journal article·2017-10

A comparative study of progressive wear of four dental monolithic, veneered glass-ceramics

Zhenzhen Zhang, Yuanping Yi, Xuesong Wang, Jiawen Guo, Ding Li, Lin He, Shaofeng Zhang

Publisher page

Abstract

Objectives This study evaluated the wear performance and wear mechanisms of four dental glass-ceramics, based on the microstructure and mechanical properties in the progressive wear process. Methods Bar (N = 40, n = 10) and disk (N = 32, n = 8) specimens were prepared from (A) lithium disilicate glass-ceramic (LD), (B) leucite reinforced glass-ceramic (LEU), (C) feldspathic glass-ceramic (FEL), and (D) fluorapatite glass-ceramic (FLU). The bar specimens were tested for three-point flexural strength, hardness, fracture toughness and elastic modulus. The disk specimens paired with steatite antagonists were tested in a pin-on-disk tribometer with 10N up to 1000,000 wear cycles. The wear analysis of glass-ceramics was performed using a 3D profilometer after every 200,000 wear cycles. Wear loss of steatite antagonists was calculated by measuring the weight and density using sensitive balance and Archimedes' method. Wear morphologies and microstructures were analyzed by scanning electron microscopy (SEM). The crystalline phase compositions were determined using X-ray diffraction (XRD). One-way analysis of variance (ANOVA) was used to analyze the data. Multiple pair-wise comparison of means was performed by Tukey's post-hoc test. Results LD showed the highest fracture toughness, flexural strength, elastic modulus and crystallinity, followed by LEU and FEL, and FLU showed the lowest. However, the hardness of LD was lower than all the other three types of ceramics. For steatite antagonists, LD produced the least wear loss of antagonist, followed by LEU and FEL, and FLU had the most wear loss. For glass-ceramic materials, LD exhibited similar wear loss as LEU, but more than FLU and FEL did. Moreover, fracture occurred on the wear surface of FLU. Conclusions In the progressive wear process, veneering porcelains showed better wear resistance but fluorapatite veneering porcelains appeared fracture surface. Monolithic lithium disilicate glass-ceramics with higher mechanical properties showed more wear loss, however, they did not fracture and produced less wear loss of antagonists.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Advanced ceramic materials synthesis · Recycling and utilization of industrial and municipal waste in materials production

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Fracture toughness and hardness evaluation of three pressable all-ceramic dental materials10.1016/S0300-5712(03)00025-3 ↗
2. Two-body wear of different ceramic materials opposed to zirconia ceramic10.1016/S0022-3913(10)60102-3 ↗
3. Three-body wear potential of dental yttrium-stabilized zirconia ceramic after grinding, polishing, and glazing treatments10.1016/j.prosdent.2013.12.021 ↗
4. Residual stress in glass: indentation crack and fractography approaches
5. Influence of hardness of the counterbody in three-body abrasive wear—an overlooked hardness effect10.1016/0301-679X(94)90003-5 ↗
6. Fatigue of restorative materials10.1177/10454411010120040501 ↗
7. Stone age man's dentition: with reference to anatomically correct occlusion, the etiology of malocclusion, and a technique for its treatment10.1016/0002-9416(54)90118-9 ↗
8. Effect of microstructure on sliding-wear properties of liquid-phase-sintered α-SiC10.1111/j.1551-2916.2005.00394.x ↗
9. Crystallization of high-strength fine-sized leucite glass-ceramics10.1177/0022034510377795 ↗
10. Crystallization and flexural strength optimization of fine-grained leucite glass-ceramics for dentistry
11. A comparative study of sliding wear of nonmetallic dental restorative materials with emphasis on micromechanical wear mechanisms10.1002/jbm.b.33193 ↗
12. Investigation of the time-dependent wear behavior of veneering ceramic in porcelain fused to metal crowns during chewing simulations10.1016/j.jmbbm.2014.08.006 ↗
13. Studies of crystal phase formations in high-strength lithium disilicate glass–ceramics10.1016/j.jnoncrysol.2006.06.039 ↗
14. Wear evaluation of the human enamel opposing different Y-TZP dental ceramics and other porcelains10.1016/j.jdent.2012.08.004 ↗
15. Investigation on the tribological behavior and wear mechanism of five different veneering porcelains
16. Miragaya, L.M., Guimarães, R.B., Assunção e Souza, R.O.d., Santos Botelho, G.d., Antunes Guimarães, J.G., da Silva, E.M., Effect of intra-oral aging on t→m phase transformation, microstructure, and mechanical properties of Y-TZP dental ceramics. Journal of the mechanical behavior of biomedical materials.
17. Development and testing of multi-phase glazes for adhesive bonding to zirconia substrates10.1016/j.jdent.2010.06.008 ↗
18. Factors affecting enamel and ceramic wear: a literature review10.1067/mpr.2002.123851 ↗
19. Effect of heat treatment on fracture toughness K(IC) and microstructure of a fluorcanasite-based glass-ceramic10.1111/j.1532-849X.2007.00233.x ↗
20. A fractographic study of clinically retrieved zirconia-ceramic and metal-ceramic fixed dental prostheses10.1016/j.dental.2015.07.003 ↗
21. Cycle-dependent in vitro wear performance of dental ceramics after clinical surface treatments10.1016/j.jmbbm.2015.08.009 ↗
22. Influence of microstructure and chemistry on the fracture toughness of dental ceramics10.1016/S0109-5641(03)00002-2 ↗
23. Sliding contact fracture of dental ceramics: principles and validation10.1016/j.actbio.2014.03.004 ↗
24. Failure analysis of ceramic clinical cases using qualitative fractography
25. Crystallization toughening of a model glass-ceramic10.1016/j.actamat.2014.12.007 ↗
26. Wear of human enamel opposing monolithic zirconia, glass ceramic, and composite resin: an in vitro study10.1016/j.prosdent.2014.05.006 ↗
27. Effects of multiple firings on the mechanical properties and microstructure of veneering ceramics for zirconia frameworks10.1016/j.jdent.2012.01.014 ↗
28. The effects of repeated heat-pressing on the mechanical properties and microstructure of IPS e.max Press10.1016/j.jmbbm.2014.09.016 ↗
29. Reduced wear of enamel with novel fine and nano-scale leucite glass-ceramics10.1016/j.jdent.2013.02.006 ↗
30. Effects of P 2 O 5 and sintering temperature on microstructure and mechanical properties of lithium disilicate glass-ceramics10.1016/j.actamat.2007.02.009 ↗
31. Friction behavior of dental porcelain with different leucite particle sizes10.1111/j.1551-2916.2007.02179.x ↗
32. Improved densification and properties of pressureless-sintered lithium disilicate glass-ceramics10.1016/j.msea.2014.10.037 ↗