Influence of artificial aging on mechanical properties of commercially and non-commercially available zirconia dental implants
Source abstract
Abstract
Objective To evaluate the effect of artificial aging on the mechanical resistance and micromechanical properties of commercially and noncommercially available zirconia dental implants. Methods Scanning electron microscopy (SEM) and X-ray computed tomography (X-CT) were performed on implant systems including: Z-systems®, Straumann®, Zibone® and commercially and non-commercially available TAV dental® with varying grain sizes. Accelerated aging was performed at 134 °C and 2-bar pressure for 30 hours. Before and after aging, the mechanical load to failure was investigated and the bending moments were calculated. Nanoindentation responses of the representative Zibone implant before and after aging were performed to evaluate the effects of aging on hardness (H) and Young's modulus (E). A two-sample t-test statistical analysis was used to determine significant differences of bending moments within groups. Results All implants presented with compact and homogenous core structures without porosities. The bending moment was significantly increased after aging for all groups (P ≤ 0.05) except for Z-systems (significant decrease (P = 0.022)) and TAV group 3 (no significant increase (P = 0.181)). The increase in bending moment was less pronounced with increasing grain size in TAV groups (group 1: P = 0.036, group 2: P = 0.05, group 3: P = 0.18). E and H were reduced approximately 32% and 18% respectively following aging within the transformed, microcracked zone of the presentative Zibone implant. Conclusions Aging led to both increase and decrease of the mechanical properties of the implant systems analyzed. The apparent contrast amongst groups can be explained based on differences in grain sizes and surface features. Aging decreased micromechanical properties of one implant system which warrants further investigation.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental Implant Techniques and Outcomes · Dental materials and restorations · Bone Tissue Engineering Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. A 15-year study of osseointegrated implants in the treatment of the edentulous jaw10.1016/S0300-9785(81)80077-4 ↗
2. Survival of NebelDirect Implants: an analysis of 550 consecutively placed implants at different clinical centers10.1111/j.1708-8208.2007.00054.x ↗
3. Are ceramic implants a viable alternative to titanium implants? A systematic literature review10.1111/j.1600-0501.2009.01785.x ↗
4. Influence of hydrothermal and mechanical conditions on the strength of zirconia10.1016/j.actbio.2010.07.025 ↗
5. The effect of ceria co-doping on chemical stability and fracture toughness of Y-TZP10.1007/BF00351622 ↗
6. Intra-osseous anchorage of dental prostheses. I. Experimental studies
7. Osseointegrated implants in the treatment of edentulous jaw. Experience from a 10-year period
8. Low temperature degradation of a Y-TZP dental ceramic10.1016/j.actbio.2010.09.020 ↗
9. Effect of different surface treatments on the hydrothermal degradation of a 3Y-TZP ceramic for dental implants10.1016/j.dental.2014.07.004 ↗
10. On the relationship between plastic zone radius and maximum depth during nanoindentation10.1016/j.surfcoat.2006.08.099 ↗
11. What future for zirconia as a biomaterial?10.1016/j.biomaterials.2005.07.034 ↗
12. Low-temperature degradation of zirconia and implications for biomedical implants10.1146/annurev.matsci.37.052506.084250 ↗
13. The tetragonal-monoclinic transformation in zirconia: lessons learned and future trends10.1111/j.1551-2916.2009.03278.x ↗
14. The tetragonal-monoclinic transformation in zirconia: lessons learned and future trends10.1111/j.1551-2916.2009.03278.x ↗
15. Low-temperature degradation in zirconia with a porous surface10.1016/j.actbio.2011.03.006 ↗
16. Mechanical properties and short-term in-vivo evaluation of yttrium-oxide-partially-stabilized zirconia10.1002/jbm.820230105 ↗
17. Current status pf Zirconia used in total hip implants10.2106/00004623-200300004-00009 ↗
18. The influence of surface modification techniques on the performance of a Y-TZP dental ceramics10.1016/j.jdent.2005.06.006 ↗
19. Quantification of hydrothermal degradation in zirconia by nanoindentation10.1016/j.actamat.2008.04.050 ↗
20. Ageing effects on the nanoindentation response of sub-micrometric 3Y-TZP ceramics10.1007/s10853-006-1177-2 ↗
21. Influence of sintering conditions on low-temperature degradation of dental zirconia10.1016/j.dental.2014.03.005 ↗
22. Focused ion beam tomography of zirconia degraded under hydrothermal conditions10.1016/j.jeurceramsoc.2012.02.011 ↗
23. Influence of surface treatments on surface roughness, phase transformation, and biaxial flexural strength of Y-TZP ceramics10.1002/jbm.b.31477 ↗
24. Direct evidence for continuous linear kinetics in the low-temperature degradation of Y-TZP10.1016/j.actbio.2012.08.032 ↗
25. Phase change and mechanical properties of ZrO2-Y2O3 solid electrolyte after ageing10.1016/0167-2738(81)90138-7 ↗
26. The effects of cyclic loading and prepatation on the fracutre strength of zirconium-dioxide implants: an in vitro investigation10.1111/j.1600-0501.2010.02067.x ↗
27. Low-temperature degradation of different zirconia ceramics for dental applications10.1016/j.actbio.2011.11.016 ↗
28. Evaluation of intensity of artifacts in cone beam computer tomography by radiopacity of composite filling material and simulation models of implants
29. Lawn · 1993
30. Environmental degradation of zirconia ceramics10.1016/0955-2219(95)00035-S ↗
31. Increased levels of dissolved titanium are associated with Peri-implantitis- a cross-sectional study
32. Low temperature degradation-aging-of zirconia: a critical review of the relevant aspects in dentistry10.1016/j.dental.2010.04.006 ↗
33. Strengthening of vickers indented 3Y-TZP by hydrothermal ageing10.1016/j.jeurceramsoc.2011.08.019 ↗
34. The impact of in vitro accelerated aging, approximating 30 and 60 Years in vivo, on commercially available zirconia dental implants
35. In vivo forces on implants influenced by occlusal scheme and food consistency
36. A critical review of dental implant materials with an emphasis on titanium versus zirconia10.3390/ma8030932 ↗
37. Zirconia as a ceramic biomaterial10.1016/S0142-9612(98)00010-6 ↗
38. Low temperature degradtion and reliability of one-piece ceramic oral implants with a porous surface10.1016/j.dental.2013.01.007 ↗
39. A new testing protocol for zirconia dental implants10.1016/j.dental.2014.09.002 ↗
40. Two-piece Zirconia oral implants withstand masticatory loads: an investigation in the artificial mouth10.1016/j.jmbbm.2015.07.005 ↗
41. Effect of alumina addition on the tetragonal to monoclinic phase transformation in zirconia-3 mol% yttria10.1111/j.1151-2916.1991.tb06905.x ↗
42. 10‐year survival rate and the incidence of peri‐implant disease of 374 titanium dental implants with a SLA surface: a prospective cohort study in 177 fully and partially edentulous patients10.1111/clr.12499 ↗
43. Role of H2O on degradation process of Y-TZP10.1007/BF01756800 ↗