel average misorientation values than the unsupported specimens, which suggested that the support structure reduced the residual strain during the SLM process and helped to prevent micro-cracks led by thermal distortion. In addition, the supported specimens cooled more rapidly, thereby forming a finer grain size compared to that of the unsupported specimens, which contributed to improving the fatigue strength. The results of this study suggest that the fatigue strength of overhanging parts can be improved by intentionally adding support structures.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Dental materials and restorations · Additive Manufacturing and 3D Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. Improving the fatigue behaviour of a selectively laser melted aluminium alloy: influence of heat treatment and surface quality10.1016/j.matdes.2016.05.041 ↗
2. On the microstructural and mechanical properties of post-treated additively manufactured Inconel 718 superalloy under quasi-static and cyclic loading10.1016/j.msea.2016.05.089 ↗
3. Clinical performance of cast clasp-retained removable partial dentures: a retrospective study
4. Design optimization of supports for overhanging structures in aluminum and titanium alloys by selective laser melting10.1016/j.matdes.2014.07.043 ↗
5. 2008
6. Direct retainers
7. Fatigue performance evaluation of selective laser melted Ti–6Al–4V10.1016/j.msea.2014.01.041 ↗
8. Finite element simulation of selective laser melting process considering optical penetration depth of laser in powder bed10.1016/j.matdes.2015.10.002 ↗
9. Practical support structures for selective laser melting10.1016/j.jmatprotec.2016.08.006 ↗
10. Analysis of defect generation in Ti–6Al–4V parts made using powder bed fusion additive manufacturing processes
11. Henry · 2009
12. Implementation of a thermomechanical model for the simulation of selective laser melting10.1007/s00466-014-1024-2 ↗
13. Advanced lattice support structures for metal additive manufacturing10.1016/j.jmatprotec.2013.01.020 ↗
14. Finite element simulation of the temperature and stress fields in single layers built without-support in selective laser melting10.1016/j.matdes.2013.05.070 ↗
15. An RE/RM approach to the design and manufacture of removable partial dentures with a biocompatibility analysis of the F75 Co–Cr SLM alloy
16. The influence of cooling conditions on grain size, secondary phase precipitates and mechanical properties of biomedical alloy specimens produced by investment casting10.1016/j.jmbbm.2013.04.013 ↗
17. Fatigue strength of Co–Cr–Mo alloy clasps prepared by selective laser melting10.1016/j.jmbbm.2016.02.032 ↗
18. Characterization of microstructural damage due to low-cycle fatigue by EBSD observation10.1016/j.matchar.2009.07.003 ↗
19. Fatigue damage evaluation using electron backscatter diffraction10.2320/matertrans.M2011014 ↗
20. Improvement of fatigue resistance and ductility of TiAl6V4 processed by selective laser melting10.1016/j.jmatprotec.2015.01.025 ↗
21. Selective laser melting technique of Co–Cr dental alloys: a review of structure and properties and comparative analysis with other available techniques10.1111/jopr.12268 ↗
22. Densification behavior of gas and water atomized 316L stainless steel powder during selective laser melting10.1016/j.apsusc.2010.02.030 ↗
23. A study on the residual stress during selective laser melting (SLM) of metallic powder10.1007/s00170-016-8466-y ↗
24. Deflection fatigue of Ti–6Al–7Nb, Co–Cr, and gold alloy cast clasps10.1016/j.prosdent.2004.11.011 ↗
25. Mechanical behavior of additive manufactured, powder-bed laser-fused materials10.1016/j.msea.2015.10.068 ↗
26. Clasp fabrication using one-process molding by repeated laser sintering and high-speed milling10.1016/j.jpor.2016.10.002 ↗
27. CAD/CAM-fabricated implant-supported restorations: a systematic review10.1111/clr.12633 ↗
28. Phoenix · 2008
29. On the fatigue crack growth behavior in 316L stainless steel manufactured by selective laser melting10.1016/j.engfracmech.2014.03.008 ↗
30. A comparison of the tensile, fatigue, and fracture behavior of Ti–6Al–4V and 15-5 PH stainless steel parts made by selective laser melting10.1007/s00170-013-5106-7 ↗
31. Complications and failures in removable partial dentures: a clinical evaluation10.1046/j.1365-2842.2002.00898.x ↗
32. A comparison of EBSD based strain indicators for the study of Fe–3Si steel subjected to cyclic loading10.1016/j.matchar.2016.03.020 ↗
33. A new approach to the design and optimisation of support structures in additive manufacturing10.1007/s00170-012-4403-x ↗
34. Surface roughness analysis, modelling and prediction in selective laser melting10.1016/j.jmatprotec.2012.11.011 ↗
35. Microstructures and mechanical properties of Co–29Cr–6Mo alloy fabricated by selective laser melting process for dental applications10.1016/j.jmbbm.2013.01.021 ↗
36. Functional encapsulation of laser melted Inconel 718 by Arc-PVD and HVOF for post compacting by hot isostatic pressing10.1179/0032589915Z.000000000250 ↗
37. Thomas, D., Bibb, R., 2008. Identifying the geometric constraints and process specific challenges of selective laser melting, In: Proceedings of Time Compression Technologies Rapid Manufacturing Conference 2008, Rapid News Publications Plc., Coventry, West Midlands, UK.
38. Analysis of fracture toughness and crack propagation of Ti6Al4V produced by selective laser melting10.1002/adem.201100233 ↗
39. Designing for additive manufacturing10.1016/j.procir.2012.07.108 ↗
40. Research on the fabricating quality optimization of the overhanging surface in SLM process10.1007/s00170-012-4271-4 ↗
41. Use of CAD/CAM technology to fabricate a removable partial denture framework10.1016/j.prosdent.2006.05.029 ↗
42. Effects of process time interval and heat treatment on the mechanical and microstructural properties of direct laser deposited 316L stainless steel10.1016/j.msea.2015.07.056 ↗
43. Mechanical properties and microstructure of removable partial denture clasps manufactured using selective laser melting
44. Usage and status of cobalt–chromium removable partial dentures 5–6 years after placement10.1046/j.1365-2842.2002.00846.x ↗
45. Thermal behavior and microstructure evolution during laser deposition with laser-engineered net shaping: Part II. Experimental investigation and discussion10.1007/s11661-008-9566-6 ↗
46. Study on fatigue threshold behavior and fatigue crack-propagation in a cast Co–Cr–Mo Alloy used for surgical implants10.1111/j.1460-2695.1989.tb00537.x ↗