Enhancing bond strength on demineralized dentin by pre-treatment with selective remineralising agents
Source abstract
Abstract
Bonding to demineralized dentin of a diseased tooth has shown to be a significant clinical issue. This study evaluated the effect of 0.2% NaF-(NaF), MI Paste™-(CPP-ACP) and the self-assembling peptide 'P11-4' (Ace-QQRFEWEFEQQ-NH2) contained in Curodont™ Repair, have on microtensile bond strength-(µTBS) of two different adhesive systems (Adper™ Single Bond-(SB) or Clearfil™ SE Bond (CSE)) and wettability of demineralized dentin slices after remineralising agents were applied. The highest µTBS were found for the demineralized dentin-(DD) treated with CPP-ACP; both adhesives systems (p < 0.05) did not significantly difference from P11-4 treatment associated with SB, and also presented higher values than sound dentin-(SD/SB) (p < 0.01). DD treated with P11-4 associated with CSE did not differ from DD/CSE (p > 0.05). The NaF treatment associated with CSE recovered the bond strength values of SD/CSE and associated with CSE demonstrated lower µTBS than other groups, although significantly higher than DD (p < 0.05). P11-4 and CPP-ACP increased significantly the wettability of demineralized dentin (p < 0.05); etching acid improved wettability for all groups (p < 0.05), whilst NaF did not affect the wettability of demineralized dentin (p > 0.05). Morphological analysis of the dentin surface and dentin-resin interface revealed unique features of the applied remineralizing agent. The results indicated that self-assembling peptide P11-4 associated with SB and CPP-ACP associated with SB or CSE significantly enhanced the bond strength to demineralized dentin (p < 0.05). We conclude that by modifying the dentine surface and restoring conditions found on sound dentin, this can enhance the interfacial bonding.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Dental Erosion and Treatment · Orthodontics and Dentofacial Orthopedics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. pH as a trigger of peptide β-sheet self-assembly and reversible switching between nematic and isotropic phases10.1021/ja021047i ↗
2. NaF inhibits matrix-bound cathepsin-mediated dentin matrix degradation10.1159/000444222 ↗
3. Remineralization of bovine dentine in vitro10.1159/000261198 ↗
4. Influence of 3-month simulated pulpal pressure on the microtensile bond strength of simplified resin luting systems
5. Effect of casein Phosphopeptide-amorphous calcium phosphate treatment on microtensile bond strength to carious affected dentin using two adhesive strategies
6. Effect of dentin pre-treatment with a casein phosphopeptide-amorphous calcium phosphate (CPP-ACP) paste on dentin bond strength in tridimensional cavities
7. Effect of sodium fluoride on the endogenous MMP activity of dentin matrices
8. Treatment of early caries lesions using biomimetic self-assembling peptides--a clinical safety trial10.1038/sj.bdj.2013.741 ↗
9. Biomimetic mineralisation of phosphorylated dentine by CPP-ACP10.1016/j.jdent.2013.06.008 ↗
10. Confocal laser scanning microscopic analysis of the depth of dentin caries-like lesions in primary and permanent teeth10.1590/S0103-64402008000200010 ↗
11. Microtensile bond strength of total-etch and self-etching adhesives to caries-affected dentine10.1016/S0300-5712(03)00088-5 ↗
12. Effect of self‐assembling peptide P11‐4 on enamel erosion: AFM and SEM studies10.1002/sca.21276 ↗
13. Effect of metalloproteinase inhibitors on the microtensile bond strength of composite resin to Er: YAG laser-irradiated dentin10.1590/0103-6440201600825 ↗
14. Self-assembly of amphiphilic beta-sheet peptide tapes based on aliphatic side chains10.1002/psc.1335 ↗
15. Two layers of carious dentin; diagnosis and treatment
16. Self-etch adhesive systems: a literature review10.1590/0103-6440201302442 ↗
17. CPP-ACP complex as a new adjunctive agent for remineralisation: a review
18. Efficacy of the self-assembling peptide P11-4 in constructing a remineralization scaffold on artificially-induced enamel lesions on smooth surfaces10.1007/s00056-014-0211-2 ↗
19. Biomimetic remineralization of carious lesions by self-assembling peptide10.1177/0022034517698419 ↗
20. Self-assembling peptide scaffolds promote enamel remineralization10.1177/154405910708600507 ↗
21. Recombinant self-assembling peptides as biomaterials for tissue engineering10.1016/j.biomaterials.2010.08.051 ↗
22. Does the method of caries induction influence the bond strength to dentin of primary teeth
23. Limitations in bonding to dentin and experimental strategies to prevent bond degradation10.1177/0022034510391799 ↗
24. Effect of chlorhexidine on the bond strength of a self-etch adhesive system to sound and demineralized dentin10.1590/S1806-83242013005000008 ↗
25. The dentin substrate: structure and properties related to bonding10.1016/S0300-5712(96)00065-6 ↗
26. Remineralization of advanced root dentin lesions in vitro10.1159/000063924 ↗
27. In vitro longevity of bonding properties of universal adhesives to dentin10.2341/14-055-L ↗
28. Biomimetic remineralization of dentin10.1016/j.dental.2013.07.013 ↗
29. Molecular and structural evaluation of dentin caries-like lesions produced by different artificial models10.1590/0103-6440201302357 ↗
30. State of the art etch-and-rinse adhesives10.1016/j.dental.2010.10.016 ↗
31. Bond strengths of a 1-step self-etching system to caries-affected and normal dentin10.2341/05-131 ↗
32. Carious affected dentine: its behaviour in adhesive bonding10.1111/adj.12309 ↗
33. In vitro remineralization of enamel subsurface lesions and assessment of dentine tubule occlusion from NaF dentifrices with and without calcium10.4103/0970-4388.112403 ↗
34. Effect of a CPP-ACP agent on the demineralization and remineralization of dentine in vitro10.1016/j.jdent.2007.05.008 ↗
35. Calcium phosphate‐based remineralization systems: scientific evidence?10.1111/j.1834-7819.2008.00061.x ↗
36. Influence of cavity disinfectant and adhesive systems on the bonding procedure in demineralized dentin-a one-year in vitro evaluation
37. Bonding of resin luting cements to dentine after casein phosphopeptide–amorphous calcium phosphate (CPP–ACP) treatment10.1016/j.ijadhadh.2014.05.008 ↗
38. Evaluation of microtensile bond strength of self-etching adhesives on normal and caries-affected dentin10.4012/dmj.2014-330 ↗
39. Remineralization of natural early caries lesions in vitro by P11‐4 monitored with photothermal radiometry and luminescence10.1111/jicd.12257 ↗
40. Assessment of enamel remineralisation after treatment with four different remineralising agents: a scanning electron microscopy (SEM) study
41. Strategies to prevent hydrolytic degradation of the hybrid layer – a review10.1016/j.dental.2013.07.016 ↗
42. Surface microanalysis and chemical imaging of early dentin remineralization10.1017/S1431927613013639 ↗
43. Wettability and surface morphology of eroded dentin treated with chitosan10.1016/j.archoralbio.2016.11.017 ↗
44. Bonding of self-etch and total-etch adhesives to carious dentin10.1177/154405910208100811 ↗
45. CO2laser irradiation enhances CaF2formation and inhibits lesion progression on demineralized dental enamel—in vitro study10.1007/s10103-016-1900-4 ↗
46. Contemporary research findings on dentine remineralization10.1002/term.1814 ↗