journal article·2016-06

Modified maximum tangential stress criterion for fracture behavior of zirconia/veneer interfaces

M.M. Mirsayar, P. Park

Publisher page

Abstract

The veneering porcelain sintered on zirconia is widely used in dental prostheses, but repeated mechanical loadings may cause a fracture such as edge chipping or delamination. In order to predict the crack initiation angle and fracture toughness of zirconia/veneer bi-layered components subjected to mixed mode loadings, the accuracy of a new and traditional fracture criteria are investigated. A modified maximum tangential stress criterion considering the effect of T-stress and critical distance theory is introduced, and compared to three traditional fracture criteria. Comparisons to the recently published fracture test data show that the traditional fracture criteria are not able to properly predict the fracture initiation conditions in zirconia/veneer bi-material joints. The modified maximum tangential stress criterion provides more accurate predictions of the experimental results than the traditional fracture criteria.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Advanced ceramic materials synthesis · Dental Implant Techniques and Outcomes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (24)

Show source-provided references
1. Analysis of fracture initiation angle in some cracked ceramics using the generalized maximum tangential stress criterion10.1016/j.ijsolstr.2012.03.029 ↗
2. Experimental determination of stress field parameters in bi-material notches using photoelasticity10.1016/j.matdes.2011.06.002 ↗
3. Evaluation of first non-singular stress term in bi-material notches10.1016/j.commatsci.2010.10.007 ↗
4. On the interfacial fracture of porcelain/ zirconia and graded zirconia10.1016/j.actbio.2014.04.016 ↗
5. A test specimen for determining the fracture resistance of bimaterial interfaces10.1115/1.3176069 ↗
6. Slightly curved or kinked cracks10.1007/BF00012619 ↗
7. Stresses and distortions within zirconia-fixed dental prostheses due to the veneering process10.1016/j.actbio.2009.04.025 ↗
8. On the crack extension in plates under plane loading and transverse shear
9. Effect of zirconia surface treatments on the shear strength of zirconia/veneering ceramic composites10.4012/dmj.27.448 ↗
10. Effect of thermal expansion mismatch on the Y-TZP/veneer interfacial adhesion determined by strain energy release rate10.1016/j.jpor.2011.09.002 ↗
11. Influence of cooling rate on zirconia/veneer interfacial adhesion10.1016/j.actbio.2010.06.026 ↗
12. Strength, reliability and mode of fracture of bilayered porcelain/zirconia (Y-TZP) dental ceramics10.1016/j.biomaterials.2004.02.036 ↗
13. Kinking of a crack out of an interface10.1115/1.3176078 ↗
14. Effect of zirconia surface treatments on the shear bond strength of veneering ceramic10.1016/S0022-3913(11)60060-7 ↗
15. Adhesion determination of dental porcelain to zirconia using the schwickerath test: strength vs. fracture energy approach10.1016/j.actbio.2014.07.028 ↗
16. Analysis of interfacial fracture in dental restorations10.1016/j.dental.2011.06.009 ↗
17. On fracture of kinked interface cracks – the role of T-stress10.1016/j.matdes.2014.04.074 ↗
18. On fracture initiation angle near bi-material notches – effect of first non-singular stress term10.1016/j.engfracmech.2014.02.017 ↗
19. The role of T-stress on kinking angle of interface cracks10.1016/j.matdes.2015.05.007 ↗
20. Influence of surface modification techniques on shear bond strength between different zirconia cores and veneering ceramics10.4047/jap.2011.3.4.221 ↗
21. The theory of critical distances10.1016/j.engfracmech.2007.04.007 ↗
22. Fracture mechanics analyses of ceramic/veneer interface under mixed-mode loading10.1016/j.jmbbm.2014.07.019 ↗
23. Interface toughness of a zirconia–veneer system and the effect liner application10.1016/j.prosdent.2013.12.010 ↗
24. Stress based criterion for an interface crack kinking out of the interface in dissimilar materials10.1016/0013-7944(92)90150-D ↗