Mechanical behavior and microstructure of compressed Ti foams synthesized via freeze casting
Source abstract
Abstract
Pure Ti and Ti-5%W foams were prepared via freeze casting. The porosity and grain size of both the materials were 32-33% and 15-17µm, respectively. The mechanical behavior of the foams was investigated by uniaxial compression up to a plastic strain of ~0.26. The Young׳s moduli of both foams were ~23GPa, which was in good agreement with the value expected from their porosity. The Young׳s moduli of the foams were similar to the elastic modulus of cortical bones, thereby eliminating the osteoporosis-causing stress-shielding effect. The addition of W increased the yield strength from ~196MPa to ~235MPa. The microstructure evolution in the grains during compression was studied using electron backscatter diffraction (EBSD) and X-ray line profile analysis (XLPA). After compression up to a plastic strain of ~0.26, the average dislocation densities increased to ~3.4×10(14)m(-2) and ~5.9×10(14)m(-2) in the Ti and Ti-W foams, respectively. The higher dislocation density in the Ti-W foam can be attributed to the pinning effect of the solute tungsten atoms on dislocations. The experimentally measured yield strength was in good agreement with the strength calculated from the dislocation density and porosity. This study demonstrated that the addition of W to Ti foam is beneficial for biomedical applications, because the compressive yield strength increased while its Young׳s modulus remained similar to that of cortical bones.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Bone Tissue Engineering Materials · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Effect of tungsten additions on the mechanical properties of Ti-6Al-4V10.1016/j.msea.2005.01.051 ↗
2. Tribological properties of biocompatible Ti–10W and Ti–7.5TiC–7.5W10.1016/j.jmbbm.2013.11.014 ↗
3. Load along the femur shaft during activities of daily living10.1016/j.jbiomech.2013.06.012 ↗
4. Contrast factors of dislocations in the hexagonal crystal system10.1107/S0021889802009536 ↗
5. Titanium with controllable pore fractions by thermoreversible gelcasting of TiH210.1016/j.actamat.2008.06.035 ↗
6. Microstructure and mechanical properties of Ti/W and Ti-6Al-4V/W composites fabricated by powder-metallurgy10.1016/S0921-5093(02)00426-4 ↗
7. Ti based biomaterials, the ultimate choice for orthopedic implants – a review10.1016/j.pmatsci.2008.06.004 ↗
8. Gubicza · 2014
9. Microstructure and mechanical behavior of ultrafine-grained titanium10.4028/www.scientific.net/MSF.589.99 ↗
10. Microstructure and mechanical properties of reticulated titanium scrolls10.1002/adem.201100082 ↗
11. Processing of porous Ti and Ti5Mn foams by spark plasma sintering10.1016/j.matdes.2010.06.019 ↗
12. Low stiffness porous Ti structures for load-bearing implants10.1016/j.actbio.2007.03.008 ↗
13. X-ray diffraction line broadening due to dislocations in non-cubic materials. II. The case of elastic anisotropy applied to hexagonal crystals10.1107/S002188988800336X ↗
14. An evaluation of yield criteria and flow rules for aluminium alloys10.1016/S0749-6419(98)00064-3 ↗
15. Effect of pore morphology and bone ingrowth on mechanical properties of microporous titanium as an orthopedic implant material10.2320/matertrans.45.1124 ↗
16. Gradient ultrafine-grained titanium: Computational study of mechanical and damage behaviour10.1016/j.actamat.2014.03.017 ↗
17. Titanium alloys in total joint replacement—a materials science perspective10.1016/S0142-9612(97)00146-4 ↗
18. Porosity-dependence of elastic moduli and hardness of 3Y-TZP ceramics10.1016/S0272-8842(98)00037-6 ↗
19. Magee · 2008
20. The evolution of non-basal dislocations as a function of deformation temperature in pure magnesium determined by X-ray diffraction10.1016/j.actamat.2004.02.034 ↗
21. On the influence of space holder in the development of porous titanium implants: mechanical, computational and biological evaluation10.1016/j.matchar.2015.08.019 ↗
22. Mechanical biocompatibilities of titanium alloy for biomedical applications10.1016/j.jmbbm.2007.07.001 ↗
23. Processing and properties of porous titanium using space holder technique10.1016/j.msea.2008.11.022 ↗
24. Deformation mechanism map for titanium10.1016/0036-9748(77)90151-X ↗
25. Orientation dependent mechanical properties of commercially pure (cp) titanium10.1016/j.matchar.2014.10.011 ↗
26. Young׳s modulus of trabecular and cortical bone material: ultrasonic and microtensile measurements10.1016/0021-9290(93)90042-D ↗
27. Correlation between strength and microstructure of ball-milled Al–Mg alloys determined by X-ray diffraction10.1016/j.msea.2004.01.089 ↗
28. Fabrication methods of porous metals for use in orthopedic applications10.1016/j.biomaterials.2005.12.002 ↗
29. The role of porous polymeric materials in prosthesis attachment10.1002/jbm.820080315 ↗
30. Measurements and micro-mechanical modelling of the response of sintered titanium foams10.1016/j.jmbbm.2016.02.024 ↗
31. Effect of pore size on bone ingrowth into porous titanium implants fabricated by additive manufacturing: an in vivo experiment10.1016/j.msec.2015.10.069 ↗
32. Osteocondustivity and hydrophilicity of TiO2 coatings on Ti substrates prepared by different oxidizing process10.1155/2012/495218 ↗
33. The influence of cell morphology on the compressive fatigue behavior of Ti-6Al-4V meshes fabricated by electron beam melting10.1016/j.jmbbm.2016.01.034 ↗