journal article·2021-07

Fatigue resistance of monolithic strength-gradient zirconia materials

Lisa Marie Schönhoff, Nina Lümkemann, Ramona Buser, Rüdiger Hampe, Bogna Stawarczyk

Publisher page

Abstract

Purpose Evaluation of the effect of three different dynamic fatigue protocols on the fracture resistance of two monolithic strength-gradient zirconia materials. Materials and methods A total of 240 specimens (3 × 4 × 45 mm) was milled from two different layers (incisal and middle) of two types of strength-gradient zirconia blanks (IPS e. max ZirCAD MT Multi A2 vs. IPS e. max ZirCAD Prime A2), resulting in 60 specimens per material and layer group (IPS e. max ZirCAD MT Multi A2: incisal (MI), middle (MM); IPS e. max ZirCAD Prime A2: incisal (PI), middle (PM)). Each group was divided into one static (n = 15) and three dynamic fatigue protocols (N = 45, n = 15): i. 50 N increase every 5000 cycles ii. Increase by 5% of static fracture load every 5000 cycles iii. 10 N increase every 1000 cycles until facture. All specimens were loaded until facture in CeraTest 2 k. Kaplan-Meier, Log-Rank and Chi-squared-test as well as Weibull statistics were performed. A fractographic analysis was performed. The specimens were classified according to the number of crack origins and evaluated using the Ciba-Geigy table. Results With regard to the fracture load, in the static loading MI and PI showed a higher fracture load and in dynamic fatigue protocol 2 PI showed a lower fracture load. The number of cycles until fracture only differed within three groups: MM and MI survived a higher number of cycles in dynamic fatigue protocol 2; PI survived a higher number of cycles in dynamic fatigue protocol 2 than in protocol 1. Within dynamic fatigue protocols, PM resisted the highest number of cycles in protocol 1 and 3 and MI in protocol 2. Comparing groups, Weibull modulus differed only within the static loading, with PI showing lower values than MM and MI. Within the material groups, MI showed higher values in static loading than in dynamic fatigue protocol 1 and 2, and PI showed higher values in the dynamic fatigue protocol 3 than in static loading. With regard to fracture patterns, no differences were found between the groups. Conclusions Dynamic fatigue protocols provide clinically relevant information on the long-term stability and reliability of monolithic strength-gradient zirconia materials. However, no definitive instructions for dynamic testing can be provided from this investigation.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Dental materials and restorations · Polymer Nanocomposites and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Fatigue limit of monolithic Y-TZP three-unit-fixed dental prostheses: effect of grinding at the gingival zone of the connector10.1016/j.jmbbm.2017.03.002 ↗
2. Step-stress analysis for predicting dental ceramic reliability10.1016/j.dental.2013.05.009 ↗
3. Two regression methods for estimation of a two-parameter Weibull distribution for reliability of dental materials10.1016/j.dental.2014.11.014 ↗
4. Fatigue resistance of CAD/CAM complete crowns with a simplified cementation process10.1016/j.prosdent.2013.09.020 ↗
5. In vitro study of the fracture resistance of monolithic lithium disilicate, monolithic zirconia, and lithium disilicate pressed on zirconia for three-unit fixed dental prostheses10.4047/jap.2017.9.4.244 ↗
6. Coelho · 2014 · 1
7. Load-bearing capacity of screw-re- tained CAD/CAM-produced titanium implant frameworks (I-Bridge®2) before and after cyclic mechanical loading10.1590/1678-775720130077 ↗
8. Misfit and fracture load of implant-supported monolithic crowns in zirconia-rein- forced lithium silicate10.1590/1678-7757-2016-0233 ↗
9. Fracture frequency of all-ceramic crowns during dynamic loading in a chewing simulator using different loading and luting protocols10.1016/j.dental.2008.02.019 ↗
10. Assessing flexural strength degradation of new cubic containing zirconia materials10.5005/jp-journals-10024-2762 ↗
11. Impact of high-speed sintering on translucency, phase content, grain sizes, and flexural strength of 3Y-TZP and 4Y-TZP zirconia materials10.1016/j.prosdent.2019.02.005 ↗
12. Fracture strength of monolithic all-ceramic crowns made of high translucent yttrium oxide-stabilized zirconium dioxide compared to porcelain-veneered crowns and lithium disilicate crowns10.3109/00016357.2013.822098 ↗
13. All-ceramic single crown restauration of zirconia oral implants and its influence on fracture resistance: an investigation in the artificial mouth10.3390/ma8041577 ↗
14. Fracture strength of aged monolithic and bilayer zirconia-based crowns
15. Fracture of porcelain-veneered gold-alloy and zirconia molar crowns using a modified test set-up
16. Impact of hydrothermal aging on the light transmittance and flexural strength of colored yttria-stabilized zirconia materials of different formulations
17. Comparison between novel strength-gradient and color-gradient multilayered zirconia using conventional and high-speed sintering10.1016/j.jmbbm.2020.103977 ↗
18. Failure probability of three designs of zirconia crowns10.11607/prd.2448 ↗
19. Approach for valuating the significance of laboratory simulation10.1016/j.jdent.2008.09.001 ↗
20. Fatigue and wear behaviour of zirconia materials10.1016/j.jmbbm.2020.103970 ↗
21. Multilayer zirconia: influence of positioning within blank and sintering conitions on the in vitro performance of 3-unit fixed partial dentures
22. ADM guidance-Ceramics: guidance to the use of fractography in failure analysis of brittle materials10.1016/j.dental.2017.03.004 ↗
23. Reliability and aging behavior of three different zirconia grades used for monolithic four-unit fixed dental prostheses10.1016/j.dental.2020.08.002 ↗
24. Three generations of zirconia: from veneered to monolithic. Part I
25. Three generations of zirconia: from veneered to monolithic. Part II
26. Fatigue fracture strength of implant-supported full contour zirconia and metal ceramic fixed partial dentures
27. In-vitro performance and fracture strength of thin monolithic zirconia crowns10.4047/jap.2018.10.2.79 ↗
28. Effect of fatigue on biaxial flexural strength of bilayered porcelain/zirconia (Y-TZP) dental ceramics10.1016/j.dental.2011.03.019 ↗
29. Novel zirconia materials in dentistry10.1177/0022034517737483 ↗