Mechanical performance of Y-TZP monolithic ceramic after grinding and aging: Survival estimates and fatigue strength
Source abstract
Abstract
This study aims to evaluate the flexural fatigue strength and survival estimates of an Y-TZP monolithic ceramic after grinding and aging. Ceramic discs (1.2 mm thickness × 15.0 mm diameter - ISO, 6872, 2015) of zirconia (Zirlux FC2 - Ardent; Ivoclar Vivadent) were made and randomly allocated into 6 groups (n = 10), according to grinding and aging factors: Ctrl - as-sintered; Ctrl Sto - as-sintered and dry stored at room temperature for 2 years; Ctrl Aut Sto - as-sintered, submitted to autoclaved aging (134 °C, 2 bar, 20 h) and then dry stored for 2 years; and similar conditions for ground samples (Ground; Ground Sto; Ground Aut Sto). Grinding was performed with diamond burs (#3101G, KG Sorensen) coupled to a contra-angle torque multiplier attached to a low speed motor under constant irrigation. Fatigue testing followed a step-stress approach. Data from strength and number of cycles until fracture were recorded and analyzed through Kaplan-Meier and Mantel-Cox tests. Both grinding and aging increase monoclinic phase content. The topography was altered by grinding but not by aging procedures. Grinding did not alter the fatigue strength (Ctrl = Ground), while aging increase it only for ground groups (Ground Sto, Ground Aut Sto). Aged conditions (Ctrl Sto; Ground Sto; Ctrl Aut Sto; Ground Aut Sto) showed increased survival probabilities for both flexural fatigue strength and cycles for failure. Therefore, despite promoting monoclinic phase increase, aging and grinding did not deleteriously affect the fatigue behavior of Y-TZP ceramics.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Advanced ceramic materials synthesis · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Fatigue behavior of zirconia under different loading conditions10.1016/j.dental.2016.03.012 ↗
2. Degradability of dental ceramics10.1177/08959374920060012201 ↗
3. Biosmart materials: breaking new ground in dentistry10.1155/2014/986912 ↗
4. Biaxial flexure strength and low temperature degradation of Ce-TZP/Al2O3 nanocomposite and Y-TZP as dental restoratives10.1002/jbm.b.31131 ↗
5. A critical perspective on mechanical testing of implants and prostheses10.1177/0022034515624445 ↗
6. Step-stress analysis for predicting dental ceramic reliability10.1016/j.dental.2013.05.009 ↗
7. Low-temperature degradation of zirconia and implications for biomedical implants10.1146/annurev.matsci.37.052506.084250 ↗
8. Fatigue testing procedures and statistical interpretations of data
9. Emerging ceramic-based materials for dentistry10.1177/0022034514553627 ↗
10. Loading frequencies up to 20 Hz as an alternative to accelerate fatigue strength tests in a Y-TZP ceramic10.1016/j.jmbbm.2016.01.008 ↗
11. Phase analysis in zirconia systems10.1111/j.1151-2916.1972.tb11290.x ↗
12. Mechanical behavior of yttria-stabilized tetragonal zirconia polycrystal: effects of different aging regimens10.1590/1807-3107bor-2017.vol31.0094 ↗
13. Transformation toughening in zirconia-containing ceramics10.1111/j.1151-2916.2000.tb01221.x ↗
14. Dentistry – Ceramic Materials
15. ADM guidance-ceramics: fatigue principles and testing10.1016/j.dental.2017.09.006 ↗
16. Clinically relevant approach to failure testing of all-ceramic restorations10.1016/S0022-3913(99)70103-4 ↗
17. The effect of low temperature aging on the mechanical property & phase stability of Y-TZP ceramics10.4047/jap.2009.1.3.113 ↗
18. Clinical evaluation of monolithic zirconia crowns: a short-term pilot report10.11607/ijp.5444 ↗
19. Phase change and mechanical properties of ZrO2–Y2O3 solid electrolyte after ageing10.1016/0167-2738(81)90138-7 ↗
20. Fracture load of metal-ceramic, monolithic, and bi-layered zirconia-based posterior fixed dental prostheses after thermo-mechanical cycling10.1016/j.jdent.2018.04.012 ↗
21. Low temperature degradation -aging- of zirconia: a critical review of the relevant aspects in dentistry10.1016/j.dental.2010.04.006 ↗
22. Mettas A., Vassiliou P., 2002. Modeling and analysis of time-dependent stress accelerated life data. In: Proceedings of the Annual Reliability and Maintainability Symposium. IEEE. 343–348. doi: 10.1109/RAMS.2002.981665.10.1109/RAMS.2002.981665 ↗
23. Microstructural changes in ground 3Y-TZP and their effect on mechanical properties10.1016/j.actamat.2011.07.024 ↗
24. Fracture resistance of monolithic zirconia molar crowns with reduced thickness10.3109/00016357.2015.1007479 ↗
25. Nelson W. 1980. Accelerated life testing step-stress models and data analyses. IEEE Transactions of Reliability. r-29(2):103-108. doi: 10.1109/TR.1980.5220742.10.1109/TR.1980.5220742 ↗
26. The effect of grinding on the mechanical behavior of Y-TZP ceramics: a systematic review and meta-analyses10.1016/j.jmbbm.2016.06.028 ↗
27. Fatigue limit of polycrystalline zirconium oxide ceramics: effect of grinding and low-temperature aging. Pereira GKR, Silvestri T, Amaral M, Rippe MP, Kleverlaan CJ, Valandro LF10.1016/j.jmbbm.2016.01.006 ↗
28. Low-temperature degradation of Y-TZP ceramics: a systematic review and meta-analysis10.1016/j.jmbbm.2015.10.017 ↗
29. Surface properties of monolithic zirconia after dental adjustment treatments and in vitro wear simulation10.1016/j.jdent.2014.08.011 ↗
30. Contemporary materials and technologies for all-ceramic fixed partial dentures: a review of the literature10.1016/j.prosdent.2004.09.015 ↗
31. All-ceramic or metal-ceramic tooth-supported fixed dental prostheses (FDPs)? A systematic review of the survival and complication rates. Part I: single crowns (SCs)10.1016/j.dental.2015.02.011 ↗
32. ADM guidance—ceramics: guidance to the use of fractography in failure analysis of brittle materials10.1016/j.dental.2017.03.004 ↗
33. Optical properties of zirconia ceramics for esthetic dental restorations: a systematic review10.1016/j.prosdent.2017.07.009 ↗
34. Effect of grinding and multi-stimuli aging on the fatigue strength of a Y-TZP ceramic10.1590/0103-6440201801735 ↗
35. Three generations of zirconia: from veneered to monolithic. Part I
36. Color aspect of monolithic zirconia restorations: a review of the literature
37. Calibration curve for quantitative analysis of the monoclinic tetragonal ZrO2 system by X-rays diffraction10.1111/j.1151-2916.1984.tb19715.x ↗
38. Chairside CAD/CAM materials. Part 2: flexural strength testing10.1016/j.dental.2016.10.008 ↗
39. Stress fatigue: basic principles and prosthodontic implications