Influence of material type, thickness and storage on fracture resistance of CAD/CAM occlusal veneers
Source abstract
Abstract
Objectives The present study aimed to evaluate the effect of restoration thickness, CAD/CAM material, and 6 months of artificial saliva storage on the fracture resistance of occlusal veneers. Materials and methods A total of 84 intact maxillary molars were sectioned 4.0 mm occlusal to the cementoenamel junction to expose the dentine. The teeth were assigned into 3 main groups according to the type of restorative material (e.max CAD, Vita Enamic, and Lava Ultimate). In each group, the teeth were allocated into 2 subgroups (n = 14) according to restoration thickness (1.0 and 1.5 mm). The veneers were adhesively bonded using dual-cure self-adhesive luting agent. A total of 42 specimens comprising half the tested subgroups were stored in distilled water for 24-h before the test. The remaining half was stored in artificial saliva at 37 ± 1 °C in an incubator for 6 months. All specimens (n = 84) were subjected to 5000 thermal cycles between 5 and 55 °C ± 2 before the fracture resistance test. The maximum force at fracture was recorded in Newton. Failure mode was analyzed using a stereomicroscope. The results were analyzed using a parametric Three-way ANOVA test. Results The results of the Three-way ANOVA test revealed that material type and restoration thickness significantly affected fracture resistance values (p < 0.5), while 6 months of storage in artificial saliva had no significant effect on mean fracture resistance values (p˃0.5). The most common failure patterns in CAD/CAM resin composite and polymer-infiltrated ceramics were scores I and score II. For glass ceramic groups, score IV and III were more dominant. Conclusions All the tested CAD/CAM restorations in both thicknesses exhibited fracture resistance values exceeding normal and parafunctional bite forces. Polymer-infiltrated ceramics and CAD/CAM resin composite veneers showed more favorable fracture patterns.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Dental Research and COVID-19 · Endodontics and Root Canal Treatments
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (58)
Show source-provided references
1. Fracture resistance of ceramic and polymer-based occlusal veneer restorations10.1016/j.jmbbm.2017.06.013 ↗
2. Porcelain fracture resistance of screw-retained, cement-retained, and screw-cement-retained implant-supported metal ceramic posterior crowns10.1111/j.1532-849X.2009.00560.x ↗
3. Impact of tooth wear on daily living
4. Fracture resistance of CAD/CAM occlusal veneers: a systematic review of laboratory study10.1016/j.jmbbm.2020.103948 ↗
5. Effect of different computer-aided design/computer-aided manufacturing (CAD/CAM) materials and thicknesses on the fracture resistance of occlusal veneers10.2341/17-131-L ↗
6. Fracture strength of all-ceramic crowns luted using two bonding methods10.1016/j.prosdent.2003.12.005 ↗
7. Influence of ceramic thickness and ceramic materials on fracture resistance of posterior partial coverage restorations10.2341/12-459-L ↗
8. Strength and fracture pattern of monolithic CAD/CAM-generated posterior crowns10.1016/j.dental.2005.02.007 ↗
9. Effect of etching and airborne particle abrasion on the microstructure of different dental ceramics10.1016/S0022-3913(02)52704-9 ↗
10. Effect of the seating pressure on the adhesive bonding of indirect restorations
11. The effect of application sustained seating pressure on adhesive luting procedure10.1016/j.dental.2006.01.006 ↗
12. Fracture resistance of premolars restored with inlay and onlay ceramic restorations and luted with two different agents10.1016/j.jpor.2010.07.001 ↗
13. In vitro comparison of mechanical properties and degree of cure of bulk fill composites10.1007/s00784-012-0702-8 ↗
14. Effect of different storage media on the microhardness and wear resistance of resin‐matrix ceramics10.1111/ijac.13307 ↗
15. Bonding of an auto-adhesive luting material to enamel and dentin10.1016/j.dental.2004.03.002 ↗
16. Effect of thermocycling on the microleakage of conventional and resin-modified glass ionomers
17. Adhesion to Y-TZP ceramic: study of silica nanofilm coating on the surface of Y-TZP10.1002/jbm.b.33184 ↗
18. Fracture strength of ultrathin occlusal veneer restorations made from CAD/CAM composite or hybrid ceramic materials10.1016/S1348-8643(15)00017-8 ↗
19. Fracture resistance and microleakage of endocrowns utilizing three CAD-CAM blocks10.2341/13-143-L ↗
20. In vivo validation of the historical in vitro thermocycling temperature range for dental materials testing10.1007/s00784-004-0267-2 ↗
21. Influence of preparation design and ceramic thicknesses on fracture resistance and failure modes of premolar partial coverage restorations10.1016/S0022-3913(13)60374-1 ↗
22. Fracture resistance of premolars restored with partial ceramic restorations and submitted to two different loading stresses10.2341/05-11 ↗
23. A novel polymer infiltrated ceramic for dental simulation10.1007/s10856-011-4350-3 ↗
24. Bonding effectiveness of adhesive luting agents to enamel and dentin10.1016/j.dental.2005.12.002 ↗
25. Data on changes in flexural strength and elastic modulus of dental CAD/CAM composites after deterioration tests10.1016/j.dib.2019.103889 ↗
26. Fracture toughness of water-aged resin composite restorative materials10.1016/0109-5641(95)80019-0 ↗
27. Ultra-thin occlusal veneers bonded to enamel and made of ceramic or hybrid materials exhibit load-bearing capacities not different from conventional restorations10.1016/j.jmbbm.2018.09.041 ↗
28. Fracture strength of CAD/CAM composite and composite-ceramic occlusal veneers10.1016/j.jpor.2014.01.001 ↗
29. Ten-year outcome of three-unit fixed dental prostheses made from monolithic lithium disilicate ceramic10.14219/jada.archive.2012.0147 ↗
30. Mechanical properties of composite resin blocks for CAD/CAM10.4012/dmj.2014-208 ↗
31. Artificial salivas: present and future10.1177/00220345870660S215 ↗
32. The effect of thermocycling regimens on the nanoleakage of dentin bonding systems10.1016/S0109-5641(01)00081-1 ↗
33. Severe tooth wear: European consensus statement on management guidelines
34. Load-bearing properties of minimal-invasive monolithic lithium disilicate and zirconia occlusal onlays: finite element and theoretical analyses10.1016/j.dental.2013.04.004 ↗
35. Numeric simulation of occlusal interferences in molars restored with ultrathin occlusal veneers10.1016/j.prosdent.2016.07.008 ↗
36. Porcelain veneers: dentin bonding optimization and biomimetic recovery of the crown
37. In vitro fatigue resistance of CAD/CAM composite resin and ceramic posterior occlusal veneers10.1016/S0022-3913(10)60111-4 ↗
38. Survival of Dicor glass-ceramic dental restorations over 14 years. Part II: effect of thickness of Dicor material and design of tooth preparation10.1016/S0022-3913(99)70104-6 ↗
39. Fluoride release from three glass ionomer materials and the effects of varnishing with or without finishing10.1159/000261466 ↗
40. Fracture strength of teeth restored with ceramic inlays and overlays10.1590/S0103-64402009000200010 ↗
41. Thermal cycling for restorative materials: does a standardized protocol exist in laboratory testing? A literature review10.1016/j.jmbbm.2013.09.013 ↗
42. Self-adhesive resin cements: a literature review
43. Performance of dental ceramics: challenges for improvements10.1177/0022034510391795 ↗
44. Influence of restoration thickness and dental bonding surface on the fracture resistance of full-coverage occlusal veneers made from lithium disilicate ceramic10.1016/j.dental.2015.04.017 ↗
45. A comparative study of fracture resistance between morphologic dowel and cores and a resin-reinforced dowel system in the intraradicular restoration of structurally compromised roots
46. Novel-design ultra-thin CAD/CAM composite resin and ceramic occlusal veneers for the treatment of severe dental erosion10.1016/S0022-3913(11)60035-8 ↗
47. Microleakage after thermocycling of cemented crowns--a meta-analysis10.1016/j.dental.2011.05.002 ↗
48. Influence of cavity preparation design on fracture resistance of posterior Leucite-reinforced ceramic restorations10.1016/j.prosdent.2006.03.022 ↗
49. CAD/CAM ceramic restorative materials for natural teeth10.1177/0022034518779759 ↗
50. Three-unit reinforced polyetheretherketone composite FDPs: influence of fabrication method on load-bearing capacity and failure types10.4012/dmj.2013-345 ↗
51. Fracture resistance and failure modes of polymer infiltrated ceramic endocrown restorations with variations in margin design and occlusal thickness10.1016/j.jpor.2017.11.003 ↗
52. Fracture resistance of maxillary premolars with class II MOD cavities restored with Ormocer, Nanofilled, and Nanoceramic composite restorative systems
53. Full-mouth adhesive rehabilitation of a severely eroded dentition: the three-step technique. Part 1
54. A novel bite force recorder and maximal isometric bite force values for healthy young adults
55. Bite force and dentofacial morphology in men with severe dental attrition10.1111/j.1600-0722.1994.tb01161.x ↗
56. Enamel mineral loss10.1016/S0300-5712(14)50002-4 ↗
57. Long-term strength of ceramics for biomedical applications10.1002/jbm.b.20039 ↗
58. Deep-penetrating conical cracks in brittle layers from hydraulic cyclic contact10.1002/jbm.b.30195 ↗