Processing and mechanical characteristics of magnesium-hydroxyapatite metal matrix biocomposites
Source abstract
Abstract
Magnesium/hydroxyapatite composites were produced by conventional extrusion and their mechanical behavior studied under uniaxial compression at room temperature. The results evidence the capability of the HA for strengthening the Mg material, lowering its microstructural anisotropy and inhibiting deformation twinning. They also reveal that the ECAP processing is effective for improving the grain structure and reducing the crystallographic texture of these composites, giving rise to a significant enhancement of their yield strength and microhardness although the ultimate compressive stress worsens. The analysis of the strain hardening rate of the flow curves demonstrates that the HA addition and the ECAP processing are also effective in inhibiting non-basal dislocation slip.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. The plastic deformation of polycrystalline aggregates10.1080/14786436208201857 ↗
2. Corrosion mechanism applicable to biodegradable magnesium implants10.1016/j.mseb.2010.12.017 ↗
3. Influence of grain size on the compressive deformation of wrought Mg-3Al-1Zn10.1016/j.actamat.2004.07.015 ↗
4. Bunge · 2015 · 88
5. On the strain behavior of magnesium at room temperature10.1016/j.msea.2005.12.113 ↗
6. Strain hardening behavior and the Taylor factor of pure magnesium10.1080/14786430801968611 ↗
7. Strain hardening due to {1 0 1 2} twinning in pure magnesium10.1080/14786430701881211 ↗
8. Mechanical properties and corrosión behavior of Mg-HAP composites10.1016/j.jmbbm.2014.07.014 ↗
9. Grain-size dependence of the flow stress of Cu from millimeters to nanometers10.1007/s11661-004-0214-5 ↗
10. Significance of twinning in the anisotropic behavior of a magnesium alloy processed by equal-channel angular pressing10.1016/j.scriptamat.2010.05.016 ↗
11. Microstructure, mechanical property, bio-corrosion and cytotoxicity evaluations of Mg/HA composites10.1016/j.msec.2010.03.016 ↗
12. Plane-strain compression of magnesium and magnesium alloy crystals
13. Physics and phenomenology of strain hardening: the FCC case10.1016/S0079-6425(02)00003-8 ↗
14. The development of binary Mg-Ca alloys for use as biodegradable materials within bone10.1016/j.biomaterials.2007.12.021 ↗
15. Mechanical and corrosion properties of magnesium-hydroxyapatite composite thin films10.1016/j.jmst.2013.04.019 ↗
16. Thermal stability and corrosion behavior of Mg-Y-Nd and Mg-Tb-Nd alloys10.1016/j.msea.2005.11.077 ↗
17. Grain boundary strengthening in strongly textured magnesium produced by hot rolling10.1007/BF02648393 ↗
18. De-twinning and texture change in an extruded AM30 magnesium alloy during compression along normal direction10.1016/j.jmst.2014.11.018 ↗
19. Control of biodegradation of biocompatible magnesium alloys10.1016/j.corsci.2007.01.001 ↗
20. Magnesium and its alloys as orthopedic materials: a review10.1016/j.biomaterials.2005.10.003 ↗
21. Effect of Zr on the microstructure, mechanical properties and corrosion resistance of Mg-10Gd-3Y magnesium alloy10.1016/j.msea.2009.06.002 ↗
22. Biodegradable Mg and Mg alloys: corrosion and biocompatibility10.1016/j.mseb.2011.05.028 ↗
23. Effects of preferred orientation on the grain size dependence of yield strength in metals10.1080/14786436308207317 ↗
24. Ductility of polycrystalline magnesium below 300 K
25. The history of biodegradable magnesium implants: a review10.1016/j.actbio.2010.02.028 ↗
26. Biodegradable magnesium-hydroxyapatite metal matrix composites10.1016/j.biomaterials.2006.12.027 ↗
27. Degradable biomaterials based on magnesium corrosion10.1016/j.cossms.2009.04.001 ↗
28. In vivo corrosion of four magnesium alloys and the associated bone response10.1016/j.biomaterials.2004.09.049 ↗