journal article·2020-01

Tribological and wear behaviour of alumina toughened zirconia nanocomposites obtained by pressureless rapid microwave sintering

L. Gil-Flores, M.D. Salvador, F.L. Penaranda-Foix, A. Dalmau, A. Fernández, A. Borrell

Publisher page

Abstract

Dense alumina toughened zirconia nanocomposites (ATZ, 3Y-TZP with 20 wt% Al2O3) were densified by non-conventional microwave sintering technology at relatively low temperatures (1200 and 1300 °C). The sintering method and its effect on densification, microstructure, mechanical properties and tribological behaviour were investigated. The outcomes demonstrated that the density rose as the sintering temperature was higher, and therefore the mechanical properties were enhanced, reaching a maximum hardness (18.4 ± 0.4 GPa) and fracture toughness (5.7 ± 0.3MPa· m1/2). In addition, the samples were subjected to a tribological test in dry and wet conditions, using artificial saliva. In both cases, the coefficient of friction and wear volume for samples obtained by microwave sintering are lower than conventional samples, with the wear volume being two times higher in dry conditions than in wet conditions.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. ASTM C373-14 standard test method for water absorption, bulk density, apparent porosity, and apparent specific gravity of fired whiteware products
2. ASTM E112-13: standard test methods for determining average grain size
3. Mechanical properties and microstructural evolution of alumina-zirconia nanocomposites by microwave sintering10.1016/j.ceramint.2014.03.153 ↗
4. Microwave, spark plasma and conventional sintering to obtain controlled thermal expansion β-eucryptite materials
5. Zirconia as a dental biomaterial10.3390/ma8084978 ↗
6. Densification mechanisms in spark plasma sintering of nanocrystalline ceramics10.1016/j.msea.2006.07.092 ↗
7. Metallic implant biomaterials10.1016/j.mser.2014.10.001 ↗
8. The tetragonal-monoclinic transformation in zirconia: lessons learned and future trends10.1111/j.1551-2916.2009.03278.x ↗
9. Tribological characterization of alumina and silicon carbide under lubricated sliding10.1016/0301-679X(93)90016-T ↗
10. Fracture toughness determinations by indentation10.1111/j.1151-2916.1976.tb10991.x ↗
11. Chemical treatment on alumina-zirconia composites inducing apatite formation with maintained mechanical properties10.1016/j.jeurceramsoc.2011.12.020 ↗
12. Densification and grain growth during sintering of nanosized particles10.1179/174328008X353538 ↗
13. Machining of biocompatible ceramics with femtosecond laser pulses
14. Microstructure and mechanical properties of 5.8 GHz microwave-sintered ZrO2/Al2O3 ceramics10.1016/j.ceramint.2019.06.026 ↗
15. Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramics10.1016/j.dental.2003.05.002 ↗
16. Field-assisted sintering technology/spark plasma sintering: mechanisms, materials, and technology developments10.1002/adem.201300409 ↗
17. Tribology of ceramics10.1016/0043-1648(90)90075-L ↗
18. Stabilized zirconia as a structural ceramic: an overview10.1016/j.dental.2007.05.005 ↗
19. Alumina toughened zirconia from yttria coated powders10.1016/j.jeurceramsoc.2012.03.014 ↗
20. Microstructure and mechanical properties of ZrO 2 (Y 2O 3)-Al 2O 3 nanocomposites prepared by spark plasma sintering10.1016/j.partic.2011.05.002 ↗
21. An overview of zirconia ceramics: basic properties and clinical applications10.1016/j.jdent.2007.07.008 ↗
22. Development of alumina toughened zirconia nanocomposites using spark plasma sintering
23. Microwave hybrid fast sintering of porcelain bodies10.1016/j.jmatprotec.2007.02.041 ↗
24. Microwave-material interaction phenomena: heating mechanisms, challenges and opportunities in material processing10.1016/j.compositesa.2015.10.035 ↗
25. Mechanical properties of alumina-zirconia composites for ceramic abutments10.1590/S1516-14392004000400021 ↗
26. Quantitative analysis of monoclinic phase in 3Y-TZP by Raman spectroscopy10.1111/j.1551-2916.2010.03635.x ↗
27. On the wide range of mechanical properties of ZTA and ATZ based dental ceramic composites by varying the Al2O3 and ZrO2 content10.1016/j.ijrmhm.2009.06.001 ↗
28. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
29. Effect of microwave sintering on microstructure and mechanical properties in Y-TZP materials used for dental applications10.1016/j.ceramint.2015.02.025 ↗
30. Hydrothermal degradation behavior of Y-TZP ceramics sintered by nonconventional microwave technology10.1111/jace.13810 ↗
31. Comparison between microwave and conventional sintering on the properties and microstructural evolution of tetragonal zirconia10.1016/j.ceramint.2018.02.086 ↗
32. The design and manufacture of biomedical surfaces10.1016/j.cirp.2007.10.001 ↗
33. Microwave sintering: fundamentals and modeling10.1111/jace.12278 ↗
34. Development and characterization of zirconia–alumina composites for orthopedic implants10.1016/j.ceramint.2016.09.216 ↗
35. Nanotechnology in joint replacement10.1002/wnan.47 ↗
36. Microwave sintering of zirconia ceramics10.1023/A:1017966703650 ↗
37. Low temperature degradation of Al2O3-doped 3Y-TZP sintered at various temperatures10.1016/j.ceramint.2013.02.065 ↗
38. Effect of micro-alumina content on mechanical properties of Al2O3/3Y-TZP composites10.1016/j.ceramint.2015.06.081 ↗