Abstract

Aim To investigate the two-body wear performance of dental ceramics after different clinical surface treatments as a function of number of wear cycles. Material and methods Standardized specimens (n=72/material) were prepared from two different zirconia ceramics, a veneering porcelain, and a lithiumdisilicate glass ceramic. Specimens were progressively glazed, ground, and polished. After each treatment step 24 specimens per material were kept at the obtained surface state. Steatite and human enamel specimens served as reference materials. Two-body wear tests were performed with steatite spheres as antagonists in a pin-on-block design (50N, 1.6 Hz, lateral movement: 1mm, mouth opening: 2mm) under simultaneous thermal cycling (5/55 °C, 2 min/cycle). For investigating the dynamic evolution of the wear process, 9 groups per material (n=8/group) were defined, differing in surface state (glazed, ground, and polished) and number of chewing cycles (40T, 80T, and 120T; T: ×1000): glazed 40T, glazed 80T, glazed 120T, ground 40T, ground 80T, ground 120T, polished 40T, polished 80T, polished 120T. Surface roughness, wear depth of the specimens and relative wear area of the steatite antagonists were determined using an optical 3D laser scanning microscope. SEM evaluation was done. Mean values and standard deviations were calculated and statistically analyzed (one-way ANOVA, post-hoc Bonferroni, α=0.05). Results Veneering and lithiumdisilicate ceramics showed higher wear depths than zirconia ceramics (p<0.05). Wear of veneering and lithiumdisilicate ceramics and their antagonists increased with wear cycles but was only marginally influenced by the initial surface state. Wear of zirconia was not influenced by wear cycles but antagonists of zirconia showed a cycle-dependent wear increase. Polished zirconia surfaces showed lowest wear for material and antagonist. Wear mechanism of common ceramics was characterized by abrasive wear. Zirconia in contrast showed a superficial cyclic shifting of worn material of the antagonist. Conclusions Wear of zirconia and standard ceramics showed different wear performances, strongly influenced by surface treatments as well as number of wear cycles.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Erosion and Treatment · Bone Tissue Engineering Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Two-body wear of different ceramic materials opposed to zirconia ceramic10.1016/S0022-3913(10)60102-3 ↗
2. Three-body wear potential of dental yttrium-stabilized zirconia ceramic after grinding, polishing, and glazing treatments10.1016/j.prosdent.2013.12.021 ↗
3. Intra-oral restorative materials wear: rethinking the current approaches: how to measure wear10.1016/j.dental.2006.02.003 ↗
4. Two-body wear of resin and ceramic denture teeth in comparison to human enamel10.1016/j.dental.2007.04.012 ↗
5. Investigation of the time-dependent wear behavior of veneering ceramic in porcelain fused to metal crowns during chewing simulations10.1016/j.jmbbm.2014.08.006 ↗
6. Two-body wear of artificial acrylic and composite resin teeth in relation to antagonist material10.1016/S0022-3913(09)60051-2 ↗
7. Two-body wear of dental restorative materials10.1016/j.jmbbm.2010.06.001 ↗
8. How to qualify and validate wear simulation devices and methods10.1016/j.dental.2006.02.002 ↗
9. The wear of polished and glazed zirconia against enamel10.1016/S0022-3913(13)60005-0 ↗
10. Lifetime-limiting strength degradation from contact fatigue in dental ceramics10.1177/00220345000790020501 ↗
11. A study on the in-vitro wear of the natural tooth structure by opposing zirconia or dental porcelain10.4047/jap.2010.2.3.111 ↗
12. Wear evaluation of the human enamel opposing different Y-TZP dental ceramics and other porcelains10.1016/j.jdent.2012.08.004 ↗
13. Influence of surface treatment on the wear of solid zirconia10.3109/00016357.2012.696690 ↗
14. The influence of antagonist standardization on wear10.1177/00220345990780021201 ↗
15. Wear of ceramic inlays, their enamel antagonists, and luting cements10.1016/0022-3913(93)90192-Q ↗
16. Quantitative in vivo wear of human enamel10.1177/00220345890680120601 ↗
17. Wear of enamel opposing zirconia and lithium disilicate after adjustment, polishing and glazing10.1016/j.jdent.2014.09.008 ↗
18. Wear: mechanisms, manifestations and measurement. Report of a workshop10.1016/0300-5712(95)00043-7 ↗
19. Complete and partial contour zirconia designs for crowns and fixed dental prostheses: a clinical report10.1016/S0022-3913(11)60112-1 ↗
20. In vitro investigation of the wear of human enamel by dental porcelain10.1016/S0022-3913(99)70280-5 ↗
21. Wear behavior of dental Y-TZP ceramic against natural enamel after different finishing procedures10.1016/j.dental.2012.04.010 ↗
22. Wear characteristics of current esthetic dental restorative CAD/CAM materials: two-body wear, gloss retention, roughness and Martens hardness10.1016/j.jmbbm.2013.01.003 ↗
23. Antagonist wear of three CAD/CAM anatomic contour zirconia ceramics10.1016/j.prosdent.2013.06.002 ↗
24. In vitro wear behavior of zirconia opposing enamel: a systematic review10.1111/jopr.12167 ↗
25. Wear performance of dental ceramics after grinding and polishing treatments10.1016/j.jmbbm.2012.03.002 ↗
26. Wear performance of substructure ceramics and veneering porcelains10.1016/j.dental.2011.04.001 ↗
27. Wear performance of dental materials: a comparison of substructure ceramics, veneering ceramics, and non-precious alloys10.1002/adem.201180015 ↗
28. Surface properties of monolithic zirconia after dental adjustment treatments and in vitro wear simulation10.1016/j.jdent.2014.08.011 ↗
29. Wear performance of monolithic dental ceramics with different surface treatments
30. Influence of stress simulation parameters on the fracture strength of all-ceramic fixed-partial dentures10.1016/j.dental.2005.04.024 ↗
31. Two-body wear of dental porcelain and substructure oxide ceramics10.1007/s00784-011-0589-9 ↗
32. Potential countersample materials for in vitro simulation wear testing10.1016/S0109-5641(01)00043-4 ↗
33. Two-body wear of monolithic, veneered and glazed zirconia and their corresponding enamel antagonists10.3109/00016357.2011.654248 ↗
34. Enamel wear caused by monolithic zirconia crowns after 6 months of clinical use10.1111/joor.12139 ↗