Failure behavior of plasma-sprayed HAp coating on commercially pure titanium substrate in simulated body fluid (SBF) under bending load
Source abstract
Abstract
Four point bending tests with acoustic emission (AE) monitoring were conducted for evaluating failure behavior of the plasma-sprayed hydroxyapatite (HAp) top coat on commercially pure titanium (cp-Ti) plate with and without mixed HAp/Ti bond coat. Effect of immersion in simulated body fluid (SBF) on failure behavior of the coated specimen was also investigated by immersing the specimen in SBF. The AE patterns obtained from the bending test of the HAp coating specimens after a week immersion in SBF clearly showed the earlier stage of delamination and spallation of the coating layer compared to those without immersion in SBF. It was also found that the bond coating improved failure resistance of the HAp coating specimen compared to that without the bond coat. Four point bend fatigue tests under ambient and SBF environments were also conducted with AE monitoring during the entire fatigue test for investigating the influence of SBF environment on fatigue failure behavior of the HAp coating specimen with the mixed HAp/Ti bond coat. The specimens tested at a stress amplitude of 120 MPa under both ambient and SBF environments could survive up to 10⁷ cycles without spallation of HAp coating layer. The specimens tested under SBF environment and those tested under ambient environment after immersion in SBF showed shorter fatigue life compared to those tested under ambient environment without SBF immersion. Micro-cracks nucleated in the coating layer in the early stage of fatigue life and then propagated into the cp-Ti substrate in the intermediate stage, which unstably propagated to failure in the final stage. It was found from the XRD analysis that the dissolution of the co-existing phases and the precipitation of the HAp phase were taken place during immersion in SBF. During this process, the co-existing phases disappeared from the coating layer and the HAp phase fully occupied the coating layer. The degradation of bending strength and fatigue life of the HAp coating specimens tested under SBF environment would be induced by dissolution of the co-existing phases from the coating layer during immersion in SBF.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Bone Tissue Engineering Materials · Orthopaedic implants and arthroplasty · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Acoustic emission analysis of thermal sprayed hydroxyapatite coating examined under four point bend loading10.1179/sur.1998.14.4.309 ↗
2. Dissolution behavior of plasma-sprayed hydroxyapatite coatings
3. Effect of heat treatments on HVOF hydroxyapatite coatings10.1007/s11666-007-9034-7 ↗
4. Bioactive glass and glass-ceramic scaffolds for bone tissue engineering10.3390/ma3073867 ↗
5. In vitro studies of plasma-sprayed hydroxyapatite/Ti–6Al–4V composite coatings in simulated body fluid (SBF)10.1016/S0142-9612(02)00573-2 ↗
6. Activity of plasma sprayed yttria stabilized zirconia reinforced hydroxyapatite/Ti–6Al–4V composite coating in simulated body fluid10.1016/j.biomaterials.2003.09.101 ↗
7. Comparison of bone-implant interface shear strength of solid hydroxyapatite and hydroxyapatite-coated titanium implants10.1002/jbm.820270502 ↗
8. Thermal spraying of biomaterials10.1016/j.surfcoat.2006.04.052 ↗
9. Comparison of bone-implant interface shear strength of hydroxyapatite-coated and alumina-coated implants10.1002/jbm.820290104 ↗
10. Seven-year results of a tapered, titanium, hydroxyapatite-coated cementless femoral stem in primary total Hip arthroplasty10.4055/cios.2010.2.4.214 ↗
11. How useful is SBF in predicting in vivo bone bioactivity10.1016/j.biomaterials.2006.01.017 ↗
12. Novel bioactive materials with different mechanical properties10.1016/S0142-9612(03)00044-9 ↗
13. Acoustic emission and fatigue damage induced in plasma sprayed hydroxyapatite coating layer10.1016/j.jmbbm.2011.11.011 ↗
14. Fatigue and acoustic emission behavior of plasma sprayed HAp top coat and HAp/Ti bond coat with HAp top coat on commercially pure titanium10.4028/www.scientific.net/KEM.452-453.857 ↗
15. Acoustic emission source analysis of vacuum plasma sprayed CoNiCrAlY coatings
16. Adhesive and bending failure of thermal sprayed hydroxyapatite coatings: effect of nanostructures at interface and crack propagation phenomenon during bending10.1016/j.engfracmech.2006.06.001 ↗
17. Theoretical analysis of calcium phosphate precipitation in simulated body fluid10.1016/j.biomaterials.2004.05.034 ↗
18. Acoustic emission source analysis of plasma sprayed thermal barrier coatings during four-point bend tests10.1016/S0257-8972(01)00995-1 ↗
19. Acoustic emission study on WC–Co thermal sprayed coatings10.1016/S0921-5093(02)00546-4 ↗
20. Electrolyte crystal growth mechanisms10.1016/0022-0248(84)90189-1 ↗
21. The characterization and development of bioactive hydroxyapatite coatings JOM10.1007/s11837-006-0145-2 ↗
22. Preparation and assessment of revised simulated body fluids10.1002/jbm.a.10482 ↗
23. Acoustic emission characteristics for diagnosis of TBC damaged by high-temperature thermal fatigue10.1016/j.jmatprotec.2006.11.219 ↗
24. Plasma spraying induced changes of calcium phosphate ceramic characteristic and the effect on in vitro stability
25. Formation of hydroxyapatite layer on bioactive Ti and Ti–6Al–4V by simple chemical technique
26. Electrochemical depositions of calcium phosphate film on commercial pure titanium and Ti–6Al–4V in two types of electrolyte at room temperature10.1016/j.msec.2008.06.028 ↗
27. Characterization and fatigue damage of plasma sprayed HAp top coat with Ti and HAp/Ti bond coat layers on commercially pure titanium substrate10.1016/j.jmbbm.2008.11.001 ↗
28. Six-year results of hydroxyapatite—coated total hip replacement
29. Calcium phosphate coatings for bio-implant applications: materials, performance factors, and methodologies10.1016/j.mser.2009.05.001 ↗
30. The effect of structural characteristics on the in vitro bioactivity of hydroxyapatite10.1002/jbm.10087 ↗
31. Bone ingrowth behaviour of hydroxyapatite coated, polyethylene intruded and uncoated, sandblasted pure titanium implants in an infected implantation site: an experimental study in miniature pigs
32. Acoustic emission evaluation of the fracture behavior of APS-TBCs subjecting to bondcoating oxidation10.1002/sia.2586 ↗
33. Mechanical properties and Young's modulus of plasma-sprayed hydroxyapatite coating on Ti substrate in simulated body fluid10.1002/jbm.a.10145 ↗
34. Bond degradation at the plasma-sprayed HA coating/Ti–6Al–4V alloy interface: an in vitro study