Enhancement of stress corrosion cracking of AZ31 magnesium alloy in simulated body fluid thanks to cryogenic machining
Source abstract
Abstract
Magnesium and its alloys have recently attracted great attention as potential materials for the manufacture of biodegradable implants. Unfortunately, their inadequate resistance to the simultaneous action of corrosion and mechanical stresses in the human body have hampered their use as implant materials. This work aims at evaluating the Stress Corrosion Cracking (SCC) susceptibility of the AZ31 Mg alloy after being machined under cryogenic cooling. The SCC behaviour was evaluated by means of Slow Strain Rate Tests (SSRTs) in Simulated Body Fluid (SBF) at 37 °C. Prior to testing, a full characterization of the machined surface integrity, including microstructural observations, residual stress, nano-hardness measurements and surface texture analysis was carried out together with the assessment of the corrosion properties through potentiodynamic polarization curves. In addition, the morphology of the fracture surfaces after SSRTs was analysed by means of 3D optical profiler and Scanning Electron Microscopy (SEM). The improved corrosion resistance due to the increased extension of the nano-surface layer and to the compressive residual stresses represents the reason of the reduced SCC susceptibility of cryogenically machined AZ31 samples as compared to dry machined ones.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (65)
Show source-provided references
1. Effects of microstructure on the short fatigue crack initiation and propagation characteristics of biomedical α/β titanium alloys10.1007/s11661-000-0222-z ↗
2. Osseointegrated titanium implants: Requirements for Ensuring a long-lasting, direct bone-to-implant Anchorage in man10.3109/17453678108991776 ↗
3. Corrosion fatigue of biomedical metallic alloys: mechanisms and mitigation10.1016/j.actbio.2011.09.012 ↗
4. The pathology of total joint arthroplasty.II. Mechanisms of implant failure10.1007/s002560050552 ↗
5. Microbially-influenced corrosion: damage to prostheses, delight for bacteria10.1177/039139880602900415 ↗
6. The effect of cooling strategies and machining feed rate on the corrosion behavior and wettability of AZ31 alloy for biomedical applications10.1016/j.procir.2017.03.168 ↗
7. Large strain extrusion machining under cryogenic cooling to enhance corrosion resistance of magnesium alloys for biomedical applications10.1016/j.promfg.2018.07.030 ↗
8. Stress corrosion cracking of rare-earth containing magnesium alloys ZE41, QE22 and Elektron 21 (EV31A) compared with AZ8010.1016/j.msea.2007.07.070 ↗
9. Analysis of tool wear in cryogenic machining of additive manufactured Ti6Al4V alloy10.1016/j.wear.2015.01.030 ↗
10. Bradley · 2004
11. Residual stresses — measurement and causes in machining processes10.1016/S0007-8506(07)60172-3 ↗
12. Machining-induced surface transformations of magnesium alloys to enhance corrosion resistance in human-like environment10.1016/j.cirp.2018.04.040 ↗
13. Effectiveness of using low-temperature coolants in machining to enhance durability of AISI 316L stainless steel for reusable biomedical devices10.1016/j.jmapro.2019.02.003 ↗
14. Metallic implant biomaterials10.1016/j.mser.2014.10.001 ↗
15. Influence of a MAO + PLGA coating on biocorrosion and stress corrosion cracking behavior of a magnesium alloy in a physiological environment
16. Acta Biomaterialia Magnesium alloys as body implants : fracture mechanism under dynamic and static loadings in a physiological environment10.1016/j.actbio.2011.10.031 ↗
17. In-vitro characterization of stress corrosion cracking of aluminium-free magnesium alloys for temporary bio-implant applications10.1016/j.msec.2014.06.018 ↗
18. Biocompatible magnesium alloys as absorbable implant materials – adjusted surface and subsurface properties by machining processes10.1016/j.cirp.2007.05.029 ↗
19. Mechanical compatibility of noncemented hip prostheses with the human femur10.1016/S0883-5403(06)80102-6 ↗
20. The influence of stem size and extent of porous coating on femoral bone resorption after primary cementless hip arthroplasty10.1097/00003086-198806000-00002 ↗
21. Mechanical behaviour of cp-magnesium with duplex hydroxyapatite and PEO coatings10.1016/j.msec.2014.12.081 ↗
22. Calcium phosphate cements as bone drug delivery systems: a review10.1016/j.jconrel.2006.04.007 ↗
23. Surface integrity of dry machined titanium alloys10.1016/j.ijmachtools.2008.10.011 ↗
24. The relation between severe plastic deformation microstructure and corrosion behavior of AZ31 magnesium alloy10.1016/j.jallcom.2008.01.084 ↗
25. Hanawa · 2010 · 3
26. Hänzi · 2009
27. Corrosion of metal orthopaedic implants10.2106/00004623-199802000-00015 ↗
28. Metal degradation products: a cause for concern in metal-metal bearings?10.1097/01.blo.0000096810.78689.62 ↗
29. A review of stress-corrosion cracking and corrosion fatigue of magnesium alloys for biodegradable implant applications
30. Stress corrosion cracking and corrosion fatigue characterisation of MgZn1Ca0.3 (ZX10) in a simulated physiological environment10.1016/j.jmbbm.2016.09.033 ↗
31. Stress corrosion cracking of an extruded magnesium alloy (ZK21) in a simulated body fluid10.1016/j.engfracmech.2018.09.002 ↗
32. Cryogenic machining of biomedical implant materials for improved functional performance, life and sustainability10.1016/j.procir.2016.04.133 ↗
33. In vitro degradation and mechanical integrity of calcium-containing magnesium alloys in modified-simulated body fluid10.1016/j.biomaterials.2008.02.003 ↗
34. Correlation between pre-operative periprosthetic bone density and post-operative bone loss in THA can be explained by strain-adaptive remodelling10.1016/S0021-9290(99)00041-X ↗
35. How useful is SBF in predicting in vivo bone bioactivity?10.1016/j.biomaterials.2006.01.017 ↗
36. Novel magnesium alloys developed for biomedical application: a review10.1016/j.jmst.2013.02.005 ↗
37. Effects of compressive stress on localized corrosion in AA2024-T310.1016/j.corsci.2005.12.003 ↗
38. Effects of grain size on the corrosion resistance of pure magnesium by cooling rate-controlled solidification10.1007/s11706-015-0299-3 ↗
39. Hydroxyapatite coating containing multi-walled carbon nanotubes on AZ31 magnesium: mechanical-electrochemical degradation in a physiological environment10.1016/j.ceramint.2018.02.015 ↗
40. Microstructure, mechanical behavior and low temperature superplasticity of ECAP processed ZM21 Mg alloy10.1016/j.jallcom.2015.03.029 ↗
41. Mg and its alloys for biomedical applications: exploring corrosion and its interplay with mechanical failure10.3390/met7070252 ↗
42. Corrosion behavior of metallic materials in biomedical applications . I . Ti and its alloys
43. Corrosion behavior of metallic materials in biomedical applications . II . Stainless steels and Co-Cr alloys
44. Surface integrity in dry and cryogenic machining of AZ31B Mg alloy with varying cutting edge radius tools10.1016/j.proeng.2011.11.113 ↗
45. Cryogenic machining and burnishing of magnesium alloys to improve in vivo corrosion resistance
46. Role of chlorides on pitting and hydrogen embrittlement of Mg–Mn wrought alloy10.1016/j.corsci.2013.05.030 ↗
47. In vitro and in vivo studies of biodegradable fine grained AZ31 magnesium alloy produced by equal channel angular pressing10.1016/j.msec.2015.10.028 ↗
48. Toxicological evaluations of rare earths and their health impacts to workers: a literature review10.5491/SHAW.2013.4.1.12 ↗
49. Bone-healing pattern at the surface of titanium implants: an experimental study in the dog,10.1111/clr.12097 ↗
50. Retardation of crack initiation and growth in austenitic stainless steels by laser peening without protective coating10.1016/j.msea.2005.11.017 ↗
51. Numerical study of the behavior of magnesium alloy AM50 in tensile and torsional loadings10.1007/s00419-018-1492-5 ↗
52. Enhanced surface integrity from cryogenic machining of AZ31B Mg alloy: a physics-based analysis with microstructure prediction10.1115/1.4034279 ↗
53. Corrosion fatigue fracture of magnesium alloys in bioimplant applications: a review10.1016/j.engfracmech.2014.08.009 ↗
54. Magnesium and its alloys as orthopedic biomaterials: a review10.1016/j.biomaterials.2005.10.003 ↗
55. Environmentally-induced cracking of magnesium10.1016/0010-938X(84)90017-9 ↗
56. Determinants of stress shielding: design versus materials versus interface
57. Fatigue of biomaterials: a review10.1016/S0142-1123(00)00052-9 ↗
58. Comparison of the corrosion behaviour of AZ31B magnesium alloy under immersion test and potentiodynamic polarization test in NaCl solution10.1016/j.jma.2014.01.004 ↗
59. Maintenance of proximal cortical bone with use of a less stiff femoral component in hemiarthroplasty of the hip without cement. An investigation in a canine model at six months and two years10.2106/00004623-199709000-00013 ↗
60. The mechanism of bone remodeling and resorption around press-fitted THA stems10.1016/0021-9290(93)90001-U ↗
61. A critical review of the Stress Corrosion Cracking (SCC) of magnesium alloys10.1002/adem.200500071 ↗
62. Degradable biomaterials based on magnesium corrosion10.1016/j.cossms.2009.04.001 ↗
63. Wolff · 1986
64. Stress corrosion cracking behavior of fine-grained AZ61 magnesium alloys processed by equal-channel angular pressing10.3390/met7090343 ↗
65. Enhanced biodegradation behavior of ultrafine-grained ZE41A magnesium alloy in Hank's solution10.1016/j.pnsc.2013.06.003 ↗