Abstract
This study aims at developing the prediction model of cyclic delamination lives of plasma-sprayed HAp coating on Ti-6Al-4V substrate by considering wear by interface contacts and dissolution effect by Simulated Body Fluid (SBF). Delamination of HAp coating can lead to loosening of implants stem and final failure in vivo. In the fracture mechanism of interfaces between HAp coating with Ti substrates, only adhesive strength (interracial tensile strength) or fatigue behavior by longitudinal cracking have been observed. Cyclic delamination mechanism by considering various loading modes and corrosion effect has not been revealed yet. The interface delamination rates by cyclic loading were much higher than those by static loading tests. The result clearly demonstrated that the interface demalination behaviors are dominated not by maximum stress, but by stress range. Surface profile measurement and SEM observation also demonstrated damages by interface contact or third body wear at delamination tips of HAp coating only in the cases of compressions. The mechanisms of acceleration on the delaminations are third-body wear or wedge effect by worn particles which increased mean stress level during cyclic loading. Cyclic loading tests under SBF also revealed that cyclic delamination lives were shortened probably due to crevice corrosion at interfaces. Dissolutions at the tips of delaminations were observed by SEM images under tensile loading condition in SBF. Linearly adding the effects of wear and dissolutions into Paris law could successfully predict the delamination lives of HAp coating for various loading ratios in SBF.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Bone Tissue Engineering Materials · Orthopaedic implants and arthroplasty · Dental materials and restorations
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. The pathology of total joint arthroplasty II. Mechanisms of implant failure10.1007/s002560050552 ↗
2. Effect of atmosphere on phase transformation in plasma-sprayed hydroxyapatite coatings during heat treatment10.1002/(SICI)1097-4636(199701)34:1<15::AID-JBM3>3.0.CO;2-Q ↗
3. High revision rate of hydroxyapatite-coated abg-i prosthesis10.1007/s00776-009-1367-2 ↗
4. Six-year results of hydroxyapatite-coated total hip replacement10.1302/0301-620X.77B4.7615595 ↗
5. Compositional and microstructural changes of engineered plasma-sprayed hydroxyapatite coatings on Ti6Al4V substrates during incubation in protein-free simulated body fluid10.1002/1097-4636(2000)53:6<685::AID-JBM11>3.0.CO;2-B ↗
6. Hakozaki, Y., Otsuka, Y., Miyashita, Y., Mutoh, Y., 2016. Effects of adhesives on interfacial strength of plasma-sprayed hydroxyapatite coating. In: Proceedings of APCFS2016, Toyama, Japan.10.1299/jsmemecj.2016.W041004 ↗
7. Failure analysis of a total hip prosthesis implanted in active patient10.1016/j.jmbbm.2010.06.004 ↗
8. In vivo surface wear mechanisms of femoral components of cemented total hip arthroplasties10.1016/S0883-5403(03)00278-X ↗
9. Implants for surgery—partial and total hip joint prostheses—Part 4: Determination of endurance properties and performance of stemmed femoral components, ISO 7206-4:2010.
10. Basic knowledge and clinical cases of loosing of total hip joint (thp)
11. Analysis of surface cracking in lubricated rolling contact10.1299/kikaic.51.2618 ↗
12. Plasma spraying of functionally graded hydroxyapatite/Ti-6Al4V coatings10.1016/S0257-8972(03)00238-X ↗
13. Observations of surface crack growth and wear in Si3N4 under ball-on-plate contact10.1299/kikaia.65.846 ↗
14. How useful is {SBF} in predicting in vivo bone bioactivity?10.1016/j.biomaterials.2006.01.017 ↗
15. Acoustic emission and fatigue damage induced in plasma-sprayed hydroxyapatite coating layers10.1016/j.jmbbm.2011.11.011 ↗
16. Failure behavior of plasma-sprayed {HAp} coating on commercially pure titanium substrate in simulated body fluid (sbf) under bending load10.1016/j.jmbbm.2012.05.017 ↗
17. N. Hailer, Increased risk of revision of acetabular cups coated with hydroxyapatite10.3109/17453670903413178 ↗
18. NEDO, Technology assessment technology of bio-compatibility implant material (in Japanese), NEDO, 2008.
19. NIH Consensus Conference: Total hip replacement. NIH consensus development panel on total hip replacement. J. Am. Med. Assoc. 273 (24) (1995) 1950–1956.10.1001/jama.1995.03520480070043 ↗
20. Mechanical properties of biomedical titanium alloys10.1016/S0921-5093(97)00806-X ↗
21. Mechanical biocompatibilities of titanium alloys for biomedical applications10.1016/j.jmbbm.2007.07.001 ↗
22. Effect of dissolution/precipitation on the residual stress redistribution of plasma-sprayed hydroxyapatite coating on titanium substrate in simulated body fluid (sbf)10.1016/j.jmbbm.2014.04.007 ↗
23. Cyclic delamination behavior of plasma-sprayed hydroxyapatite coating on Ti–6Al–4V substrates in simulated body fluid10.1016/j.msec.2016.05.058 ↗
24. Hydroxyapatite coating improves 8-to-10–year performance of the link {RS} cementless femoral stem10.1054/arth.2002.29395 ↗
25. Characterization and fatigue damage of plasma sprayed {HAp} top coat with Ti and HAp/Ti bond coat layers on commercially pure titanium substrate10.1016/j.jmbbm.2008.11.001 ↗
26. Long-term results of ha coated threaded versus ha coated hemispheric press fit cups10.1007/s00402-006-0176-8 ↗
27. Resonant ultrasound spectroscopy measurement of Young׳s modulus, shear modulus and Poisson׳s ratio as a function of porosity for alumina and hydroxyapatite10.1080/14786430902915388 ↗
28. Material fundamentals and clinical performance of plasma-sprayed hydroxyapatite coatings10.1002/jbm.1056 ↗
29. T.J.S. of Mechanical Engineers ed., Biomechanics (in Japanese), The Japan Society of Mechanical Engineers, 1993.
30. Near-threshold fatigue crack propagation under mode iii torsional loading10.1299/kikaia.63.1627 ↗
31. Hydroxyapatite-coated femoral stems10.1302/0301-620X.81B1.0810148 ↗
32. Yamamoto, Y., Kaneta, M., 2000. Tribology, 2nd Ed. (in Japanese), Rikougakusya.
33. Influence of residual stress on bonding strength and fracture of plasma-sprayed hydroxyapatite coatings on Ti-6Al-4V substrate10.1016/S0142-9612(00)00364-1 ↗
34. Neck fracture of femoral stems with a sharp slot at the neck10.1007/s00776-015-0745-1 ↗
35. Fretting behavior of cortical bone against titanium and its alloy10.1016/j.wear.2005.01.037 ↗
36. Mechanical properties, electrochemical corrosion and in-vitro bioactivity of yttria stabilized zirconia reinforced hydroxyapatite coatings prepared by gas tunnel type plasma spraying10.1016/j.jmbbm.2011.11.002 ↗
37. Evaluation of the fatigue strength of adhesive joints based on interfacial fracture mechanics10.2472/jsms.41.1299 ↗
38. Yuuki, R., 1993. Mechanics of Interface (in Japanese), Baihuukan.