journal article·2020-03

Fatigue performance of distinct CAD/CAM dental ceramics

Guilardi LF, Soares P, Werner A, de Jager N, Pereira GKR, Kleverlaan CJ, Rippe MP, Valandro LF

Publisher page

Abstract

This study investigated the effect of surface roughness (polished vs. CAD/CAM milling roughness simulation) on the fatigue behavior of five dental ceramics for manufacturing CAD/CAM monolithic restorations. Specimens of five dental ceramics (FC- feldspathic; PICN- polymer-infiltrated ceramic-network; ZLS- zirconia-reinforced lithium silicate glass-ceramic; LD-lithium disilicate glass-ceramic; YZ-yttria-stabilized tetragonal zirconia polycrystal), to be tested under fatigue (12 × 12 × 1.2 mm3), were assigned into two groups according to surface treatment: polished 'p' (#2500-grit SiC papers) and CAD/CAM milling roughness simulation 'gr' (grinding with #60-grit SiC paper). The fatigue test was performed through the stepwise method (40N-660N; step of 20N; 10,000 cycles/step; 20 Hz frequency). Roughness, topographic and fractographic analyses were performed. The fatigue data were analyzed by Kaplan-Meier and Mantel-Cox (Log rank), and Pearson correlation was used to correlate roughness vs. fatigue data. CAD/CAM milling roughness simulation led to significantly (p < 0.05) greater roughness (Ra and Rz), promoting a more irregular topography with scratches and grooves, and led to a lower fatigue performance for all the tested ceramics. Fractographic analysis depicted the origin of failure at the higher stress concentration side, the side subjected to tensile tension during the fatigue test. The CAD/CAM milling roughness simulation significantly decreased the fatigue performance of the evaluated ceramic materials.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Dental Erosion and Treatment

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. Quantifying the strength of a resin-coated dental ceramic10.1177/154405910808700610 ↗
2. Translucency of esthetic dental restorative CAD/CAM materials and composite resins with respect to thickness and surface roughness10.1016/j.prosdent.2014.12.003 ↗
3. Chairside CAD/CAM materials. Part 1: measurement of elastic constants and microstructural characterization10.1016/j.dental.2016.10.009 ↗
4. Wear of ceramic-based dental materials10.1016/j.jmbbm.2019.01.009 ↗
5. Grinding damage assessment on four high-strength ceramics10.1016/j.dental.2015.11.028 ↗
6. Cohen · 1988
7. Damage tolerance of indirect restorative materials (including PICN) after simulated bur adjustments10.1016/j.dental.2015.03.007 ↗
8. The influence of surface roughness on porcelain strength10.1016/S0109-5641(00)00030-0 ↗
9. The effect of internal roughness and bonding on the fracture resistance and structural reliability of lithium disilicate ceramic10.1016/j.dental.2017.09.018 ↗
10. Optical properties of CAD-CAM ceramic systems10.1016/j.jdent.2014.07.005 ↗
11. Ceramics for dental applications: a review10.3390/ma3010351 ↗
12. A literature review on the new polymer-infiltrated ceramic-network material (PICN)10.1111/jerd.12370 ↗
13. Impact of machining on the flexural fatigue strength of glass and polycrystalline CAD/CAM ceramics10.1016/j.dental.2017.07.019 ↗
14. Hard machining, glaze firing and hydrofluoric acid etching: do these procedures affect the flexural strength of a leucite glass-ceramic?10.1016/j.dental.2015.04.005 ↗
15. Slow crack growth and reliability of dental ceramics10.1016/j.dental.2010.10.025 ↗
16. The phenomena of rupture and flow in solids10.1098/rsta.1921.0006 ↗
17. A novel polymer infiltrated ceramic for dental simulation10.1007/s10856-011-4350-3 ↗
18. ISO 4287 · 1997
19. ISO 6872 · 2015
20. ADM guidance-ceramics: fatigue principles and testing10.1016/j.dental.2017.09.006 ↗
21. Fracture surface analysis of dental ceramics; clinically failed restorations
22. Recent advances in understanding the fatigue and wear behavior of dental composites and ceramics10.1016/j.jmbbm.2018.08.008 ↗
23. Thickness of CAD-CAM composite resin overlays influences fatigue resistance of endodontically treated premolars10.1016/j.dental.2009.05.007 ↗
24. Fatigue failure load of zirconia-reinforced lithium silicate glass ceramic cemented to a dentin analogue: effect of etching time and hydrofluoric acid concentration10.1016/j.jmbbm.2017.09.028 ↗
25. Fatigue strength of several dental ceramics indicated for CAD-CAM monolithic restorations
26. Mechanical reliability, fatigue strength and survival analysis of new polycrystalline translucent zirconia ceramics for monolithic restorations10.1016/j.jmbbm.2018.05.029 ↗
27. Strength and fracture origins of a feldspathic porcelain10.1016/j.dental.2011.12.005 ↗
28. A practical and systematic review of Weibull statistics for reporting strengths of dental materials10.1016/j.dental.2009.09.006 ↗
29. Microstructure characterization and SCG of newly engineered dental ceramics10.1016/j.dental.2016.03.018 ↗
30. Influence of the geometry of ceramic specimens on biaxial flexural strength: experimental testing and finite element analysis10.1590/0366-69132018643692287 ↗
31. Internal adjustments decrease the fatigue failure load of bonded simplified lithium disilicate restorations10.1016/j.dental.2018.05.015 ↗
32. ADM guidance-Ceramics: guidance to the use of fractography in failure analysis of brittle materials10.1016/j.dental.2017.03.004 ↗
33. Strengthening of porcelain provided by resin cements and flowable composites10.2341/15-025-L ↗
34. Fracture surface characterization of clinically failed all-ceramic crowns10.1177/00220345940730120601 ↗
35. Dental ceramics and the molar crown testing ground10.1590/S1678-77572004000500004 ↗
36. The effect of hydrofluoric acid concentration on the fatigue failure load of adhesively cemented feldspathic ceramic discs10.1016/j.dental.2018.01.010 ↗
37. Chairside CAD/CAM materials. Part 2: flexural strength testing10.1016/j.dental.2016.10.008 ↗
38. Failure responses of a dental porcelain having three surface treatments under three stressing conditions10.1016/j.dental.2011.09.002 ↗
39. Dental ceramics for restoration and metal veneering10.1016/j.cden.2017.06.005 ↗
40. CAD/CAM machining vs pre-sintering in-lab fabrication techniques of Y-TZP ceramic specimens: effects on their mechanical fatigue behavior10.1016/j.jmbbm.2017.03.013 ↗