Hertzian contact response and damage tolerance of dental ceramics
Source abstract
Abstract
Objectives To determine the contact response and damage tolerance or strength degradation of a range of dental CAD/CAM ceramic materials including novel polymer-infiltrated-ceramic-network (PICN) materials by means of spherical indentations at various loads and indenter radii. Methods The seven tested materials included Mark II, PICN test materials 1 and 2, In-Ceram Alumina, VM 9, In-Ceram YZ (Vita Zahnfabrik, Bad Saeckingen, Germany) and IPS e.max CAD, (Ivoclar Vivadent, Schaan, Liechtenstein). To evaluate the damage tolerance and role of indenter size, indentations with tungsten carbide spheres (0.5mm and 1.25mm radius) were placed on bending bars with varying loads (1.96-1000N). The indented bending bars were subsequently loaded to fracture in three-point bending. The contact induced damage was analyzed by light microscopy (LM) and SEM. The spherical contact response was measured on polished surfaces. Results The initial strengths for the individual materials were found to reduce above specific indentation loads, which were a function of the indenter radius. Employing a 0.5mm radius sphere resulted in the following strength degrading loads and ordering of materials: VM9 (98N)SignificanceThis study aims to emulate the likely clinical behavior of contact loading by opposing cusps to dental restorative ceramic materials by utilizing spherical indentations at various loads and sphere diameters.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Endodontics and Root Canal Treatments
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (18)
Show source-provided references
1. The fracture behaviour of dental enamel10.1016/j.biomaterials.2009.09.050 ↗
2. In-vitro strength degradation of dental ceramics and novel PICN material by sharp indentation10.1016/j.jmbbm.2013.05.004 ↗
3. Mechanical properties of polymer-infiltrated-ceramic-network materials10.1016/j.dental.2013.01.002 ↗
4. Hertzian contact response of dentin with loading rate and orientation10.1016/j.archoralbio.2008.02.013 ↗
5. An evaluation of dental operative simulation materials10.4012/dmj.2011-264 ↗
6. A novel polymer infiltrated ceramic for dental simulation
7. Nanoindentation derived stress–strain properties of dental materials10.1016/j.dental.2006.06.017 ↗
8. A novel polymer infiltrated ceramic dental material10.1016/j.dental.2011.02.002 ↗
9. ISO Standard 6872:2008, 2009. Dentistry – Ceramic Materials. January 2009.
10. Contact damage resistance and strength degradation of glass-infiltrated alumina and spinel ceramics10.1177/00220345990780031401 ↗
11. Indentation of ceramics with spheres: a century after Hertz10.1111/j.1151-2916.1998.tb02580.x ↗
12. Use of contact testing in characterization and design of all-ceramic crownlike layer structures: a review10.1067/mpr.2001.119581 ↗
13. Strength degradation of brittle surfaces: blunt indenters10.1111/j.1151-2916.1975.tb19015.x ↗
14. Mechanical characterization of dental ceramics by Hertzian contacts10.1177/00220345980770041201 ↗
15. Role of microstructure on contact damage and strength degradation of micaceous glass–ceramics10.1016/S0109-5641(98)00013-X ↗
16. Brittle fracture versus quasi plasticity in ceramics: a simple predictive index10.1111/j.1151-2916.2001.tb00698.x ↗
17. Tomography of indentation cracks in feldspathic dental porcelain on zirconia10.1016/j.dental.2013.01.001 ↗
18. Indentation damage and mechanical properties of human enamel and dentin10.1177/00220345980770030601 ↗