Degradation kinetics of high-translucency dental zirconias: Mechanical properties and in-depth analysis of phase transformation
Source abstract
Abstract
This study aimed to evaluate the effects of low temperature degradation (LTD) on commercial dental zirconias (conventional and high-translucent - HT) with different microstructures, as well as on their mechanical properties and t-m phase transformation. The amount of monoclinic zirconia in different depths was quantified using X-ray diffraction (XRD) with different anode tubes (Cr, Co and Cu). XRD was also used to measure the residual stress of the materials at 0 h, 26 h and 140 h aging times. Vickers microhardness and biaxial flexural strength tests were performed. Data were subjected to two-way ANOVA and Tukey's post-hoc test, both with α = 0.05 for means comparisons. Weibull parameters were calculated and compared based on the overlapping of confidence intervals (CI = 95%). HT Zirconia presented smaller grain sizes and had a higher rate of t-m transformation over time. The microstructure of the conventional zirconia showed an expressive increase of the grain size and consequently greater morphological variation with the LTD. The non-aged samples (control) did not present any residual stress and the aged ones presented compression stress. All zirconia showed a residual stress increase with the increase of LTD time, but the conventional one showed a decrease after 140 h. HT zirconia showed no significant change in flexural strength over LTD time, but the conventional one showed a strength decrease after 140 h (681.78 ± 121.18 MPa). Vickers hardness decreased for all zirconia samples after 26 h. The mechanics of LTD is significantly altered in different zirconia microstructures. Zirconias with smaller grains are more prone to t-m phase transformation, but present lower variation of residual stress, while larger grains zirconias have a lower surface area and therefore a more pronounced increase in stress over LTD time. Stress values close to the maximum compression stress generates ejection of the zirconia grains, producing defects and causing reduction of the compression stress and consequently decrease of flexural strength.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Dental Erosion and Treatment
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Low-temperature degradation of a Y-TZP ceramic after surface treatments10.1002/jbm.b.32957 ↗
2. Quantitative phase analysis from X-ray diffraction in Y-TZP dental ceramics: a critical evaluation10.1016/j.jdent.2014.08.010 ↗
3. ASTM C1327-15 · 2015
4. ASTM E384-89 · 1997
5. Influence of hydrothermal and mechanical conditions on the strength of zirconia10.1016/j.actbio.2010.07.025 ↗
6. Hydrothermal degradation of a 3Y-TZP translucent dental ceramic: a comparison of numerical predictions with experimental data after 2 years of aging10.1016/j.dental.2015.12.015 ↗
7. Low-temperature aging of Y-TZP ceramics10.1111/j.1151-2916.1999.tb02055.x ↗
8. Low-temperature degradation of zirconia and implications for biomedical implants10.1146/annurev.matsci.37.052506.084250 ↗
9. Weibull analysis and flexural strength of hot-pressed core and veneered ceramic structures10.1016/S0109-5641(03)00010-1 ↗
10. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
11. A critical comparison of methods for the determination of the aging sensitivity in biomedical grade yttria-stabilized zirconia10.1002/jbm.b.30123 ↗
12. Phase analysis in zirconia systems10.1111/j.1151-2916.1972.tb11290.x ↗
13. Ceramic steel?10.1038/258703a0 ↗
14. Sub-surface assessment of hydrothermal ageing in zirconia-containing femoral heads for hip joint applications10.1016/j.actbio.2017.12.021 ↗
15. Influence of low-temperature degradation on the wear characteristics of zirconia against polymer-infiltrated ceramic-network material10.1016/j.prosdent.2017.12.014 ↗
16. Aging resistance of surface-treated dental zirconia10.1016/j.dental.2014.11.018 ↗
17. Effect of multistep processing technique on the formation of micro-defects and residual stresses in zirconia dental restorations10.1111/jopr.12094 ↗
18. Phase change and mechanical properties of ZrO2-Y2O3 solid electrolyte after ageing10.1016/0167-2738(81)90138-7 ↗
19. Zirconia in Dentistry: Part 2. Evidence-based clinical breakthrough
20. Fracture strength of four-unit Y-TZP FPD cores designed with varying connector diameter. An in-vitro study10.1111/j.1365-2842.2007.01770.x ↗
21. Effect of grain size on the monoclinic transformation, hardness, roughness, and modulus of aged partially stabilized zirconia10.1016/j.dental.2015.09.014 ↗
22. Low temperature degradation -aging- of zirconia: a critical review of the relevant aspects in dentistry10.1016/j.dental.2010.04.006 ↗
23. An overview of zirconia ceramics: basic properties and clinical applications10.1016/j.jdent.2007.07.008 ↗
24. New high-translucent cubic-phase-containing zirconia: clinical and laboratory considerations and the effect of air abrasion on strength
25. Current status of zirconia restoration10.1016/j.jpor.2013.09.001 ↗
26. Low-temperature degradation of Y-TZP ceramics: a systematic review and meta-analysis10.1016/j.jmbbm.2015.10.017 ↗
27. Fatigue limit of polycrystalline zirconium oxide ceramics: effect of grinding and low-temperature aging10.1016/j.jmbbm.2016.01.006 ↗
28. Zirconia as a ceramic biomaterial10.1016/S0142-9612(98)00010-6 ↗
29. A practical and systematic review of Weibull statistics for reporting strengths of dental materials10.1016/j.dental.2009.09.006 ↗
30. Effect of in vitro aging on the flexural strength and probability to fracture of Y-TZP zirconia ceramics for all-ceramic restorations10.1016/j.dental.2014.05.033 ↗
31. Ultrathin monolithic zirconia veneers: reality or future? Report of a clinical case and one-year follow-up10.2341/16-350-T ↗
32. The relationship between isothermal and non-isothermal description of Johnson-Mehl-Avrami-Kolmogorov kinetics10.1016/0022-3697(92)90096-V ↗
33. Role of H2O on the degradation process of Y-TZP10.1007/BF01756800 ↗
34. Novel zirconia materials in dentistry10.1177/0022034517737483 ↗
35. Effect of aging time and thickness on low-temperature degradation of dental zirconia