journal article·2015-04Open access

High compressive pre-strains reduce the bending fatigue life of nitinol wire

Shikha Gupta, Alan R. Pelton, Jason D. Weaver, Xiao-Yan Gong, Srinidhi Nagaraja

Abstract

Prior to implantation, Nitinol-based transcatheter endovascular devices are subject to a complex thermo-mechanical pre-strain associated with constraint onto a delivery catheter, device sterilization, and final deployment. Though such large thermo-mechanical excursions are known to impact the microstructural and mechanical properties of Nitinol, their effect on fatigue properties is still not well understood. The present study investigated the effects of large thermo-mechanical pre-strains on the fatigue of pseudoelastic Nitinol wire using fully reversed rotary bend fatigue (RBF) experiments. Electropolished Nitinol wires were subjected to a 0%, 8% or 10% bending pre-strain and RBF testing at 0.3-1.5% strain amplitudes for up to 10(8) cycles. The imposition of 8% or 10% bending pre-strain resulted in residual set in the wire. Large pre-strains also significantly reduced the fatigue life of Nitinol wires below 0.8% strain amplitude. While 0% and 8% pre-strain wires exhibited distinct low-cycle and high-cycle fatigue regions, reaching run out at 10(8) cycles at 0.6% and 0.4% strain amplitude, respectively, 10% pre-strain wires continued to fracture at less than 10(5) cycles, even at 0.3% strain amplitude. Furthermore, over 70% fatigue cracks were found to initiate on the compressive pre-strain surface in pre-strained wires. In light of the texture-dependent tension-compression asymmetry in Nitinol, this reduction in fatigue life and preferential crack initiation in pre-strained wires is thought to be attributed to compressive pre-strain-induced plasticity and tensile residual stresses as well as the formation of martensite variants. Despite differences in fatigue life, SEM revealed that the size, shape and morphology of the fatigue fracture surfaces were comparable across the pre-strain levels. Further, the mechanisms underlying fatigue were found to be similar; despite large differences in cycles to failure across strain amplitudes and pre-strain levels, cracks initiated from surface inclusions in nearly all wires. Compressive pre-strain-induced damage may accelerate such crack initiation, thereby reducing fatigue life. The results of the present study indicate that large compressive pre-strains are detrimental to the fatigue properties of Nitinol, and, taken together, the findings underscore the importance of accounting for thermo-mechanical history in the design and testing of wire-based percutaneous implants.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Shape Memory Alloy Transformations · Ferroelectric and Piezoelectric Materials · Magnetic and transport properties of perovskites and related materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (64)

Show source-provided references
1. Bannantine · 1990
2. Impact of thermomechanical texture on the superelastic response of Nitinol implants10.1016/j.jmbbm.2011.05.013 ↗
3. Bending of Superelastic Wires. 1. Experimental Aspects10.1115/1.2895952 ↗
4. Bhattacharya · 2003
5. Stress-induced transformation behavior of a polycrystalline NiTi shape memory alloy: micro and macromechanical investigations via in situ optical microscopy10.1016/j.jmps.2004.01.001 ↗
6. Surface cracks in notched round bars under cyclic tension and bending10.1016/j.ijfatigue.2005.05.006 ↗
7. A.S.M. International. Factors causing compressive damage-induced cracking in Nitinol
8. An overview of Nitinol medical applications10.1016/S0921-5093(99)00294-4 ↗
9. Duerig · 1990
10. Fracture of the GORE HELEX septal occluder: associated factors and clinical outcomes
11. The role of texture in tension-compression asymmetry in polycrystalline NiTi10.1016/S0749-6419(98)00060-6 ↗
12. Tension–ompression asymmetry of the stress-strain response in aged single crystal and polycrystalline NiTi10.1016/S1359-6454(98)00432-7 ↗
13. Superelastic deformation of a TiNi shape memory alloy subjected to various cyclic loadings
14. Fatigue-life computational analysis for the self-expanding endovascular Nitinol stents10.1007/s11665-012-0150-2 ↗
15. On the experimental testing of fine Nitinol wires for medical devices10.1016/j.jmbbm.2010.10.004 ↗
16. Effect of stress state on the stress-induced martensitic transformation in polycrystalline Ni–Ti alloy10.1007/BF02663855 ↗
17. James, B., et al. (2004). Compressive Damage-Induced Cracking in Nitinol. Proceedings of the International Conference on Shape Memory and Superelastic Technologies. Baden-Baden, Germany SMST: 117-124
18. Five-year clinical and echocardiographic evaluation of the Das AngelWings atrial septal occluder
19. Computational mechanics of Nitinol stent grafts10.1016/j.jbiomech.2008.05.032 ↗
20. Design and finite element-based fatigue prediction of a new self-expandable percutaneous mitral valve stent10.1016/j.cad.2013.05.003 ↗
21. Self-expanding aortic valve stent—material optimization10.1016/j.compbiomed.2012.08.007 ↗
22. Influence of microstructural purity on the bending fatigue behavior of VAR-melted superelastic Nitinol10.1016/j.jmbbm.2014.02.008 ↗
23. The influence of carbon content of cyclic fatigue of NiTi SMA wires10.1111/j.1365-2591.2011.01864.x ↗
24. Crystallography of martensitic-transformation in Ti–Ni crystals10.1016/0001-6160(87)90042-3 ↗
25. Effect of thermal cycling on the transformation temperatures of Ti–Ni alloys10.1016/0001-6160(86)90263-4 ↗
26. The habit plane and transformation strains associated with the martensitic-transformation in Ti–Ni single crystals10.1016/0036-9748(84)90254-0 ↗
27. Morgan, N.B., Painter, J., Moffat, A., 2004. Mean strain effects and microstructural observations during in vitro fatigue testing of NiTi. SMST - Proceedings on International Conference on Shape Memory and Superelastic Technologies, Pacific Grove, CA, pp. 303–310
28. Fracture of self-expanding nitinol stents stressed in vitro under simulated intravascular conditions10.1016/j.jvs.2008.02.029 ↗
29. A comparison of zero mean strain rotating beam fatigue test methods for Nitinol wire10.1007/s11665-014-0939-2 ↗
30. A study of the effect of diameter on the fatigue properties of NiTi wire10.1007/s11665-009-9415-9 ↗
31. Power-Law Creep in Near-Equiatomic Nickel-Titanium Alloys10.1016/j.scriptamat.2007.05.004 ↗
32. Physical metallurgy of Ti–Ni-based shape memory alloys10.1016/j.pmatsci.2004.10.001 ↗
33. Patel, M., Plumley, D., Bouthot, R., Proft, J., 2006. The effects of varying active af temperatures on the fatigue properties of nitinol wire. In: Venugopalan, R., Wu, M. (Eds.), Medical Device Materials III: Proceedings from the Materials & Processes for Medical Devices Conference 2005, pp. 148–153.
34. Patel, M.M., Gordon, R.F., 2008. An investigation of diverse surface finishes on fatigue properties of superelastic Nitinol wire. In: Berg, B., Mitchell, M.R., Proft, J. (Eds.), SMST 2006: Proceedings of the International Conference on Shape Memory and Superelastic Technologies, pp. 61–70.
35. Nitinol fatigue: a review of microstructures and mechanisms10.1007/s11665-011-9864-9 ↗
36. Optimisation of processing and properties of medical grade Nitinol wire10.3109/13645700009063057 ↗
37. A guide to shape memory and superelasticity in Nitinol medical devices10.1080/13645700410017236 ↗
38. Rotary-bending fatigue characteristics of medical-grade Nitinol wire10.1016/j.jmbbm.2013.06.003 ↗
39. Effects of thermal cycling on microstructure and properties in Nitinol10.1016/j.msea.2011.10.073 ↗
40. The physical metallurgy of Nitinol for medical applications10.1007/s11837-003-0243-3 ↗
41. Fatigue and durability of Nitinol stents10.1016/j.jmbbm.2007.08.001 ↗
42. Strength differential effect in pseudoelastic NiTi shape memory alloys10.1016/S1359-6454(96)00354-0 ↗
43. Bending rotation HCF testing of pseudoelastic Ni–Ti shape memory alloys10.1002/mawe.201300118 ↗
44. Impurity levels and fatigue lives of pseudoelastic NiTi shape memory alloys10.1016/j.actamat.2013.02.054 ↗
45. Study of a Nitinol stent deployed into anatomically accurate artery geometry and subjected to realistic service loading10.1007/s11665-009-9375-0 ↗
46. Tension, compression, and bending of superelastic shape memory alloy tubes10.1016/j.jmps.2012.12.012 ↗
47. Reinoehl, M., Bradley, D., Bouthot, R., Proft, J., 2001. The influence of melt practice on final fatigue properties of superelastic NiTi wires, In: Russell, S.M., Pelton, A.R. (Eds.), 2000 SMST – Proceedings on International Conference on Shape Memory and Superelastic Technologies. Pacific Grove, CA, pp. 397–403.
48. Effect of product form and heat treatment on the crystallographic texture of austenitic Nitinol10.1007/s10853-006-6478-y ↗
49. Evolution of crack-tip transformation zones in superelastic Nitinol subjected to in situ fatigue: a fracture mechanics and synchrotron X-ray microdiffraction analysis10.1016/j.actamat.2007.07.028 ↗
50. Mechanical fatigue and fracture of Nitinol10.1179/1743280411Y.0000000009 ↗
51. Statistical duplex S–N characteristics of high carbon chromium bearing steel in rotating bending in very high cycle regime10.1016/j.ijfatigue.2009.08.001 ↗
52. Fatigue performance of nitinol round wire with varying cold work reductions10.1007/s11665-009-9363-4 ↗
53. Effects of cyclic loading on the uniaxial behavior of Nitinol10.1007/s11665-010-9790-2 ↗
54. Thermomechanical aspects of NiTi10.1016/0022-5096(95)00024-D ↗
55. Sheriff, J., Pelton, A.R., Pruitt, L.A., 2005. Hydrogen effects on nitinol fatigue. In: Helmus, M., Medlin, D. (Eds.), Medical Device Materials II: Proceedings from the Materials & Processes for Medical Devices Conference 2004, pp. 38–43.
56. Shape Memory Alloys
57. Micromechanical quantification of elastic, twinning, and slip strain partitioning exhibited by polycrystalline, monoclinic nickel–titanium during large uniaxial deformations measured via in-situ neutron diffraction10.1016/j.jmps.2013.05.008 ↗
58. Stephens · 2000
59. Mean stress effects on fatigue of NiTi10.1016/S0921-5093(99)00340-8 ↗
60. Incidence of stent fractures and patency after femoropopliteal stenting with the nitinol self-expandable SMART stent: a single-center study10.2459/JCM.0b013e3283383370 ↗
61. Effect of thermal cycling on the thermomechanical behaviour of NiTi shape memory alloys10.1016/j.msea.2008.10.026 ↗
62. Effects of test speed on fatigue life of Nitinol wire in rotary bend
63. Wick, A., Gong, X.Y., Fino, J., Sheriff, J., Pelton, A.R., 2005. Bending fatigue characteristics of nitinol. Medical Device Materials II: Proceedings from the Materials & Processes for Medical Devices Conference 2004, pp. Minneapolis, MN, pp. 15-20.